manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Precipitation Hardening Stainless Steel Manufacturer

Precipitation Hardening Stainless Steel

17-4PH / 15-5PH / 17-7PH Precision-Cut, Mill-Certified, Ready to Ship

AS9100D & ISO 9001:2015 Certified  ·  Ex-Stock & Custom Sizes  ·  Global Delivery in 15–30 Days

From aerospace fasteners & landing gear pins to medical device shafts, oil & gas pump components, and marine seawater pump housings — we supply PH stainless in the exact grade, aging condition, and tolerance your application demands. 12 grades in stock. Mill Test Reports (EN 10204 3.1) with every shipment.

AS9100D ISO 9001:2015 EN 10204 3.1 MTR AMS · ASTM · EN · JIS VIM / VAR Available
🇺🇸 USA 🇩🇪 Germany 🇯🇵 Japan 🇸🇦 GCC 🇬🇧 UK 🇫🇷 France 🇦🇺 Australia

PH Stainless Steel Grade Portfolio

12 precipitation hardening grades — martensitic, semi-austenitic, and ultra-high-strength custom alloys. Full standard and custom melts available.

Most Popular
17-4PH UNS S17400
AMS 5643 · ASTM A564 Gr.630 · EN 1.4542 · SUS630
Peak Hardness≤44 HRC (H900)
UTS (H900)≥1310 MPa
Cond.AH900H1025H1075H1150H1150M

Aerospace structural fasteners, landing gear components, oil & gas pump shafts, nuclear containers, food processing equipment. Workhorse PH grade — single-step aging, excellent machinability in Condition A.

15-5PH UNS S15500
AMS 5659 · ASTM A564 XM-12 · EN 1.4545
Peak Hardness≤44 HRC (H900)
UTS (H900)≥1310 MPa
H900H925H1025H1075H1150

Aircraft bulkheads & forgings, turbine components, heavy-section bars & discs. VIM+VAR melt — reduced delta-ferrite vs. 17-4PH ensures consistent through-thickness properties in large cross-sections.

17-7PH UNS S17700
AMS 5528/5529 · ASTM A693 Gr.631 · EN 1.4568 · SUS631
Peak Hardness≤48 HRC (CH900)
UTS (CH900)≥1655 MPa
Cond.ACH900TH1050RH950

Aerospace springs, diaphragms & bellows, precision flat parts, high-cycle fatigue components. Semi-austenitic; Al-hardened strip & wire achieves UTS >1655 MPa. Superior fatigue performance vs. 17-4PH in thin sections.

PH13-8Mo UNS S13800
AMS 5629 · ASTM A564 XM-13 · EN 1.4534 · X3CrNiMoAl13-8-2
Peak Hardness≥43 HRC (H950)
UTS (H950)≥1448 MPa
H950H1000H1050H1100H1150

Aircraft structural parts, landing gear, high-stress missile airframes. Mo+Al hardening delivers outstanding KIc fracture toughness at strength levels unavailable in 17-4PH. VIM+VAR melt required per AMS 5629.

PH14-8Mo UNS S14800
EN 1.4535 · NAS 14-8Mo · X3CrNiMoAl14-8-2
Peak Hardness≤47 HRC (SRH950)
TypeSemi-austenitic
SRH950CH900TH1050

Aerospace structural members, chemical-resistant high-strength fasteners. Similar to 17-7PH but Mo addition provides enhanced chloride SCC resistance; preferred in aggressive marine and chemical environments.

15-7PH UNS S15700
AMS 5520 · ASTM A693 Gr.632 · EN 1.4532 · SUS632J1
Peak Hardness≤48 HRC (CH900)
UTS (CH900)≥1655 MPa
Cond.ACH900TH1050RH950

Springs, high-strength strip & washers, aerospace defense components. Combines 15-5 corrosion resistance with 17-7 semi-austenitic hardenability. Mo addition improves pitting resistance over 17-7PH.

AM-350 UNS S35000
AMS 5548/5549 · ASTM A693 Gr.350
Peak Hardness≤47 HRC (SCT850)
TypeSemi-austenitic
Cond.ASCT850DA

Aerospace structural sheet, pressure vessels, rocket motor cases. Very high strength-to-weight ratio; good oxidation resistance to 315°C. Weldable in annealed condition with low-hydrogen process.

