manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

1.4742, X10CrAlSi18, Heat Resisting Ferritic Steel

1.4742, X10CrAlSi18, Heat Resisting Ferritic Steel

Super Duplex F55 S32760 Stainless Steel

1.4742, also known as X10CrAlSi18, represents a distinguished heat-resisting ferritic steel within Fushun’s product portfolio. Recognized for its exceptional resistance to high temperatures, this steel grade is an optimal choice for applications demanding sustained thermal endurance. Its robust corrosion resistance, mechanical properties, and precision manufacturing make it a reliable selection for critical uses in heat exchangers, furnace components, and exhaust systems. Should you require further information about this steel grade or related products, please do not hesitate to reach out to us; we stand ready to assist you.

Our Supply

Smelting line: VIM,VAR, IM, ESR, PESR, LF, VD, AOD

Danieli roll line: round & flat diameter 150mm max

Forged line: 800mm max

Heat-treatment line: annealed, quenched tempered, solution

Machining line: Turning, Milling, CNC

Chemical Composition

Name Number C Si Mn max P max S max Cr Al
X10CrAlSi18 1.4742 max 0.12 0.7-1.4 1.00 0.04 0.015 17-19 0.7-1.2

 

 

Mechanical Properties

Name Number Heat condition Hardness HB max Proof strength Tensile strength
X10CrAlSi18 1.4742 +A annealed 212 270 500-700

 

 

Our advantage of heat resisting steel

  • High creep limit and lasting strength;
  • Easy smelting and processing and good casting, forging and welding properties;
  • high oxidation resistance and corrosion resistance;
  • high high-temperature mechanical properties;
  • Small expansion coefficient and good thermal conductivity;
  • Good processability and economy.
  • Organization stability at high temperature
  • Low cost

What is heat resisting steel?

Heat resisting steel is a kind of special steel that can maintain good mechanical properties and antioxidant properties under high temperature environment. It has high temperature stability, oxidation resistance and creep resistance, can maintain high strength and hardness at high temperatures, not easy to soften and deformation.

 

Why choose heat resisting steel?

1. High-temperature stability:

heat resisting steel at high temperatures to maintain high strength and hardness, will not occur obvious softening and deformation.

 

2. Antioxidant properties:

heat resisting steel surface to form a dense layer of oxide film, can effectively prevent oxidation reaction, slow down the oxidation rate of the material.

 

3. Creep resistance:

heat resisting steel at high temperatures can resist plastic deformation and creep phenomenon, to maintain good shape stability and dimensional accuracy.

 

4. Good processing performance:

heat resisting steel has good plasticity and weldability, can be convenient for hot processing and welding.

 

 

Application of heat resisting steel

heat resisting steel is widely used in aerospace, energy, chemical industry and other fields, mainly including the following aspects:

1. Aerospace field:

heat resisting steel used in the manufacture of aero-engine turbine blades, turbine discs, combustion chambers and other components, as well as aerospace spacecraft insulation materials.

 

2. Energy field:

heat resisting steel used in the manufacture of thermal power plant boiler supercritical and ultra-supercritical boiler piping and heating surface, and nuclear power plant nuclear reactor pressure vessel and fuel components.

 

3. Chemical industry:

heat resisting steel is used in the manufacture of chemical equipment reactor, separator, oil cracker pipeline, etc., which can withstand high temperature, high pressure and corrosive media.

 

4. Other fields:

heat resisting steel is also widely used in metallurgy, machinery, automobile and other fields, used in the manufacture of a variety of parts and tools under high-temperature working environment.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x