Bearing steel is a narrow family: one through-hardening grade does most of the work, and the rest of the range exists for temperature, corrosion or load. GCr15 — the same steel as 100Cr6, SUJ2 and 52100 — covers the majority of rolling bearings in the world. The variations we supply differ in melting route, cleanliness rating and case depth rather than in composition.
Grades we supply
| Grade | Equivalent | Where it is used |
|---|---|---|
| GCr15 | 100Cr6 (1.3505), SUJ2, 52100, EN31 | Standard through-hardening bearings, 60–66 HRC after quench and temper |
| GCr15 SiMn | 100CrMn6 | Large section bearings where GCr15 will not harden through |
| M50 | AMS 6491 | Aerospace bearings to 300 °C |
| 440C | S44004, 1.4125 | Corrosion resistant bearings, instrument and medical |
What separates one delivery from another
Oxygen content, inclusion rating and carbide banding decide bearing life far more than the chemistry. We quote against your specification: whether the steel is to be supplied spheroidise annealed, whether decarburisation is measured to a stated depth, and whether the order needs VAR or ESR remelting for aerospace or high-speed spindle duty.
Bar, wire and tube are available; the certificate carries the heat number, hardness and the inclusion rating you ask for.