Grade : HS1-4-2
Number: 1.3326
Classification: High-speed tool steel
Standard: EN ISO 4957: 2000 Tool steels

 

Chemical composition %  of steel HS1-4-2 (1.3326):  EN 4957-2000

C Si Mn P S Cr Mo V W
0.85 – 0.95 max 0.65 max 0.4 max 0.03 max 0.03 3.6 – 4.3 4.1 – 4.8 1.7 – 2.2 0.8-1.4

Mechanical properties  of steel HS1-4-2 (1.3326)

Brinell hardness   (HB):   (+A) 262

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x