Quenching is the process for making material harder. The metal is heated to a specific temperature and rapidly cooled (quenched) in a bath of water, brine, oil, or air to increase its hardness.

One drawback of using this method by itself is that the metal becomes brittle. This treatment is therefore typically followed by a tempering process which is a heating process at another lower specific temperature to stress relieve the material and minimize the brittleness problem. The temperature chosen for the tempering process directly impacts the hardness of the work piece . The higher the temperature in the tempering process, the lower the hardness.

We can supply follows heat treatment services:

Normalizing, Annealing, Quenching, Tempering, Carburizing, Nitriding, High-frequency surface hardening and other processing services.

And we can strictly enforce the national standards.

And we have follows heating equipment:

  Pit furnace: Dia1300mm max, Length9500mm max.
  Salt bath furnace: Length1900mm max, Width1600mm max, Height900mm max.
  Trolley furnace: Legth15000mm max, Width6000mm max, Height6000mm max.
Tunnel type continuous reheating furnace:dia30mm-dia250mm
Induction quenching line: dia15mm-dia120mm
Normalizing cooling fan can be used in combination of wind capacity air-cooled systems.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the import and export of Tool Steel, Iron Alloy Steel and other special steel products… More Info

Contact Lists

General Manager: Ms. Florence
admin@fushunspecialsteel.com

Sales Manager for American, Oceanian, Asian market: Mr. Crane
crane@fushunspecialsteel.com

Sales Manager for European, African, Asia market: Miss Summer
summer@fushunspecialsteel.com