DIN17100 STEELS FOR GENERAL STRUCTURAL PURPOSES
Read more →DIN7527 Steel Forgings Machining Allowances and Permissible Variations for Open die Forged Bars
Read more →DIN50602 Microscopic examination of special steels using standard diagrams to assess the content of non-metallic inclusions
Read more →ASTM E45 2011 Standard Test Methods for Determining the Inclusion Content of Steel
Read more →ASTM A331 1995 Standard Specification for Cold Finished Alloy Steel Bars
Read more →ASTM A682 2002 Standard Specification for Steel Strip, High Carbon, Cold Rolled, General Requirements
Read more →ASTM A705 Standard Specification for Age Hardening Stainless Steel Forgings
Read more →ASTM E112 2010 Standard Test Methods for Determining Average Grain Size