manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Stainless Steel

Stainless steel is not one material but five metallurgical families that behave very differently in service, and choosing the wrong one is the most common mistake we see in enquiries. 304 will pit where 2205 survives; 316 is not a substitute for 904L in hot chloride; a 420 blade will not hold an edge at 600 °C. The table below groups what we supply by how the alloy is actually chosen.

Families, and the question each one answers

Family Grades we supply Choose it when
Austenitic 304/304L, 316/316L, 316LN, 321 (1.4541), 347/347H, 310/310S/310H, 317/317L, 301, 302, 303, XM-19 General corrosion resistance, weldability, cryogenic to 800 °C
Super austenitic 904L (N08904), 254SMO (S31254), 654 SMO (S32654), AL-6XN (N08367), Alloy 31 (N08031), 27-7MO, 1.4563, 1.4565 Chloride pitting and crevice corrosion, seawater, acid service
Duplex 2205 (S32205 / S31803), 2507 (S32750), F55 (S32760), 2304 (S32304), S32001 lean duplex, 329 Twice the yield of austenitic, resistance to chloride stress corrosion
Martensitic 410 (1.4006), 420 (1.4021), 431 (1.4057), 440A/B/C, 1.4125, 1.4028, 1.4034, 1.4418 Hardenable: blades, shafts, valve trim, wear parts
Ferritic 409 (1.4512), 430 / 430F / 430Ti, 444 (1.4521), 1.4003, 1.4509 Stress corrosion resistance, oxidation resistance, cost control
Precipitation hardening 17-4PH (630), 15-5PH (S15500), 17-7PH (631), 13-8PH, 15-7PH, AM350, AM355, XM-25 High strength plus corrosion resistance in one part
Rebar BS 6744 full range (1.4362, 1.4462, 1.4404, 1.4429, 1.4501, 1.4529), UNS S30400, S31603, S31803 Concrete structures specified for a 100-year design life

Forms, finishes and melting route

Round bar, wire, strip, sheet, plate, seamless tube and forgings are all supplied from the same order desk. Ultra-high purity grades for semiconductor service are melted VIM-VAR and packed for cleanroom use to SEMI F20. For duplex and super austenitic grades, state the PREN target and whether the part will be welded — both change the heat treatment and the test schedule we quote.

See the full grade list → — every designation with its UNS, Werkstoff and JIS equivalent, plus the condition we hold.

316L UHP Ultra High Purity Stainless Steel Bar – SEMI F20 | FUSHUN METAL

316L UHP Ultra High Purity Stainless Steel Bar – SEMI F20 | FUSHUN METAL

15-7PH / S15700 / 1.4532 / X8CrNiMoAl15-7-2 Stainless Steel Supplier | FUSHUN METAL

15-7PH / S15700 / 1.4532 / X8CrNiMoAl15-7-2 Stainless Steel Supplier | FUSHUN METAL

S41425 / 1.4415 / X2CrNiMoV13-5-2 Stainless Steel Supplier | FUSHUN METAL

S41425 / 1.4415 / X2CrNiMoV13-5-2 Stainless Steel Supplier | FUSHUN METAL

X53CrMnNiNbN21-9 / 1.4870 Niobium-Modified Austenitic Valve Steel (21-43N) — FUSHUN METAL

X53CrMnNiNbN21-9 / 1.4870 Niobium-Modified Austenitic Valve Steel (21-43N) — FUSHUN METAL

253MA S30815 | 1.4835 | Ce Stainless Steel | 1150°C Oxidation | Fushun Metal

253MA S30815 | 1.4835 | Ce Stainless Steel | 1150°C Oxidation | Fushun Metal

D2 Forged Rings | Cold Work Tool Steel

D2 Forged Rings | Cold Work Tool Steel

BS 6744 Grade 1.4529 Super Austenitic Stainless Steel Rebar

BS 6744 Grade 1.4529 Super Austenitic Stainless Steel Rebar

BS 6744 Grade 1.4501 Super Duplex Stainless Steel Rebar

BS 6744 Grade 1.4501 Super Duplex Stainless Steel Rebar

BS 6744 Grade 1.4429 Stainless Steel Rebar (N-Enhanced)

BS 6744 Grade 1.4429 Stainless Steel Rebar (N-Enhanced)

BS 6744 Grade 1.4404 Stainless Steel Rebar (316L)

