Available Inventory for Sale: 7CrMoVTiB10-10 1.7378 High-Temperature Steel

Available Inventory for Sale: 7CrMoVTiB10-10 1.7378 High-Temperature Steel

Introduce

7CrMoVTiB10-10 1.7378  refers to a specific type of high-temperature steel, primarily used in the construction of boilers, pressure vessels, and power plant equipment where high temperature and pressure resistance is crucial. This steel is part of the group of steels known as “bainitic chromium-molybdenum steels” with added titanium and boron.

 

Size and Quantity

Round bar diameter 88.5 mm; length 2200mm; total weight 2.5 tons

 

Chemical component

C Si Mn P S Cr Mo V Ti Al N B
0.05-0.10 0.15-0.45 0.3-0.7 0-0.02 0-0.01 2.2-2.6 0.9-1.1 0.2-0.3 0.05-0.1 0-0.02 0-0.01 0.0015-0.007

 

Smelting

EAF+AOD+LF+VD

 

Process

Hot rolled+Annealed+Grounded

 

Macrostructure

Ordinary Porosity:0.5/0.5

Center Porosity:0.5/0.5

Ingot Segregation:0/0

 

Non-Metallic Inclusions

AT:0/0

AH:0/0

BT:1.5/1.5

BH:0/0

CT:0/0

CH:0/0

DT:1.0/1.0

DH:0/0.5

 

Ultrasonic Inspection

Qualified

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x