AM-355 UNS S35500
AMS 5547/5548 · ASTM A693 Gr.355
Peak Hardness≤49 HRC (SCT850)
TypeSemi-austenitic
Cond.ASCT850DA

Missile & space vehicle structures, gas turbine blades. Higher Ni content vs. AM-350 for improved cryogenic toughness. Superior high-temperature creep strength and retention of mechanical properties to 370°C.

Custom 455® UNS S45500
AMS 5578 · XM-16 · EN 1.4543 · X12CrNiCuTi12-8-3
Peak Hardness≤49 HRC (H900)
UTS (H900)≥1655 MPa
H900H950H1000

Ultra-high-strength aircraft bolts, structural airframe parts, precision shafting. Ti+Cu aging at low temperature; excellent notch toughness at H900. Low-temperature aging minimizes quench distortion.

Custom 465® UNS S46500
AMS 5936 · EN 1.4614 · X11CrNiMoTi11-11-1
Peak Hardness≤52 HRC (H900)
UTS (H900)≥1930 MPa
H900H950H1000

Next-gen aircraft structures, high-pressure vessels, critical shafting. Highest-strength PH stainless commercially available; KIc ≥110 MPa√m in H950 — exceptional balance of strength and fracture toughness.

Custom 475® UNS S47500
AMS (in qualification)
Peak Hardness≤54 HRC (H900)
UTS (H900)>1965 MPa
H900H950

Emerging aerospace structural and landing gear applications. Ultra-high-strength PH grade with improved SCC resistance over Custom 455®; targets aerospace qualification per AMS 2369.

Custom 450® UNS S45000
XM-25 · EN 1.4594 · SUS 630J1 · X5CrNiMoCuNb14-5
Peak Hardness≤33 HRC (H900)
UTS (H900)≥1034 MPa
H900H950H1000H1100

Chemical process equipment, pumps, machinability-enhanced alternative to 17-4PH. Moderate strength with better corrosion resistance in acidic and chloride media. Excellent weldability in all conditions.

Technical Specifications

Chemical composition and mechanical properties per ASTM / AMS / EN international standards. Full MTR data available with every shipment.

17-4PH (UNS S17400) — AMS 5643 Rev. N  ·  ASTM A564/A564M Grade 630  ·  EN 1.4542

Table A — Chemical Composition (wt.%)

LimitCMnSiPSCrNiCuNb+TaFe
Min—————15.003.003.000.15Bal.
Max0.071.001.000.0400.03017.505.005.000.45Bal.

Data per AMS 5643 Rev. N, ASTM A564/A564M. N ≤ 0.10% per AMS 5643. No intentional Mo, Ti, Al additions.

Table B — Minimum Mechanical Properties (Bar/Rod — AMS 5643 / ASTM A564)

ConditionAging TreatmentUTS min (MPa)0.2% YS min (MPa)El. min (%)RA min (%)Hardness (HRC)
Cond. ASolution anneal, as-supplied≥1069≥793≥8—≤38
H900482°C / 900°F, 1 h, AC≥1310≥1170≥10≥4040–47
H925496°C / 925°F, 4 h, AC≥1172≥1103≥10≥4438–43
H1025552°C / 1025°F, 4 h, AC≥1069≥1000≥12≥4533–38
H1075579°C / 1075°F, 4 h, AC≥1000≥862≥13≥4531–36
H1100593°C / 1100°F, 4 h, AC≥965≥793≥14≥4529–34
H1150621°C / 1150°F, 4 h, AC≥931≥724≥16≥5028–34
H1150M760°C/2 h + 621°C/4 h (double age)≥862≥655≥18≥5526–32

Minimum values per AMS 5643 Rev. N & ASTM A564/A564M for bar, rod & shapes. AC = Air Cool. Certified test results on MTR (EN 10204 3.1) supplied with each shipment.

15-5PH (UNS S15500) — AMS 5659  ·  ASTM A564/A564M Grade XM-12  ·  EN 1.4545

Table A — Chemical Composition (wt.%)

LimitCMnSiPSCrNiCuNb+TaFe
Min—————14.003.502.500.15Bal.
Max0.071.001.000.0400.03015.505.504.500.45Bal.

Data per AMS 5659, ASTM A564/A564M. N ≤ 0.05% per AMS 5659. Produced via VIM+VAR for reduced delta-ferrite and improved transverse properties in heavy sections.