BS 6744 Grade 1.4404 Stainless Steel Rebar (316L)

BS 6744 Grade 1.4462 Stainless Steel Rebar (2205 Duplex)

BS 6744 Grade 1.4462 Stainless Steel Rebar (2205 Duplex)

BS 6744 Grade 1.4362 Duplex Stainless Steel Rebar

BS 6744 Grade 1.4362 Duplex Stainless Steel Rebar

BS 6744 Grade 1.4162 Duplex Stainless Steel Rebar

BS 6744 Grade 1.4162 Duplex Stainless Steel Rebar

BS 6744 Grade 1.4436 Stainless Steel Rebar

BS 6744 Grade 1.4436 Stainless Steel Rebar

BS 6744 Grade 1.4311 Stainless Steel Rebar – B500B

BS 6744 Grade 1.4311 Stainless Steel Rebar – B500B

2205 (UNS S31803) Duplex Stainless Steel Rebar

2205 (UNS S31803) Duplex Stainless Steel Rebar

316LN (UNS S31653) Stainless Steel Rebar

316LN (UNS S31653) Stainless Steel Rebar

316L (UNS S31603) Stainless Steel Rebar

316L (UNS S31603) Stainless Steel Rebar

304 (UNS S30400) Stainless Steel Rebar

304 (UNS S30400) Stainless Steel Rebar

XM-28 (UNS S24100) Stainless Steel Rebar

XM-28 (UNS S24100) Stainless Steel Rebar

XM-29 (UNS S24000) Stainless Steel Rebar

XM-29 (UNS S24000) Stainless Steel Rebar

SUS420J1 Cold Rolled Stainless Steel Strip and Sheet

SUS420J1 Cold Rolled Stainless Steel Strip and Sheet

AISI 431 S43100 SUS431 1.4057 Stainless Steel

AISI 431 S43100 SUS431 1.4057 Stainless Steel

1.2083, S136, X40Cr14, Stainless Tool Steel

1.2083, S136, X40Cr14, Stainless Tool Steel

1.4125 X105CrMo17 UNS S44004 440C Stainless Steel

1.4125 X105CrMo17 UNS  S44004 440C Stainless Steel

1.4112 X90CrMoV18 UNS S44003 440B Stainless Steel

1.4112 X90CrMoV18 UNS S44003 440B Stainless Steel

SUS420J2 Stainless Steel

SUS420J2 Stainless Steel

AISI 420 S42000 Stainless Steel

AISI 420 S42000 Stainless Steel

Special Austenitic Stainless Steel – Certified Supplier

Special Austenitic Stainless Steel – Certified Supplier

Duplex Stainless Steel | Certified 2507, 2205 Supplier

Duplex Stainless Steel | Certified 2507, 2205 Supplier

Super Austenitic Stainless Steel: 254SMO, 904L, AL-6XN

Super Austenitic Stainless Steel: 254SMO, 904L, AL-6XN

Martensitic Stainless Steel Manufacturer & Exporter | Fushun Special Steel

Martensitic Stainless Steel Manufacturer & Exporter | Fushun Special Steel

AM355 Precipitation Hardening Stainless Steel

AM355 Precipitation Hardening Stainless Steel

961 S47310 Martensitic Stainless Heat-Resistant Steel

961 S47310 Martensitic Stainless Heat-Resistant Steel

1.4362 | Alloy 2304 | S32304 Duplex Stainless Steel

1.4362 | Alloy 2304 | S32304 Duplex Stainless Steel

1.4424 / X2CrNiMoN18-14-3 Stainless Steel

1.4424 / X2CrNiMoN18-14-3 Stainless Steel

S31500 / 1.4417 Duplex Stainless Steel

S31500 / 1.4417 Duplex Stainless Steel

Alloy 350 / S35000 / AM350 Stainless Steel

Alloy 350 / S35000 / AM350 Stainless Steel

660, S66286, Alloy A-286, Stainless Steel

660, S66286, Alloy A-286, Stainless Steel

1.4420, S31655, Stainless Steel

1.4420, S31655, Stainless Steel

1.4565, Alloy 24, S34565, Super Austenitic Stainless Steel

1.4565, Alloy 24, S34565, Super Austenitic Stainless Steel

