69 documents, free to download — 43 published standards and 26 grade datasheets. The specifications our stock and forgings are produced and inspected against, grouped by the body that publishes them, followed by the mill datasheets for individual grades.
If you are checking whether a grade we supply meets a specification, start with the standard number. If you need the composition or mechanical data for a specific grade rather than the specification text, the product pages carry that.
ASTM (13)
| Standard |
Document |
Download |
| ASTM A388 |
Standard Practice for Ultrasonic Examination of Heavy Steel Forgings |
PDF |
| ASTM E112 |
2010 Standard Test Methods for Determining Average Grain Size |
PDF |
| ASTM A29 |
Standard Specification Steel Bars Carbon and Alloy Hot Wrought General Requirements |
PDF |
| ASTM A681 |
Standard Specification for Tool Steel Alloy |
PDF |
| ASTM A694 |
Carbon and Alloy Steel Forgings for Pipe Flanges Fittings Valves and Parts for High Pressure Transmission Service |
PDF |
| ASTM A304 |
2004 Standard Specification for Carbon and Alloy Steel Bars Subject to End Quench Hardenability Requirements |
PDF |
| ASTM A228A |
228M music spring steel wire |
PDF |
| ASTM A182 |
Standard Specification for Forged or Rolled Alloy Steel Pipe Flanges Forged Fittings and Valves and Parts |
PDF |
| ASTM A564 |
2004 Standard Specification for Hot Rolled and Cold Finished Age Hardening Stainless Steel Bars and Shapes |
PDF |
| ASTM E45 |
2011 Standard Test Methods for Determining the Inclusion Content of Steel |
PDF |
| ASTM A705 |
Standard Specification for Age Hardening Stainless Steel Forgings |
PDF |
| ASTM A580 |
2006 Standard Specification for Stainless Steel Wire |
PDF |
| ASTM A682 |
2002 Standard Specification for Steel Strip High Carbon Cold Rolled General Requirements |
PDF |
BS / BS EN (9)
| Standard |
Document |
Download |
| BS 970 |
Part 3 Specification for Wrought steels for mechanical and allied engineering purposes |
PDF |
| BSENISO 4957 |
2000 Tool Steel |
PDF |
| BSEN 10089 |
2002 Hot rolled steels for quenched and tempered springs |
PDF |
| BSEN 10277 3 |
2008 Bright steel products Free Cutting Steel Part 3 General |
PDF |
| BSENISO 15156 |
Petroleum and Natural Gas industries materials for use in H2s containling environments in oil and gas production Part 3 |
PDF |
| BSEN 10084 |
2008 Case hardening steels Technical delivery conditions |
PDF |
| BSEN 10277 4 |
2008 Bright steel products Case Hardening Steel Part 4 General |
PDF |
| BSEN 10250 3 |
2000 Open die steel forgings for general engineering purposes Part 3 Alloy special steels |
PDF |
| BSEN 10277 2 |
2008 Bright steel products Steel for General Engineering Purposes Part 2 |
PDF |
EN (4)
| Standard |
Document |
Download |
| EN 10088 3 |
stainless steel |
PDF |
| EN 10025 |
Part 6 flat products of high yield strength structural steels in the quenched and tempered condition |
PDF |
| EN 10025 |
Hot rolled products of structural steels Part 2 Technical delivery conditions for non alloy structure steel |
