manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

High Temperature Bolt Steel

High Temperature Bolt Steel

High Temperature Bolt Steel

Introduction

High temperature bolt steel is a specialized material designed for applications requiring high strength and excellent creep resistance at elevated temperatures. These steels are specifically engineered to maintain their mechanical properties under sustained loads at high temperatures, typically ranging from 400°C to 650°C.

FUSHUN METAL regularly produces and maintains stock of heat and creep resistant materials used for turbine bolts, valve components and other high temperature applications. We have over 400 tonnes of material in stock ranging from 16mm diameter through to 350mm diameter with some grades in square, flat, hexagon & sheet.

We manufacture the following dimensions:

Diameter: 20 – 1200 mm

Applications

  • Steam turbine bolting applications
  • Gas turbine fasteners
  • High-temperature pressure vessel connections
  • Nuclear power plant components
  • Industrial furnace equipment
  • Petrochemical plant fasteners
  • High-temperature valve components
  • Power generation equipment
  • Heat exchanger assemblies

Standards

  • ASTM A193 Alloy Steel and Stainless Steel Bolting Materials for High Temperature Service
  • ASTM A1082 High Strength Precipitation Hardening and Duplex Stainless Steel Bolting for Special Purpose Applications
  • EN 10269 Steels and nickel alloys for fasteners with specified elevated low temperature
  • DIN 17240 Quality specifications for heat-resistant and high-heat-resistant materials for bolts and nuts
  • GB/T 20410 Steel for turbine high temperature bolts
  • ASTM A437 Stainless and Alloy Steel Turbine Type Bolting Specially Heat Treated for High-Temperature

Grade List

Standard Grade Temperature Range Main Applications
ASTM A193 B5,B6,B7,B16,B8,B8CA(347),304N,316N,321,etc Up to 525°C General purpose high temperature bolting
DIN 17240 24CrMo5, 1.7258, 21CrMoV5-7, 1.7709, 40CrMoV4-7, 1.7711, X22CrMoV12-1, 1.4923, X19CrMoVNb11-1, 1.4913, X8CrNiMoBN16-16, 1.4986, NiCr20TiAl, 2.4952 Up to 450°C Pressure vessel bolting
EN 10269 25CrMo4, 1.7218, 42CrMo4, 1.7225, 42CrMo5-6, 1.7233, 40CrMoV4-6, 1.7711, 27NiCrMoV15-6, 1.6957, 26 NiCrMo 14-6, 1.6958, 21CrMoV5-7, 1.7709, 20CrMoVTiB4-10, 1.7729, 34CrNiMo6, 1.6582, 30CrNiMo8, 1.6580, X12Ni5, 1.5680, X8Ni9, 1.5662X15CrMo5-1, 1.7390, X22CrMoV12-1, 1.4923, X12CrNiMoV12-3, 1.4938, X19CrMoNbVN11-1, 1.4913, X2CrNi18-9, 1.4307, X5CrNi18-10, 1.4301, X4CrNi18-12, 1.4303, X2CrNiN18-10, 1.4311, X6CrNi25-20, 1.4951, X2CrNiMo17-12-2, 1.4404, X5CrNiMo17-12-2, 1.4401, X2CrNiMoN17-13-3, 1.4429, X3CrNiCu18-9-4, 1.4567, X6CrNi18-10, 1.4948, X10CrNiMoMnNbVB15-10-1, 1.4982, X3CrNiMoBN17-13-3, 1.4910 Up to 540°C Steam turbine bolting
GB/T 20410 35CrMoA, 42CrMoA, 21CrMoVA, 35CrMoVA, 40CrMoVA, 20Cr1Mo1VA, 45Cr1MoVA, 20Cr1Mo1V1A, 25Cr2MoVA, 25Cr2Mo1VA, 40Cr2MoVA, 18Cr1Mo1VTiB, 20Cr1Mo1VTiB, 20Cr1Mo1VNbTiB, 2Cr12MoV, 2Cr12NiMo1W1V, 2Cr11NiMoNbVN, 2Cr11Mo1VNbN, 1Cr11MoNiW1VNbN Up to 650°C Turbine bolting applications
*For more detailed technical specifications, please contact us.

Manufacturing Process

The steel be produced by the following processes: electric-furnace, ESR electroslag remelting or vacuum-induction melting (VIM). The molten steel may be vacuum-treated prior to or during pouring of the ingot or strand casting.

Inspection & quality control

Every forging manufactured by FUSHUN METAL is fully inspected by our inspectors and when accepted given a coat of anti-rust protection and packed for transport. Every forging is supplied with a certificate of conformity and dimensional report. The certificate of conformity contains the results of all the mechanical tests, chemical analysis and heat treatment cycles. NTD and test reports will be also provided.

High-Temperature Tests

Tests to determine high temperature properties shall be made in accordance with Test Methods E21, E139, and 292 and Practices E150 and E151.

Charpy Impact Tests

Charpy impact tests based on the requirements of Specification A 320/A 320M Sections 6 and 7

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.