manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

1.3344, M3 CI2, Spray Forming High Speed Steel

1.3344 Spray Forming High Speed Steel – Premium Tool Steel from FUSHUN SPECIAL STEEL

Steel Grade Introduction and Applications

1.3344 is a premium high-vanadium tungsten-molybdenum spray forming high speed steel grade that delivers exceptional performance for the most demanding cutting applications. This advanced high speed steel manufactured using cutting-edge spray forming technology offers superior red hardness, excellent wear resistance, and outstanding toughness. The spray forming process creates an ultra-fine microstructure with homogeneous carbide distribution, resulting in significantly enhanced tool performance and extended service life.

As a leading manufacturer, FUSHUN SPECIAL STEEL specializes in producing high-quality 1.3344 spray forming steel for high-performance cutting tools, precision machining applications, and demanding industrial components in aerospace, automotive, and advanced manufacturing sectors.

Spray Forming Process Advantages

Process Features:

  • Rapid Solidification: Ultra-fast cooling creates refined microstructures
  • Homogeneous Structure: Eliminates macro-segregation completely
  • Near-Net Shape: Reduces material waste by 30-40%
  • Enhanced Properties: Superior mechanical performance

Performance Benefits:

  • Exceptional Hardness: Superior cutting edge retention
  • Outstanding Toughness: Reduced tool breakage risk
  • Uniform Carbides: Consistent particle distribution
  • Extended Tool Life: Outstanding wear resistance

1.3344 Chemical Composition (wt%)

Element C Cr W Mo V Co
1.3344 1.3 4 6 5 3 –

Note: Equivalent to M3 Cl2, optimized chemical composition for spray forming process to achieve superior microstructural uniformity and enhanced performance characteristics

Physical Properties at Different Temperatures

Property 20°C 400°C 600°C
Density (kg/m³) 8150 8050 8030
Elastic Modulus (MPa) 235,000 210,000 188,000
Thermal Expansion (×10⁻⁴/°C) – 11.4 11.8
Thermal Conductivity 26 30 29
Specific Heat (J/kg·°C) 410 495 580

Heat Treatment Process for 1.3344

Softening Annealing

  • Temperature: 870-900°C
  • Hold time: 4-6 hours
  • Cool to 600°C in furnace
  • Hardness: ≤280HB

Stress Relief

  • Temperature: 600-700°C
  • Hold time: 4 hours
  • Slow cooling
  • After rough machining

Hardening

  • Preheat: 450-500°C
  • Austenitize: 1200-1230°C
  • Quench in air/oil/salt
  • Hardness: 65-67 HRC

Tempering

  • Temperature: 540-580°C
  • Multiple cycles (2-3x)
  • Hold time: 1-2 hours each
  • Air cooling

Recommended Heat Treatment for Different Tools:

Tool Type Hardening Temp (°C) Tempering Temp (°C) Final Hardness (HRC)
Single Point Tools 1220 540-560 65-66
Multi Point Tools 1200-1220 550-570 64-65
Dies & Punches 1170-1200 560-580 62-64

Available Forms and Specifications

Coils & Strips

  • Thickness: 0.1-4.0mm
  • Width: 10-800mm
  • Precision tolerance control
  • Custom slitting available

Round Bars

  • Diameter: 8-350mm
  • Length: up to 6000mm
  • Ground or turned finish
  • Straightness guaranteed

Plates & Flats

  • Thickness: 4-120mm
  • Width: up to 2500mm
  • Length: up to 6000mm
  • Surface finish options

Squares & Special Shapes

  • Square: 12-250mm
  • Rectangular profiles
  • Custom dimensions
  • Near-net-shape forming

Applications of 1.3344 Spray Forming Steel

High-Performance Cutting Tools

End mills, milling cutters, drill bits, gear cutters, hobbing tools

Industrial Knives

Steel cutting blades, shear blades, slitting knives

Forming Tools

Cold forming punches, dies, extrusion tools

Precision Components

Aerospace parts, automotive components, wear plates

1.3344 Spray Forming vs Conventional Steel Performance

Property Conventional 1.3344 Spray Forming 1.3344 Improvement
Hardness 63-65 HRC 65-67 HRC +3-5%
Wear Resistance Standard Excellent +35-50%
Toughness Good Superior +20-35%
Red Hardness 60-62 HRC@600°C 62-64 HRC@600°C +3-5%
Tool Life Baseline Extended +40-60%
Carbide Uniformity Acceptable Excellent +60-80%

Technical Advantages of 1.3344 Spray Forming

Steel Properties:

  • Superior wear resistance: Uniform carbide distribution
  • Exceptional red hardness: High temperature performance
  • Enhanced toughness: Reduced tool breakage
  • Excellent machinability: Easier processing
  • Uniform structure: Consistent properties

Manufacturing Benefits:

  • Near-net shape: Minimal material waste
  • Cost effective: Reduced processing costs
  • Better surface finish: Reduced finishing time
  • Dimensional accuracy: Tighter tolerances
  • Shorter lead times: Faster delivery

Quality Assurance & Certifications

ISO Certified

International quality standards compliance

Material Testing

Complete chemical & mechanical analysis

Traceability

Full material certificates provided

Technical Support

Expert guidance & application support

Important Notes & Recommendations

1. Material Selection: 1.3344 is ideal for high-performance cutting applications requiring excellent wear resistance and red hardness.

2. Machining: Use appropriate cutting parameters and coolants to maximize tool life during machining operations.

3. Heat Treatment: Follow precise heat treatment procedures to achieve optimal hardness. Spray forming steel typically requires slightly adjusted parameters.

4. Storage: Store in dry, controlled conditions to prevent corrosion and maintain surface quality.

About FUSHUN SPECIAL STEEL

FUSHUN SPECIAL STEEL is a leading manufacturer specializing in high-quality 1.3344 spray forming high speed steel production. With decades of experience in metallurgy and advanced manufacturing technologies, we provide superior steel products to customers worldwide. Our state-of-the-art spray forming technology ensures exceptional quality and performance that exceeds industry standards.

Our commitment to innovation and quality has made us a trusted partner for industries requiring premium tool steels. We continuously invest in research and development to improve our production processes and deliver products that exceed customer expectations in performance and reliability.

Advanced Technology

State-of-the-art spray forming equipment

Global Supply

Worldwide shipping and distribution

Custom Solutions

Tailored products for specific applications

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x