manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

TITANIUM TI6AL4V GRADE 5

TITANIUM GRADE 5

TITANIUM GRADE 5

MATERIAL DESCRIPTION

This alpha-beta alloy is the workhorse alloy of the titanium industry. Titanium grade 5 has good tensile properties at ambient temperature and a useful creep resistance up to 300°C. Resistance to fatigue and crack propagation is excellent. Like most titanium alloys, Grade 5 has outstanding resistance to corrosion in most natural and many industrial process environments.

The ability to age harden this alloy makes it a good choice for such applications as springs and fasteners.

Grade 5, also known as Ti6Al4V, Ti-6Al-4V, Ti 6-4, Ti64 or R56400 is the most commonly used titanium alloy. It has a chemical composition of 6% aluminium, 4% vanadium, 0.25% (maximum) iron, 0.2% (maximum) oxygen, and the remainder titanium. Grade 5 is used extensively in Aerospace, Medical, Marine, and Chemical Processing. It is significantly stronger than commercially pure titanium while having the same stiffness and thermal properties. Among its many advantages, it is heat treatable. This grade has an excellent combination of strength, corrosion resistance, weld and fabricability. In consequence, its uses are numerous such as for military aircraft or turbines. It is also used in surgical implants. Generally, it is used in applications up to 400 degrees Celsius. Its properties are very similar to those of the 300 stainless steel series, especially 316. Ti-6Al-4V is a two phase alpha + beta grade of titanium and is the most widely used of all the titanium grades.

 

APPLICATIONS

Titanium Grade 5 is a pure alpha-beta titanium with aluminum as the alpha stabilizer and vanadium as the beta stabilizer. This alloy is primarily use for corrosion resistance and is the most widely used specification in all product forms. The alloy features very high strength, good corrosion resistance, excellent strength to weight ratio and high strength at cryogenic temperatures.

Weldability

Grade 5 alloy is easily welded in the annealed condition, or in the solution and partially aged condition, with aging being completed during the post weld heat treatment. Precautions must be taken to prevent oxygen, nitrogen, and hydrogen contamination. Fusion welding can be done in inert gas filled chambers, or using inert gas welding of the molten metal and the adjacent heated zones using a trailing shield.

Spot, seam, and flash welding can be performed without resorting to protective atmospheres.

CHEMICAL COMPOSITION

Weight % Al V Fe N C O H Ti
Min. 5,5 3,5
Max. 6,8 4,5 0,25 0,05 0,08 0,2 0,015 BAL.

MECHANICAL PROPERTIES: BAR

Yield strength Rp0.2,

MPa

Tensile strength Rm,

MPa

Elongation

[%]

Hardness

[HRC]

Min. 828 897 10
Max. 910 1000 18 36

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com