13-8PH 1.4534 Martensitic Precipitation-Hardening Stainless Steel
Premium Quality by FUSHUN METAL
Advanced Manufacturing Excellence
As a leading Chinese manufacturer of specialty stainless steels, FUSHUN METAL produces high-quality 13-8PH martensitic precipitation-hardening stainless steel through advanced double-melting processes including Vacuum Induction Melting followed by Vacuum Arc Remelting (VIM-VAR) or Electroslag Remelting (ESR) techniques. This premium alloy demonstrates exceptional strength, high hardness, superior toughness, and excellent corrosion resistance comparable to 304 stainless steel, with optimal performance achieved in the fully hardened condition.
Our 13-8 PH steel features outstanding transverse toughness properties through precise chemical composition control, low carbon content design, and vacuum melting technology, offering a wide range of mechanical properties through single precipitation hardening heat treatment. The material exhibits excellent weldability with helium gas shielding recommended for optimal results, and maintains corrosion resistance similar to standard austenitic grades.
Chemical Composition Analysis
| Symbol | Element | Min % | Max % |
|---|---|---|---|
| C | Carbon | – | 0.05% |
| Mn | Manganese | – | 0.10% |
| Si | Silicon | – | 0.10% |
| P | Phosphorus | – | 0.010% |
| S | Sulfur | – | 0.008% |
| Cr | Chromium | 12.25% | 13.25% |
| Ni | Nickel | 7.50% | 8.50% |
| Mo | Molybdenum | 2.00% | 2.50% |
| N | Nitrogen | – | 0.010% |
| Al | Aluminum | 0.90% | 1.35% |
| Fe | Iron | – | Balance |
Heat Treatment Conditions
| Condition | Temperature |
|---|---|
| H950 | 950 °F ± 10 °F (510 °C ± 6 °C) |
| H1000 | 1000 °F ± 10 °F (538 °C ± 6 °C) |
| H1025 | 1025 °F ± 10 °F (552 °C ± 6 °C) |
| H1050 | 1050 °F ± 10 °F (566 °C ± 6 °C) |
| H1100 | 1100 °F ± 10 °F (593 °C ± 6 °C) |
| H1150 | 1150 °F ± 10 °F (621 °C ± 6 °C) |
Mechanical Properties Performance
| Condition | Tensile Strength | Yield 0.2% Offset | Elongation (%in 2″) | Reduction of Area | Brinell Hardness | Rockwell Hardness |
|---|---|---|---|---|---|---|
| Ann | 175 ksi max | – | – | – | 363 max | – |
| H950 | 220 ksi | 205 ksi | 10% | 45% | – | C45 min |
| H1000 | 205 ksi | 190 ksi | 10% | 50% | – | C45 min |
| H1025 | 185 ksi | 175 ksi | 11% | 50% | – | – |
| H1050 | 175 ksi | 165 ksi | 12% | 50% | – | C40 min |
| H1100 | 150 ksi | 135 ksi | 14% | 50% | – | C34 min |
| H1150 | 135 ksi | 90 ksi | 14% | 50% | – | C30 min |
Key Applications & Industries
High-performance aircraft structural parts and components
Precision manufacturing tools and machinery
High-pressure cutting system components
Corrosion-resistant process equipment
Critical nuclear facility components
High-performance marine applications
Our products are widely utilized in aerospace, marine engineering, petrochemical, and other high-performance applications requiring exceptional combinations of strength, toughness, and corrosion resistance, backed by our comprehensive production capabilities and stringent quality control systems.
Complete Product Range & Specifications
Available Product Forms
| Product Forms | Classification | Specifications (mm) |
|---|---|---|
| Ingots | Master alloy | Φ70~280 mm |
| Ingots | Φ360~700 mm | |
| Forged Products | Round bar | Φ30~450 mm |
| Square bar | 30~600 mm | |
| Plate, disc, flange, ring | According to your request | |
| Rods & Bars | Hot Rolled | Φ8~200 |
| Cold Drawn | Φ1~60 | |
| Tubes | Seamless | OD:6~273 WT:1~30 L:500~10000 |
| Welded | According to your request | |
| Fitting | Wrought/forged | Delivery according ASTM B16.9 B16.11 |
| Wires | Roll/straight | Φ0.1~25 mm |
| Strip | hot/cold roll | T:0.10~3.5 W:200~400mm |
| Plate & Sheet | Hot Rolled | T:3~50mm W:400~2500mm L:1000~8000mm |
| Cold Rolled | T:0.4~4mm W:400~1200mm L:1000~2200mm |
International Standards & Specifications
Common Specifications:
• AMS 5629 Bars, Forgings, Wire, Extrusions
• AMS 5629/H1000 (produced & precipitation hardened to H1000 condition)
• AMS 5864 (Plate)
• ASTM A564 (Type XM-13 Bars, Wires, Shapes)
• ASTM A693 (Sheet, Plate, Strip)
• ASTM A705 (Forgings)
Common Trade Names:
• PH13-8Mo
• XM-13
• UNS S13800
• 1.4534
• X3CrNiMoAl13-8-2
• DMS 2100 Grade
• HMS 6-1105 REV A AMD 3
• ST0160LB0013 REV E
• ASTM F899-12B
• RMS-150 REV N
Comprehensive Heat Treatment Services
Heat treatment, which is one of the special processes in which the mechanical properties of the material are re-shaped and which requires high engineering knowledge and experience, has been serving for more than 20 years with FUSHUN METAL’s expert engineers. We have a huge range of heat treatment facilities that can make special processes on tool steel, mould steel, high speed steels, stainless steel, alloy steel, nickel alloy, etc.
Advanced Machining Capabilities
FUSHUN METAL offers not only an optimum material in various forms, but also pre-machined and ready-to-install parts. We put extensive consulting know-how and modern machining facilities at the disposal of our customers.
Comprehensive Quality Control
All production workflows at FUSHUN METAL are monitored, inspected and controlled – from material checking, from melting to casting, and from the internal, surface, dimensional and identity checks in the finishing shops of the rolling mills and forging shops or on the bright steel lines, all the way to mechanical and technological tests on specimens.
Precise measurement of material strength properties
Maximum stress material can withstand
Ductility and flexibility testing
Brinell, Vickers, Rockwell C testing methods
Grain size, structure, micro-cleanliness, and flaws
Performance under elevated temperatures
Toughness and impact resistance evaluation
Non-destructive testing for defect detection
FUSHUN METAL – Your Trusted Steel Partner
Over 20 years of expertise in specialty stainless steel manufacturing with advanced production facilities and stringent quality control systems. We supply 13-8PH stainless steel in various forms including bars, wire, forgings, rings, extrusions, sheet, and plate materials conforming to AMS 5629 aerospace specifications.