1.4906 (X12CrMoWVNbN10-1-1) Turbine Blade Steel

 

1.4906 (X12CrMoWVNbN10-1-1) Turbine Blade Steel

Professional Steel Manufacturer – FUSHUN SPECIAL STEEL

Steel Grade Introduction and Applications

FUSHUN SPECIAL STEEL specializes in manufacturing 1.4906 (X12CrMoWVNbN10-1-1) turbine blade steel, a premium martensitic stainless steel engineered for the most demanding power generation applications. This advanced steel grade is specifically designed for high-pressure steam turbine blades, rotors, and critical components in both conventional and nuclear power plants.

As a leading steel manufacturer, FUSHUN SPECIAL STEEL provides 1.4906 steel with exceptional high-temperature strength (Rp0.2 ≥ 750 N/mm² at room temperature) and superior creep resistance at temperatures up to 600°C. Our fully martensitic microstructure after heat treatment ensures optimal performance in the most challenging power generation environments.

This steel grade is equivalent to T505SC (Japanese standard) and is used extensively in steam turbine blades, rotors, and high-temperature fasteners. The material demonstrates excellent long-term creep resistance and maintains structural integrity under extreme operating conditions.

We welcome large-volume orders and provide comprehensive manufacturing solutions for power generation industry clients worldwide.

Chemical Composition

Element C Si Mn Cr Mo W V Nb N
Content % 0.11-0.13 ≤0.12 0.40-0.50 10.2-10.8 1.00-1.10 0.95-1.05 0.15-0.25 0.04-0.06 0.045-0.060

FUSHUN SPECIAL STEEL maintains strict quality control with melt analysis for all specified elements, ensuring precise chemical composition meeting international turbine blade steel standards.

Available Processing Types

Hot Rolled

FUSHUN SPECIAL STEEL provides hot rolled 1.4906 steel with superior surface quality and dimensional accuracy. Our hot rolling process ensures optimal microstructure for turbine blade applications with controlled grain size (ASTM 4 or finer).

Hot Forged

Our advanced forging capabilities produce high-strength 1.4906 components with refined grain structure and fully martensitic microstructure. Forging temperature range 1100-900°C ensures optimal mechanical properties for turbine applications.

Available Shapes and Forms

Round Bars

Precision round steel bars for turbine shafts and rotors

Flat Bars

High-quality flat steel for turbine blade blanks

Plates

Steel plates for large turbine components

Tubes

Seamless tubes for high-pressure steam applications

Size Capabilities and Dimensions

Hot Rolled Rounds

Maximum diameter: 260mm

Ultrasonic testing for bars ≥30mm diameter per EN 10308

Forged Products

Maximum diameter: 1200mm

Large-scale forging for turbine rotors and critical components

Precision Machining

Ultra-precise dimensions available

In-house turning and grinding capabilities for turbine blade applications

Mechanical Properties

Room Temperature Properties

Property 0.2% Proof Strength (MPa) Tensile Strength (MPa) Elongation (%) Impact Energy (J) Hardness (HB)
1.4906 750-830 870-1020 ≥14 ≥55 270-310

High Temperature Performance (600°C)

Property 0.2% Proof Strength (MPa) Tensile Strength (MPa) Elongation (%) Reduction of Area (%)
1.4906 at 600°C ≥405 ≥420 ≥18 ≥65

Creep and Rupture Properties

Creep Rupture Strength at 600°C:

10,000 hours: ≥100 MPa

100,000 hours: ≥80 MPa (estimated)

Creep Rate: Typically <1×10⁻⁷ %/h at 600°C under 100 MPa stress

Heat Treatment Capabilities

Hardening Process

Temperature: 1050-1100°C

Quenching: Air or liquid cooling

Must be cooled to ≤100°C for complete martensitic transformation

Double Tempering

First temper: 570-680°C

Second temper: 680-720°C

Final condition: Quenched and Tempered (+QT)

FUSHUN SPECIAL STEEL operates advanced heat treatment facilities with precise temperature control ensuring optimal martensitic microstructure and mechanical properties.

FUSHUN SPECIAL STEEL Manufacturing Advantages

In-House Heat Treatment

Complete heat treatment facilities with precise control ensure fully martensitic microstructure and stable quality for turbine applications.

Precision Machining

Advanced turning and grinding capabilities reduce downstream processing time and costs for turbine blade manufacturers.

Quality Assurance

Comprehensive testing including ultrasonic testing, creep rupture testing, and elevated temperature tensile tests ensuring turbine-grade quality.

Large Volume Manufacturing

As a professional steel manufacturer, we welcome large-scale orders for power generation industry with competitive pricing and reliable delivery.

Contact FUSHUN SPECIAL STEEL today for your 1.4906 turbine blade steel requirements. We specialize in large-volume manufacturing with superior quality, complete testing certification, and competitive delivery times for the power generation industry.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x