Table B — Minimum Mechanical Properties (Bar/Rod — AMS 5659 / ASTM A564)

ConditionAging TreatmentUTS min (MPa)0.2% YS min (MPa)El. min (%)RA min (%)Hardness (HRC)
H900482°C / 900°F, 1 h, AC≥1310≥1170≥10≥4040–47
H925496°C / 925°F, 4 h, AC≥1172≥1103≥10≥4438–43
H1025552°C / 1025°F, 4 h, AC≥1069≥1000≥12≥4533–38
H1075579°C / 1075°F, 4 h, AC≥1000≥862≥13≥4531–36
H1100593°C / 1100°F, 4 h, AC≥965≥793≥14≥4529–34
H1150621°C / 1150°F, 4 h, AC≥931≥724≥16≥5028–34

Minimum values per AMS 5659 & ASTM A564/A564M. VIM+VAR melt ensures minimal delta-ferrite — ideal for forgings and thick bar >150 mm dia. Full MTR (EN 10204 3.1) with each shipment.

17-7PH (UNS S17700) — AMS 5528 (strip/sheet) · AMS 5529 (bar/rod)  ·  ASTM A693 Grade 631  ·  EN 1.4568

Table A — Chemical Composition (wt.%)

LimitCMnSiPSCrNiAlFe
Min—————16.006.500.75Bal.
Max0.091.001.000.0400.04018.007.751.50Bal.

Data per AMS 5528/5529, ASTM A693 Grade 631. Semi-austenitic PH grade; Al replaces Cu/Nb as hardening agent. No intentional Nb, Cu, Mo, or Ti additions.

Table B — Minimum Mechanical Properties (Strip/Sheet — AMS 5528 / ASTM A693)

ConditionTreatment SequenceUTS min (MPa)0.2% YS min (MPa)El. min (%)Hardness
Cond. ASolution anneal 1065°C, rapid cool≥1035≥276≥20≤92 HRB
CH900Cold-work to Cond. C + age 482°C/1 h≥1655≥1590≥6≥47 HRC
TH1050955°C/1 h + sub-zero + 565°C/90 min≥1240≥1030≥9≥38 HRC
RH950Cond. A + −73°C/8 h + 510°C/1 h, AC≥1448≥1310≥6≥43 HRC

Data per AMS 5528 Rev. F (strip/sheet) & ASTM A693 Gr. 631. CH900 requires prior cold work to "C" condition. Bar/rod properties per AMS 5529. Full MTR with each shipment.

PH13-8Mo (UNS S13800) — AMS 5629  ·  ASTM A564/A564M Grade XM-13  ·  EN 1.4534

Table A — Chemical Composition (wt.%)

LimitCMnSiPSCrNiMoAlFe
Min—————12.257.502.000.90Bal.
Max0.050.100.100.0100.00813.258.502.501.35Bal.

Data per AMS 5629, ASTM A564 Grade XM-13. Stringent C ≤0.05%, Mn ≤0.10%, Si ≤0.10% maximize cleanliness and toughness. VIM+VAR double-melt mandatory per AMS 5629.

Table B — Minimum Mechanical Properties (Bar/Rod/Forgings — AMS 5629 / ASTM A564)

ConditionAging TreatmentUTS min (MPa)0.2% YS min (MPa)El. min (%)RA min (%)Hardness (HRC)
H950510°C / 950°F, 4 h, AC≥1448≥1310≥10≥50≥43
H1000538°C / 1000°F, 4 h, AC≥1310≥1207≥12≥5540–44
H1050566°C / 1050°F, 4 h, AC≥1172≥1069≥14≥5537–42
H1100593°C / 1100°F, 4 h, AC≥1069≥1000≥15≥6033–38
H1150621°C / 1150°F, 4 h, AC≥965≥862≥16≥6030–35

Per AMS 5629, ASTM A564 Grade XM-13. Mo addition provides KIc fracture toughness 30–50% higher than 17-4PH at equivalent strength. Recommended for fatigue-critical and damage-tolerant designs. Full MTR with each shipment.

