manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Cold Finished Round Steel – Cold Drawn/Rolled

Cold Finished Round Steel – Cold Drawn/Rolled

Cold Finished Round Steel - Cold DrawnRolled

Cold Finished Round Steel – Cold DrawnRolled

Cold Finished Round, Cold Drawn Steel (CDS) and Cold Roll Steel (CRS) Round Bar is a steel product with closer dimensional accuracy, tolerances, and smoother surface finish than hot rolled bar. Cold finished steel Round tend to have higher tensile and yield strength, tighter size tolerances, and improved smoothness when compared to hot finished steel.

These standard shapes can be produced as bar or wire in a wide variety of steel grades including: Carbon Steel, Alloy Steel, Tool Steel, High Speed Steel and Stainless Steel. In addition, these standard shapes can be supplied in custom sizes with special tolerances, finishes and mechanical properties. Precision Kidd can surface improve many of these products to provide elevated surface qualities, such as: “Seam Free” and “Decarb Free,” as well as NDT tested for surface discontinuities.

 

TYPICAL OPERATIONS AND APPLICATIONS USING COLD FINISHED BARS

The below are a few of the many applications using cold drawn bars for their raw material:

Screw machines

CNC lathes

CNC mills

Rotary transfer machining

Hydraulic fittings

Gears

Bushings

Fasteners

Cylinders

Pipe fitting

 

Size Capabilities

Flats: Thickness: 1/8″ through 5″   Widths: 1/8″ through 14″

Squares: from 1/8″ through 5″ (3.175-127mm)

Hexagons: from 1/8″ through 4″

Special Profiles And Shapes: from 1/8″ through 4″

 

Tolerances for Cold Finished Round

Undersize Variations in Inches for both Thickness & Width

Up thru 3/4″ = .002″
over 3/4″ to 1-1/2″ = .003″
over 1-1/2″ to 2-1/2″ = .004″
over 2-1/2″ to 3-1/8″ = .005″

 

Straightness Tolerances for Cold Finished Round

Less than 5/8″ x 5/8″ = +/- 3/16″ in 10ft
5/8″ x 5/8″ and over = +/- 1/8″ in 10ft

 

AVAILABLE LENGTHS:

2ft, 4ft, 6ft, 10-12ft Randoms or Custom Cut
Standard Length Tolerance = +/- 1/4″
Custom Cut Tolerance = +/- 1/16″

FINISH:

Smooth, Oily Finish; Sharp Corners

 

Full Service

In house tool & die production:

CAD Design System

Multiple Wire EDM

Carbide Die Manufacturing

Hardness test and report

Decarb test and report

Shaving, grind and polishing

Controlled atmosphere coil and bar annealing

Eddy Current and Magnetic inspection

Machine straightening

Centerless grinding and polishing

Precision CNC saw cutting

Chamfering

Bundle de-magnetizing

Steel bar coil cleaning and coating

Coil-to-coil surface improvements

Metallurgical laboratory

Coil spooling and oscillate winding

Additional advanced NDT inspection

Quenching and tempering of cold drawn bar

Comprehensive chemical analysis

Multi-pass cold rolling

 

Cross Sectional Dimensions (Profile – Diameter, Thickness, Width)

Size & Sections Standard Tolerance (Inches) Special Tolerance (Inches) Min. Corner Radii (Inches) Max. Surf. Roughness (Feet) Cut Bar Length* (Feet)
Cold Drawn Steel Bar & Wire Rods, Squares, Hexagons (Inches)
.028 to .125
.125 to .4375
.4375 to .750
Over .750 thru 1.50
Over 1.50 to 2.6
Over 2.5 to 3.0
0.001″
0.002″
0.003″
0.003″
0.004″
0.005″
0.0005″
0.001″
0.0015″
0.0015″
0.002″
0.0025″
0.010″
0.015″
0.030″
0.030″
0.030″
0.030″
63 Ra
63 Ra
90 Ra
125 Ra
125 Ra
125 Ra
6′ – 12′
6′ – 20′
10′ – 18′
10′ – 20′
10′ – 20′
10′ – 20′
Cold Drawn Steel Flats (Inches)
Width to .750 – All Thicknesses
Width to .750 thru 3.00
Thickness (Widths .812″ to 5″)
0.002″
0.005″
0.003″
0.0016″
0.0026″
0.002″
0.015″
0.030″
0.030″
90 Ra
125 Ra
125 Ra
10′ – 18′
10′ – 20′
10′ – 20′
Cold Drawn Steel Ground & Polished (Inches)
0.028 to .125
.125 thru .812
Over .750 thru 3.00
0.0006″
0.001″
0.002″
0.0003″
0.0005″
0.001″
NA
NA
NA
20 Ra
20 Ra
32 Ra
10′ – 12′
10′ – 12′
10′ – 20′

 

Material Selection

We are experienced in producing cold drawn steel products in these grades:

Carbon Steels

1006, 1010, 1018, 1035, 1045, 1055, 1060, 1070, 1090, 1095, 1521, 1522, 1541, 1566

Alloy Steels

4023, 4118, 4130, 4140, 4142, 4150, 4320, 4340, 5120, 5160, 52100, 6150, 8620, 8630, 8640, 8650, 9254, 9260, 9310

Tool Steel and High Speed Steels

A-2, D-2, M-1, M-2, M-7, M-50, O-1, S-2, S-2 (Mod. # 1 & Mod. # 4), S-5, S-7, W-1

Stainless Steels

300 and 400 Series and Nitronic, (Inquire Nickel Alloys)

Please inquire regarding other steel grades, end user chemistries and/or specifications.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x