316L VIM-VAR Ultra-High Purity Stainless Steel for Semiconductor Equipment

316L VIM-VAR Ultra-High Purity Stainless Steel for Semiconductor Equipment

309Si2, 1.4828, S38240, Stainless Steel

309Si2, 1.4828, S38240, Stainless Steel

Incoloy 840 alloy, 1.4847, S33400, Stainless Steel

Incoloy 840 alloy, 1.4847, S33400, Stainless Steel

310Si2, X8CrNiSI25-21, S38340, Stainless Steel

310Si2, X8CrNiSI25-21, S38340, Stainless Steel

2.4694, Alloy 751, SUH751, N07751, Valve Nickel Alloy

2.4694, Alloy 751, SUH751, N07751, Valve Nickel Alloy

1.4875, X55CrMnNiN20-8, EV12, Valve Stainless Steel

1.4875, X55CrMnNiN20-8, EV12, Valve Stainless Steel

2.4952, Nimonic 80A, NiCr20TiAl, N07080, Valve Nickel Alloy

2.4952, Nimonic 80A, NiCr20TiAl, N07080, Valve Nickel Alloy

NCF3015, S66315, Ni30, Valve Stainless Steel

NCF3015, S66315, Ni30, Valve Stainless Steel

S63012 Valve Stainless Steel

S63012 Valve Stainless Steel

1.4871, X53CrMnNiN21-9, EV12, SUH35, Valve Stainless Steel

1.4871, X53CrMnNiN21-9, EV12, SUH35, Valve Stainless Steel

1.4882, X50CrMnNiNbN21-9, Valve Stainless Steel

1.4882, X50CrMnNiNbN21-9, Valve Stainless Steel

1.2731, X50NiCrWV13-13, SUH31, Valve & Tool Steel

1.2731, X50NiCrWV13-13, SUH31, Valve & Tool Steel

1.4866, X33CrNiMnN23-8, EV16, Valve Stainless Steel

1.4866, X33CrNiMnN23-8, EV16, Valve Stainless Steel

1.4748, X85CrMoV18-2, Stainless Valve Steel

1.4748, X85CrMoV18-2, Stainless Valve Steel

1.4718, X45CrSi9-3, HNV3, SUH1, Stainless Valve Steel

1.4718, X45CrSi9-3, HNV3, SUH1, Stainless Valve Steel

1.4731, X40CrSiMo10-2, SUH3, Valve Stainless Steel

1.4731, X40CrSiMo10-2, SUH3, Valve Stainless Steel

1.4361,X1CrNiSi18-15-4, S30600, Stainless Steel

1.4361,X1CrNiSi18-15-4, S30600, Stainless Steel

XM-19, 1.3964, S20910, Austenitic Stainless Steel

XM-19, 1.3964, S20910, Austenitic Stainless Steel

13-8PH 1.4534 Martensitic Precipitation-Hardening Stainless Steel

13-8PH 1.4534 Martensitic Precipitation-Hardening Stainless Steel

303, 1.4305, S30300, Stainless Steel

303, 1.4305, S30300, Stainless Steel

301, S30100, 1.4310, SUS301, Stainless Steel

301, S30100, 1.4310, SUS301, Stainless Steel

1.4545, S15500, XM-12, 15-5PH, Precipitation Hardening Stainless Steel

1.4545, S15500, XM-12, 15-5PH, Precipitation Hardening Stainless Steel

1.4542, S17400, 630, 17-4PH, Precipitation Hardening Stainless Steel

1.4542, S17400, 630, 17-4PH, Precipitation Hardening Stainless Steel

2205, S32205, S31803, 1.4462, F51, Duplex Stainless Steel

2205, S32205, S31803, 1.4462, F51, Duplex Stainless Steel

2507, S32750, 1.4410, F53, Super Duplex Stainless Steel

2507, S32750, 1.4410, F53, Super Duplex Stainless Steel

310, 310S, 310H, 1.4845, Stainless Steel

310, 310S, 310H, 1.4845, Stainless Steel

N08367, AL-6XN, INCOLOY 25-6HN, Super-Austenitic Stainless Steel

N08367, AL-6XN, INCOLOY 25-6HN, Super-Austenitic Stainless Steel

N08031, 1.4562, Alloy 31, Nicrofer 3127 hMo, Stainless Steel

N08031, 1.4562, Alloy 31, Nicrofer 3127 hMo, Stainless Steel

INCOLOY 27-7MO, S31277, Super-Austenitic Stainless Steel