Available Forms & Sizes

All 12 grades available in standard mill product forms — stock and custom dimensions to specification

Product FormStandard Size RangeTolerancesSurface / Finish
⬤ Round Bar Ø6 mm – Ø500 mm (¼" – 20")
Length: up to 6,000 mm
h9–h11 (hot-rolled)
h6 (centreless-ground)
Hot-rolled · Peeled · CNC-turned · Centreless-ground · Polished
▬ Flat Bar Thickness: 6–200 mm · Width: 20–600 mm
Length: up to 6,000 mm
Per EN 10278 / ASTM A484 Hot-rolled · Machined flat · Ground
▪ Plate / Sheet Thickness: 3–100 mm · Width: up to 1,500 mm
Length: up to 6,000 mm
Per ASTM A480 / EN 10029 Hot-rolled annealed (No.1) · Plasma/shear cut
〰 Strip / Coil Thickness: 0.1–4 mm · Width: 10–500 mm
Coil OD: up to 1,500 mm
Per AMS 5528 / ASTM A693 Cold-rolled · Bright Annealed (BA) · Cond. A
〜 Wire Ø0.1 mm – Ø12 mm
Coil or straight lengths
Per ASTM A580 / AMS 5678 Bright drawn · Annealed · Cond. A / CH
⬡ Forging / Billet Dia.: up to 800 mm
Weight: up to 2,000 kg/piece
Per AMS 2375 / ASTM A484 Rough-machined · As-forged · UT-tested
📐

Custom sizes available upon request — non-standard diameters, special lengths (up to 9,000 mm), close-tolerance turned/ground stock, or specific heat treatment conditions. Contact us with your print or specification.

Submit Your Specifications

Delivery & Logistics

Reliable global supply chain — from our Fushun facility to your receiving dock

⏱

Lead Time

  • Ex-Stock: 7–15 business days ex-works
  • Custom / Special: 25–30 days ex-works
  • Emergency (ex-stock): 3–5 days available
📦

Minimum Order

  • Ex-Stock: 1 piece / 1 bar minimum
  • Custom Order: Min. 3 metric tons
  • Qualification Samples: Available on request
🛡

Packaging

  • Standard: Bundle with steel strapping
  • Export: VCI anti-rust film + plywood / wooden case
  • Bright/Ground: PE sleeve + wooden crate
🚢

Shipping Options

  • Sea: FCL / LCL from Shanghai / Tianjin
  • Air: DHL / FedEx / airline cargo
  • Incoterms: FOB, CIF, CFR, EXW, DAP
📋

Export Documents

  • Commercial Invoice + Packing List
  • Bill of Lading · Certificate of Origin
  • MTR (EN 10204 3.1) · UT Report (on request)
💳

Payment Terms

  • T/T: 30% deposit + 70% before shipment
  • L/C at sight: Accepted (≥ USD 50,000)
  • Samples: PayPal / Western Union

Manufacturing Process & Capability

Complete process chain — from primary melt to final packaged product — under one AS9100D quality system

01

Melting VIM / VOD / VAR / ESR

Primary melt via Vacuum Induction Melting (VIM) or VOD. Aerospace and critical grades re-melted via VAR (Vacuum Arc Remelting) or ESR (Electroslag Remelting). Achieves ultra-low C, S, P levels with controlled non-metallic inclusion content. VIM+VAR melt practice mandatory per AMS 5629 (PH13-8Mo) and AMS 5659 (15-5PH).

▼
02

Forging 3,000T Fast Forge Press

Multi-pass open-die forging on 3,000-ton hydraulic fast-forging press. Forging reduction ratio ≥ 4:1 eliminates center porosity and develops homogeneous wrought microstructure. Produces billets, bars, rings, and disc forgings up to Ø800 mm / 2,000 kg. All forging parameters logged and retained per AS9100D.

▼
03

Hot Rolling & Drawing Rolling Mill

Computer-controlled hot rolling mill produces round bar, flat bar, and coil in precise dimensional tolerances. In-line temperature monitoring ensures consistent microstructure and surface quality. Cold drawing and wire drawing available for small-diameter product forms per ASTM A580.

▼
04

Heat Treatment Automated Furnace · AMS 2750E

Fully automated heat treatment furnaces with calibrated thermocouples and data-logging per AMS 2750E (Pyrometry). Temperature uniformity ±5°C (TUS-surveyed). All standard aging conditions — H900 through H1150M — performed in-house with full temperature charts included in documentation.

▼
05

Finishing CNC Turn · Grind · Peel

CNC turning centers, centreless grinding machines, and roller-die peeling lines deliver close-tolerance bright bar. Surface roughness Ra ≤ 0.8 µm (ground), Ra ≤ 3.2 µm (peeled/turned). Straightness ≤ 0.5 mm/m standard; precision ≤ 0.2 mm/m. Cut-to-length sawing ±1 mm.

