manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Invar 36 UNS K93600 UNS K93603 1.3912 Ni36 Nickel Alloy

Invar 36 UNS K93600 UNS K93603 1.3912 Ni36 Nickel Alloy

Invar 36 UNS K93600 UNS K93603 1.3912 Ni36 Nickel Alloy

Invar 36 UNS K93600 UNS K93603 1.3912 Ni36 Nickel Alloy

With over 35 years of industry expertise, Fushun has the industry knowledge and resources to find you the metal products that you need for your specific industry applications. We are in stock and ready to quickly deliver hard-to-find metals. Our ISO 9001-certified metal supply is one of the most comprehensive selections on the market. We provide timely customer support and quick delivery on all quantities of our in stock products.

 

Contact us for more information regarding our nickel alloy manufacturing and distribution options.  Fushun is your trusted nickel alloy supplier for all types of Nickel alloy material.

Description

Invar 36 is a nickel-iron, low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coefficient of expansion from cryogenic temperatures to about 500°F. The alloy also retains good strength and toughness at cryogenic temperatures. Invar 36 is a 36% nickel-iron alloy possessing a rate of thermal expansion approximately one-tenth that of carbon steel at temperatures up to 400°F(204°C)

Applications

This alloy has been used for applications where dimensional changes due to temperature variation must be minimized such as in radio and electronic devices, aircraft controls, optical and laser system, etc. Invar 36 alloy has also been used in conjunction with high expansion alloys in applications where a motion is desired when the temperature changes, such as in bimetallic thermostats and in rod and tube assemblies for temperature regulators.

Specifications

AFNOR NF A54-301 (chemistry only), ASTM F 1684-06, EN 1.3912, UNS K93600, UNS K93603, Werkstoff 1.3912

Chemical Composition

Grade % Ni Fe C Mn Si P S
Invar 36 Min 35 Bal. 0.2
Max 37 0.05 0.6 0.3 0.02 0.02

Mechanical Properties Typical Room Temperature Mechanical Properties Mill Annealed

Temperature Yield Strength

0.2% Offset

Tensile Strength Elongation on 50 mm

(2 inch) %

Reduction of Area %
°C °F (MPa) psi (MPa) psi
20 68 240 35.0 490 71.0 42 70

Material Advantages

Invar 36 can be hot and cold formed and machined using processes like austenitic stainless steels and is also weldable using Filler Metal CF26. Some of the other benefits associated with the use of Invar nickel alloy 36 include: Superior dimensional stability,  Numerous workability aspects, Extremely low coefficient of thermal expansion (CTE).

Welding

Invar 36 can be welded by the convetional methods. Caution must be taken so as not to overheat the molten metal. This will avoid spattering of the molten metal and pits in the welded area. When filler rod is required , Invarod has been used.

Corrosion properties

Invar 36 is corrosion resistant in dry atmospheres at room temperature. Under unfavourable conditions, i.e., in humid or moist atmospheres, corrosion can occur in the form of rust.

Machinability

Invar is tough and ductile and therefore somewhat difficult to machine. It should be machined in the annealed condition. The machining characteristics of Invar 36 are similar to austenitic stainless steels. Because of its high ductility, the chips formed during machining tend to be stringy and tough and may thus impose rapid wear on the cutting tool edges. In general, slow speeds and light feeds should be used to avoid excessive heat and minimize the possibility of the generated heat affecting the expansion characteristics. An adequate depth of cut is important, however, in order to cut below any previously formed work-hardened zone. High speed steel or sintered carbide tools should be used and cutting edges should be kept sharp.

Forging

The principal precaution to observe in forging is to heat quickly and avoid soaking in the furnace. Long soaking may result in a checked surface due to absorption of sulfur from the furnace atmosphere and/or oxide penetration. A forging temperature of 2000/2150øF (1100/1180øC) is preferred. Invar alloy 36 may also be swaged and cold upset.

Quality & Testing

Fushun supply Certification with all shipments, containing full chemical analysis and also mechanical test results if requested.

 

All incoming material is visually inspected and PMI (Positive Material Identification) tested before processing begins and all our production material is checked during each stage of processing.

 

All incoming orders are produced to the individual customer specification, some of which may involve processing sample batches for testing prior to full production.

 

Final Inspection carried out on all finished material to include:

Visual inspection

Dimensional checks

PMI (Positive Material Identification)

Mechanical tests

 

Nickel Alloy Material Available Formats

Fushun offers pure Nickel alloy materials in a variety of forms, including:

Seamless & welded pipe

Seamless & welded tube

Bar

Wire

Sheet

Plate

Forgings

Pipe fittings

Flanges

Weld Rod

 

Nickel Alloy Supply Quantities for Single Items or Full Bills

At Fushun, we can supply single items or full bills of nickel alloy materials for most any project. No inquiry is too small. We offer quick responses to customer inquiries and specialize in the rapid delivery of both large and small quantities of nickel alloy products.

 

Contact Fushun for Nickel Alloy Materials Today

Contact us for more information regarding our nickel alloy material options, or request a quote for further pricing details today. Fushun is your trusted nickel alloy supplier and manufacturer of premium nickel alloy materials.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]