INCOLOY 27-7MO, S31277, Super-Austenitic Stainless Steel

654 SMO, S32654, 1.4652, Stainless Steel

654 SMO, S32654, 1.4652, Stainless Steel

S32254 Super Austenitic Stainless Steel

S32254 Super Austenitic Stainless Steel

S32050 Super Austenitic Stainless Steel

S32050 Super Austenitic Stainless Steel

1.4547, F44, 245SMO, S31254, Super Austenitic Stainless Steel

1.4547, F44, 245SMO, S31254, Super Austenitic Stainless Steel

1.4539, 904L, N08904, Stainless Steel

1.4539, 904L, N08904, Stainless Steel

310MoLN, 1.4466, Stainless Steel

310MoLN, 1.4466, Stainless Steel

440C, SUS440C, 95Cr18, Stainless Steel For Blade Cutter

440C, SUS440C, 95Cr18, Stainless Steel For Blade Cutter

5Cr15 Blade Stainless Steel

5Cr15 Blade Stainless Steel

154CM Blade Stainless Steel

154CM Blade Stainless Steel

420HC Stainless Steel

420HC Stainless Steel

SUH31, 4Cr14Ni14W2Mo, 45KH14N14V2M, 45Х14Н14В2М, Heat Resisting Steel

SUH31, 4Cr14Ni14W2Mo, 45KH14N14V2M, 45Х14Н14В2М, Heat Resisting Steel

1.4594, XM-25, S45000, Stainless Steel

1.4594, XM-25, S45000, Stainless Steel

Stainless Steel Welding Wire

Stainless Steel Welding Wire

440C Stainless Steel Bright Small Rod

440C Stainless Steel Bright Small Rod

Stainless Steel Ultra Fine Wire

Stainless Steel Ultra Fine Wire

Stainless Steel Wires

Stainless Steel Wires

Stainless Steel Foil

Stainless Steel Foil

1.4563 Stainless Steel

1.4563 Stainless Steel

Greek Ascoloy, Alloy 418, S41800, Stainless Steel For Turbine Blades

Greek Ascoloy, Alloy 418, S41800, Stainless Steel For Turbine Blades

AISI 616, Alloy 422, S42200, Stainless Steel For Turbine Blades

AISI 616, Alloy 422, S42200, Stainless Steel For Turbine Blades

XM-32, S6412, Stainless Steel For Turbine Blades

XM-32, S6412, Stainless Steel For Turbine Blades

UNS S32001 EN 1.4482 LEAN DUPLEX STAINLESS STEEL

UNS S32001 EN 1.4482 LEAN DUPLEX STAINLESS STEEL

1.4935, X20CRMOWV12-1, AISI 422, CREEP RESISTING STEEL

1.4935, X20CRMOWV12-1, AISI 422, CREEP RESISTING STEEL

S47450 18Cr11NiMoNbVN 2Cr11NiMoNbVN Stainless Steel For Steam Turbine Blade

S47450 18Cr11NiMoNbVN 2Cr11NiMoNbVN Stainless Steel For Steam Turbine Blade

S46020 21Cr12MoV 2Cr12MoV Stainless Steel For Steam Turbine Blade

S46020 21Cr12MoV 2Cr12MoV Stainless Steel For Steam Turbine Blade

S47010 15Cr12WMoV 1Cr12W1MoV Stainless Steel For Steam Turbine Blade

S47010 15Cr12WMoV 1Cr12W1MoV Stainless Steel For Steam Turbine Blade

1Cr11MoV 1.4922 X20CrMoV11-1 Stainless Steel For Steam Turbine Blade

1Cr11MoV 1.4922 X20CrMoV11-1 Stainless Steel For Steam Turbine Blade

SUS420J1 1.4119 X15CrMo13 Stainless Steel For Steam Turbine Blade

SUS420J1 1.4119 X15CrMo13 Stainless Steel For Steam Turbine Blade

420 1.4021 X20Cr13 Stainless Steel For Steam Turbine Blade

420 1.4021 X20Cr13 Stainless Steel For Steam Turbine Blade

410 1.4006 X12Cr13 Stainless Steel For Steam Turbine Blade

410 1.4006 X12Cr13 Stainless Steel For Steam Turbine Blade

Heat Resistant Steel

Heat Resistant Steel

316LN UNS S31653 Austenitic Stainless Steel