▼
06

Inspection & Testing QC Lab · NDT · OES Spectro

Chemical: OES optical emission spectrometry per heat + wet chemistry verification. Mechanical: Tensile per AMS 2370 / ISO 6892; Rockwell & Brinell hardness; Charpy impact at room temp and −40°C. NDT: 100% Ultrasonic Testing (UT) per AMS 2630 / ASTM A388 for aerospace grades; Eddy Current (ET) for bar/wire. Dimensional: CMM, laser micrometer.

▼
07

Packaging & Dispatch Export Ready

Each item tagged with heat number, lot/batch number, grade, condition, and dimensions. MTR (EN 10204 3.1) generated per heat. VCI export packaging applied. Full documentation package — MTR, UT report, HT chart, CoO, invoice, packing list — compiled and dispatched with each shipment.

Our Fushun facility operates as one of China's largest specialty steel production bases, with annual capacity exceeding 50,000 metric tons of alloy and special steels. The production line is equipped with 3,000-ton hydraulic fast forging presses, fully automated data-logging heat treatment furnaces, and a dedicated aerospace-grade inspection laboratory operating under AS9100D.

For critical aerospace and defense applications, VIM+VAR double-melt material is available with full AMS certification. Melting records, forging parameter logs, and heat treatment charts are retained for a minimum of 10 years and are available for customer quality audits.

Industry Applications

PH stainless steel solving critical material challenges across global industries

✈️

Aerospace & Defense

17-4PH H900 and PH13-8Mo H950 are the primary choices for aircraft structural fasteners, landing gear actuator pins, missile airframe components, and hydraulic actuators. Meets AMS 5643, AMS 5629, MIL-S-81506, and Boeing/Airbus material specifications. DFARS-compliant documentation available.

🛢️

Oil & Gas

17-4PH H1025 and H1150 conditions meet NACE MR0175 / ISO 15156 hardness limits for sour service. Widely used for downhole tool mandrels, valve stems, pump shafts, subsea connectors, and wellhead components. H1150M condition provides maximum SCC resistance for the most aggressive environments.

🔬

Medical Devices

17-4PH and 15-5PH in H1025/H1150 provide the corrosion resistance, machinability, and biocompatibility needed for surgical instrument shafts, orthopedic device tooling, and dental components. Semi-non-magnetic in solution-annealed condition. Compliant with ASTM F899 for surgical instrument materials.

⚓

Marine & Offshore

17-4PH H900 delivers the ideal combination of high strength (>1310 MPa UTS) and corrosion resistance for seawater pump shafts, valve stems, deck hardware, and subsea fasteners. Significantly stronger than 316L at comparable corrosion resistance. H1150 recommended for prolonged saltwater immersion service.

⚗️

Food Processing & Chemical

H1150 and H1150M conditions provide the optimal combination of ductility, toughness, and corrosion resistance for food-grade conveyor shafting, agitator components, and pumps in acidic media — delivering strength and corrosion performance that exceeds standard 316L stainless.

⚡

Power Generation

17-4PH is widely used in turbine blade roots, pump shafting, and valve bodies in conventional and nuclear power plants. Custom 465® and PH13-8Mo are selected for components requiring >1450 MPa UTS combined with exceptional fatigue life in steam and high-pressure hydraulic environments.

Quality Assurance

Certified, traceable, and independently verified — because your critical application demands complete confidence in material data

📄

Mill Test Report (EN 10204 3.1)

Every shipment is accompanied by a full MTR to EN 10204 Type 3.1, signed and stamped by our Quality Assurance Manager. Content: chemical analysis per heat (OES + wet chemistry), mechanical test results per lot, heat treatment records with temperature charts, and dimensional inspection sign-off.

🏛️

Third-Party Inspection

We fully support pre-shipment inspection by: SGS, Bureau Veritas (BV), TÜV Rheinland, and Intertek. Services include witness testing (mechanical/chemical), dimensional inspection, visual examination, UT witnessing, and document review. Typically arranged within 3–5 business days notice.

🔍

Full Batch Traceability

Every bar, plate, strip, and forging is identified: Heat Number → lot/batch number → heat treatment batch record → NDT inspection record → dimensional inspection. Complete digital records retained for a minimum of 10 years and available for customer audit at any time.