PDF |
| EN 10025 |
Part 5 Technical delivery conditions for structural steels with improved atmospheric corrosion resistance |
PDF |
DIN (7)
| Standard |
Document |
Download |
| DIN 17100 |
STEELS FOR GENERAL STRUCTURAL PURPOSES |
PDF |
| DIN 17200 |
Steels for Quenching and Tempering |
PDF |
| DINEN 10222 |
Steel forgings for pressure purposes Part 1 General requirements for open die forgings |
PDF |
| DIN 17210 |
1986 Case hardening steels |
PDF |
| DIN 17230 |
1980 Ball and Roller Bearing Steels |
PDF |
| DIN 175 |
Polished Round Steel Dimensions Permissible Deviations |
PDF |
| DINEN 10308 |
2002 Non destructive Testing Ultrasonic Testing of Steel Bars |
PDF |
JIS (6)
| Standard |
Document |
Download |
| JIS G4053 |
2008 Low alloyed steels for machine structural use |
PDF |
| JIS G4105 |
1979 Chromium Molybdenum Steels1 |
PDF |
| JIS G4052 |
2008 Structural steels with specified hardenability bands |
PDF |
| JIS G4805 |
1999 high carbon chromium bearing steels |
PDF |
| JIS G4303 |
2005 Stainless steel bars |
PDF |
| JIS G4403 |
2006 High speed tool steels |
PDF |
API (1)
| Standard |
Document |
Download |
| API 5DP |
2009 Specification for Drill Pipe |
PDF |
AS (3)
| Standard |
Document |
Download |
| AS 1444 |
2007 Wrought alloy steels Standard hardenability H series and hardened and tempered to design |
PDF |
| AS 1710 |
2007 Non destructive testing Ultrasonic testing of carbon and low alloy steel plate and universals |
PDF |
| AS 1065 |
1988 Non Destrcutive Testing Ultrasonic testing of carbon and low alloy steel forging |
PDF |
Grade datasheets (AMS and mill datasheets) (26)
| Standard |
Document |
Download |
| AMS 5643 |
17 4 STAINLESS STEEL AISI 630 UNS S17400 |
PDF |
| AMS 5659 |
15 5 PH STAINLESS STEEL |
PDF |
| AMS 4928 |
Ti 6Al 4V Titanium Grade 5 AMS 4911 UNS R56400 |
PDF |
| AMS 6345 |
4130 AMS 6346 AMS 6350 |
PDF |
| AMS 5629 |
13 8 PH STAINLESS STEEL UNS S13800 |
PDF |
| AMS 6512 |
Maraging 250 VASCOMAX® 250 Steel |
PDF |
| — |
86CRMOV7 1.2327 fushun |
PDF |
| AMS 6514 |
Maraging 300 VASCOMAX® 300 Steel |
PDF |
| AMS 6417 |
4340 MOD Alloy Steel AMS 6419 UNS K44220 |
PDF |
| — |
F51 Stainless Steel Fushun |
PDF |
| AMS 6515 |
Maraging 350 VASCOMAX® 350 Steel |
PDF |
| AMS 6532 |
AerMet® 100 |
PDF |
| — |
14NiCr14 15NiCr13 1.5752 12X2H4A fushun |
PDF |
| AMS 6414 |
4340 ALLOY STEEL VAR UNSG43406 |
PDF |
| AMS 5662 |
Inconel® 718 Nickel Alloy UNS N07718 |
PDF |
| AMS 5599 |
Nickel Alloy Corrosion and Heat Resistant Sheet Strip and Plate Solution Heat Treated |
PDF |
| — |
310MoLN 1.4466 Stainless Steel |
PDF |
| — |
Titanium Alloy Ti 6Al 4V Grade 5 FUSHUN |
PDF |
| AMS 4930 |
Ti 6Al 4V ELI Titanium UNS R56401 Extra Low Interstitial |
PDF |
| AMS 6411 |
4330 MOD Alloy Steel VAR UNSK23080 |
PDF |
| AMS 6265 |
9310 ALLOY STEEL VAR UNS 93106 |
PDF |
| AMS 5666 |
Inconel® 625 Nickel Alloy UNS N06625 |
PDF |
| — |
6CrW2Si Tool Steel |
PDF |
| — |
1.2394 Tool Steel |
PDF |
| — |
Titanium 2 fushun |
PDF |
| — |
MARS190 FUSHUN |
PDF |
What we can supply against these standards