316LN UNS S31653 Austenitic Stainless Steel

F55, S32760, 1.4501, Super Duplex Stainless Steel

F55, S32760, 1.4501, Super Duplex Stainless Steel

1.4435 X2CrNiMo18-14-3 Austenitic Stainless Steel

1.4435 X2CrNiMo18-14-3 Austenitic Stainless Steel

1.4571 X6CrNiMoTi17-12-2 Austenitic Stainless Steel

1.4571 X6CrNiMoTi17-12-2 Austenitic Stainless Steel

1.4313 X3CrNiMo13-4 Martensitic Stainless Steel

1.4313 X3CrNiMo13-4 Martensitic Stainless Steel

1.4104 X14CrMoS17 Martensitic Stainless Steel

1.4104 X14CrMoS17 Martensitic Stainless Steel

1.4006 X12Cr13 Martensitic Stainless Steel

1.4006 X12Cr13 Martensitic Stainless Steel

1.4509 X2CrTiNb18 Ferritic Stainless Steel

1.4509 X2CrTiNb18 Ferritic Stainless Steel

1.4003 X2CrNi12 Ferritic Stainless Steel

1.4003 X2CrNi12 Ferritic Stainless Steel

1.4122 X39CrMo17-1 Stainless Steel

1.4122 X39CrMo17-1 Stainless Steel

SUS420J2 Stainless Steel

SUS420J2 Stainless Steel

X46Cr13 1.4034 Stainless Steel

X46Cr13 1.4034 Stainless Steel

X30Cr13 1.4028 Stainless Steel

X30Cr13 1.4028 Stainless Steel

1.4418 X4CrNiMo16-5-1 Stainless Steel

1.4418 X4CrNiMo16-5-1 Stainless Steel

2Cr13 20Cr13 S42020 Stainless Steel

2Cr13 20Cr13 S42020 Stainless Steel

1.4021 X20Cr13 Stainless Steel

1.4021 X20Cr13 Stainless Steel

Stainless Steel Strip and Coils

Stainless Steel Strip and Coils

X22CrMoV12-1 1.4923 Martensitic Creep Resisting Stainless Steel

X22CrMoV12-1 1.4923 Martensitic Creep Resisting Stainless Steel

329 S32900 1.4460 stainless Steel

329 S32900 1.4460 stainless Steel

347 347H 1.4550 1.4961 Stainless Steel

347 347H 1.4550 1.4961 Stainless Steel

317 317L 1.4449 1.4438 Stainless Steel

317 317L 1.4449 1.4438 Stainless Steel

430 1.4016 430F 1.4104 430Ti 1.4510 Stainless Steel

430 1.4016 430F 1.4104 430Ti 1.4510 Stainless Steel

409 1.4512 X6CrTi12 Ferritic Stainless Steel

409 1.4512 X6CrTi12 Ferritic Stainless Steel

631, S17700, 17-7PH, 1.4568, Precipitation Hardening Stainless Steel

631, S17700, 17-7PH, 1.4568, Precipitation Hardening Stainless Steel

AISI 444 1.4521 Stainless Steel

AISI 444 1.4521 Stainless Steel

AISI 410 410L 410S Stainless Steel

AISI 410 410L 410S Stainless Steel

7Cr17MoV Steel

7Cr17MoV Steel

1.4057 Stainless Steel

1.4057 Stainless Steel

AISI 321 1.4541 SUS321 S32100 Stainless Steel

AISI 321 1.4541 SUS321 S32100 Stainless Steel

302 S30200 1.4319 SUS302 Stainless Steel

302 S30200 1.4319 SUS302 Stainless Steel

ASTM A313 Stainless Steel Spring Wire

ASTM A313 Stainless Steel Spring Wire

1.4528 Cold Rolled Stainless Steel Sheet

1.4528 Cold Rolled Stainless Steel Sheet

AISI 431 S43100 SUS431 1.4057 Stainless Steel Round Bar

AISI 431 S43100 SUS431 1.4057 Stainless Steel Round Bar

400 Series Stainless Steel

400 Series Stainless Steel

440A B C Cold Rolled Stainless Steel Strip and Sheet

440A B C Cold Rolled Stainless Steel Strip and Sheet

304 Flat Bar Cold Drawn Stainless Steel

304 Flat Bar Cold Drawn Stainless Steel

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x