✅

Certifications & QMS

Quality Management System certified to AS9100D (Aerospace QMS) and ISO 9001:2015. Production and testing per AMS 2370 (mechanical testing), AMS 2630 (UT inspection), AMS 2750E (pyrometry / furnace qualification), and customer-specific quality plans for project requirements.

🧪

In-House Testing Laboratory

On-site laboratory with: OES optical emission spectrometer (per heat), universal tensile testing machines (per AMS 2370 / ISO 6892), Rockwell / Brinell / Vickers hardness testers, Charpy impact apparatus (−196°C to +200°C), metallographic suite, and digital UT flaw detection equipment.

🌐

DFARS & Regulatory Compliance

Material origin documentation available for DFARS requirements. Country of origin (China, Fushun) stated on all commercial documents. RoHS-compliant material formulations confirmed by chemical analysis. REACH compliance statements available for EU customers. Export license and HS tariff codes provided.

❝

"Full traceability from melt to delivery — every bar, every batch. Our quality commitment is not a promise; it is documented, independently certified, and available for your audit at any time."

Frequently Asked Questions

Quick answers to the questions our global industrial customers ask most often

We certify to the full range: ASTM A564/A564M (bar), A693 (strip/sheet), A580 (wire); AMS 5643 (17-4PH bar), 5659 (15-5PH bar), 5528/5529 (17-7PH), 5629 (PH13-8Mo), 5578 (Custom 455), 5936 (Custom 465); EN/DIN 10088, 10278; JIS G4303/G4304/G4305 (SUS630, SUS631, SUS632). Customer-specific or OEM proprietary specifications (Boeing BMS, Airbus AIMS) can be accommodated for qualified orders — please submit your document for feasibility review.

Yes. We routinely supply qualification material — typically 1–5 pieces or 10–100 kg — for new customers conducting material qualification or coupon testing. Samples are priced at standard commercial rates with no surcharge, and supplied with full MTR documentation. We can cut to specific lengths or supply as-bar. Lead time for ex-stock samples is typically 7–10 business days including dispatch preparation.

Standard export packaging: bundles strapped with steel bands, wrapped in VCI anti-corrosion film, loaded in plywood or wooden crates for sea freight. Bright/ground bars are individually wrapped in PE sleeves before crating. We ship from Shanghai (CNSHA) and Tianjin (CNTXG) via FCL or LCL sea freight, or via air freight (DHL, FedEx, airline cargo) for urgent small orders. All standard Incoterms available: FOB, CIF, CFR, EXW, DAP.

Absolutely. We fully support inspection by SGS, Bureau Veritas, TÜV Rheinland, Intertek, or any customer-nominated organization. Services available: witness testing of mechanical and chemical properties, dimensional inspection, visual/surface examination, and UT witnessing at our Fushun facility. 3–5 business days advance notice is required for inspector coordination. Inspection fees are typically to the buyer's account per standard commercial practice.

For ex-stock items (standard grades, common bar sizes), ex-works lead time is 7–15 business days from order confirmation — including cutting, surface preparation, heat treatment (if specific aged condition ordered), final inspection, and document preparation. Custom orders (non-standard dimensions, special grades or melting practice) require 25–30 days ex-works. Emergency expediting of ex-stock items is sometimes possible in 3–5 business days. Sea freight transit adds 15–35 days depending on destination port.

Primary method is T/T (telegraphic transfer): 30% deposit on order confirmation, 70% balance before shipment against copy of B/L. For established customers, credit terms are negotiable. L/C at sight is accepted for orders ≥ USD 50,000 from a reputable international bank. For sample orders, PayPal and Western Union are also acceptable. Transactions in USD, EUR, or CNY.

Yes — material can be supplied in any standard aging condition: H900, H925, H1025, H1075, H1100, H1150, H1150M for 17-4PH and 15-5PH; CH900, TH1050, RH950 for 17-7PH; H950–H1150 for PH13-8Mo. All heat treatments are performed in-house in calibrated furnaces per AMS 2750E, with full temperature charts and hardness verification included in the MTR. Please specify required condition at time of inquiry.

Request a Quote / Submit Inquiry

Fill in your requirements below — our technical sales team responds within 24 hours (Mon–Fri, UTC+8)

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x