4340 ALLOY STEEL – AMS 6414 VAR – UNS G43406

4340 ALLOY STEEL – AMS 6414 VAR – UNSG43406

 

4340 VAR AMS 6414 is a low alloy Chromium-Nickel-Molybdenum steel capable of being heat treated to high strength levels.

 

This specification is for a premium aircraft-quality, low-alloy steel in the form of bars, forgings, mechanical tubing, and forging stock. Service Steel Aerospace stocks Premium Aircraft Quality produced double melted in an Electric Furnace, followed by VAR, or Vacuum Arc Remelt (also known as CEVM, or Consumable Electrode Vacuum Arc Remelting). This results in a much cleaner steel meeting the magnetic particle test requirements of AMS-2300.

 

It is a steel of the highest quality with excellent transverse ductility and toughness at high strength levels. It has good shock and impact resistance as well as wear and abrasion resistance in the hardened condition. Standard Aircraft Quality air-melted AMS 6414 Air Melt material is available on request. 4340 ESR, or Electroslag Remelted material is also available on request.

<<AMS 4340 DATA SHEET PDF>>

4340 alloy steel applications:

4340 has been used typically for parts requiring a through-hardening capability up to 3.5 inches (89 mm) in nominal thickness at time of heat treatment and subject to rigid magnetic particle inspection standards, but usage is not limited to such applications. Premium Aircraft Quality is intended for use in the manufacturing of highly stressed parts at higher strength levels, such as 260/280,000 psi and where a much cleaner steel is desired.

 

Chemical Composition:

Symbol Element Min % Max %
C Carbon 0.38% 0.43%
Mn Manganese 0.65% 0.90%
Si Silicon 0.15% 0.35%
P Phosphorus 0.01%
S Sulfur 0.01%
Cr Chromium 0.70% 0.90%
Ni Nickel 1.65% 2.00%
Mo Molybdenum 0.20% 0.30%
Cu Copper 0.35%

 

Mechanical Properties:

Bar Size Temperature * Tensile Strength Yield Strength Elongation in 2″ Reduction of Area
3.5″ Dia. 400° F (204° C) 276 ksi 222 ksi 11.0% 35.0%
7.5″ Dia. 500° F (260° C) 265 ksi 222 ksi 8% 25.0%
10.5″ Dia. 1100° F (593° C) 165 ksi 150 ksi 18% 60.0%

* After Normalized 1650°/1700° F, Austenized 1500°/1525° F, Oil quenched

 

Common Trade Names:

Lescalloy 4340 Vac-Arc

European Designation 36CrNiMo4

4340 Chrome-Nickel-Molybdenum Steel

SAE 4340

AISI 4340

4340 CEVM

4340 ESR

 

4340 VAR AMS 6414 Common Specifications:

AMS 6414 VAR (CEVM)

AMS 6414 ESR

AMS 6415 (Air Melt)

AMS 6409

MIL-S-5000, AMS-S-5000 (Both are cancelled and superseded by AMS 6415)

MIL-S-8844

299-947-055 Bell Helicopter

SS 9702 Sikorsky

DMS 1555 Boeing (Previously McDonnell Douglas)

HMS 6-1121 (for 4340 ESR Only)

BPS 4807 (for 4340 ESR Only)

 

We also supply
MARS190 D6AC AMS 4130
AMS 4340 MOD AMS 4340 AMS 4330 MOD
AMS 9310 AMS 13-8 PH AMS 15-5 PH
AMS 17-4 PH AMS 625 AMS 718
AerMet® 100 Maraging 250 Maraging 300
Maraging 350 Titanium Grade 5 Ti-6Al-4V ELI Titanium

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x