AISI 4140 L80 Alloy Steel

AISI 4140 L80 Alloy Steel

AISI 4140 L80 Alloy Steel

Introduce

AISI 4140 80K, PSL 3, API 5CT Standards, NACE MR0175:2015

 

Chemical Composition

Grade C Mn Cr Mo Si P S Ni Cu V H max. ppm
Min. 0.380 0.750 0.800 0.150 0.150 – – – – – –
Max. 0.430 1.000 1.100 0.250 0.350 0.025 0.025 0.250 0.300 0.300 2.000

 

Heat Treatment

Austenizing temperature Time Tempering temperature Time
1600 ±25℉

(871 ±14℃)

Min. 60 minutes 1250 ±50℉

(677 ±27℃)

Min. 60 minutes

Oil or Polymer or Water. For Water Quenching, the temperature of water shall not exceed 38℃ (100℉) at start of quench. For bath-type quenching, the temperature of water shall not exceed 49℃(120℉) at any time during the quench cycle.

Mechanical Properties

as per ASTM A370 -20

Yield strength

 

Tensile strength minimum Elongation in

2” (minimum)

Reduction Area

(minimum)

Min. 80,000 psi (552 MPa)

Max. 95,000 psi (655 MPa)

100,000 psi (690 MPa) 18% 35%

 

Quality Inspection

  • Specimen test location & QTC
  • Charpy V-notch impact at 21℃ / -32℃ / -60℃
  • Hardness as per ASTM E10-18: On surface / 1”below surface
  • Volumetric NDE 100% – Ultrasonic
  • Minimum hot work reduction ratio 4.0 to 1
  • Grain size should be #S or Finer as per ASTM E112 – 13
  • Surface inspection

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x