manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Duplex Stainless Steel | Certified 2507, 2205 Supplier

Duplex Stainless Steel  ·  Hunan Fushun Metal Co., Ltd.

Precision-Cut, Mill-Certified
Duplex Stainless Steel —
Ready to Ship Worldwide

Duplex stainless steel from cut-to-length round bar and saw-cut plate to machined billets and structural sections — supplied with EN 10204 3.1 documentation to 52+ countries. ISO 9001 certified. 30-day lead time.

Cut-to-Length Round Bar Saw-Cut Plate & Sheet Machined Billets & Forgings Strip, Wire & Coil EN 10204 3.1 MTC Standard ISO 9001 Certified
52+
Export Countries
25+
Duplex Grades
30d
Max Lead Time
1998
Est. Year
ISO 9001 EN 10204 3.1 / 3.2 MTC ASTM / ASME Compliant NACE MR0175 / ISO 15156 NORSOK M-630 Approved PED 2014/68/EU
Ships to:
USA
EU
Japan
Mid-East
ANZ
Product Range

Duplex Stainless Steel Grades & Product Matrix

Duplex stainless steel combines a ferritic-austenitic dual-phase microstructure that delivers roughly twice the yield strength of standard 304 or 316L grades alongside exceptional resistance to chloride pitting and stress corrosion cracking. The grades below are available from stock or on order, supplied per ASTM, EN/DIN, JIS and other national standards.

Standard Duplex

Duplex 2205

S31803 / S32205  ·  EN 1.4462  ·  ASTM F51 / F60

Yield Strength
≥ 450 MPa
Hardness Max
290 HBW
PREN
~ 35
Condition
Annealed

The most widely used duplex stainless steel grade, offering a balanced combination of corrosion resistance and mechanical strength. Ideal for process piping, pressure vessels, heat exchangers, and offshore structural components in moderately aggressive chloride environments. JIS equivalent SUS329J3L; GOST 02X22H5AM3.

ASTM A240MASTM A276EN 10088-2/3JIS SUS329J3L
Super Duplex

SAF 2507

S32750  ·  EN 1.4410  ·  ASTM F53  ·  GB 022Cr23Ni5Mo3N*

Yield Strength
≥ 550 MPa
Hardness Max
310 HBW
PREN
≥ 42
Condition
Annealed

Premium super duplex stainless steel with 25% Cr, 7% Ni, 4% Mo. Outstanding resistance to pitting, crevice corrosion, and chloride stress corrosion cracking. The reference grade for offshore oil & gas, seawater desalination, and high-pressure chemical service. Trade designations: SAF 2507, UR47N+.

ASTM A276ASTM A479ASTM A182 F53EN 10088-3NORSOK M-630
Super Duplex

Zeron 100

S32760  ·  EN 1.4501  ·  ASTM F55  ·  JIS SUS329J2L

Yield Strength
≥ 550 MPa
Hardness Max
310 HBW
PREN
≥ 40
Condition
Annealed

Super duplex stainless steel enhanced with tungsten (W) and copper (Cu) for superior corrosion resistance in mixed acid and chloride environments. GB equivalent: 022Cr25Ni7Mo4WCuN. Particularly suited to subsea umbilicals, water-injection systems, and high-pressure downhole tubing applications.

ASTM A276EN 10088-3JIS SUS329J2L
Lean Duplex

LDX 2101

S32101  ·  EN 1.4162  ·  X2CrMnNiN21-5-1

Yield Strength
≥ 450 MPa
Hardness Max
290 HBW
PREN
~ 26
Condition
Annealed

Cost-effective lean duplex stainless steel with reduced nickel content, delivering twice the strength of standard 304/316 grades. Excellent for structural applications, storage tanks, water treatment equipment, and food processing machinery where moderate corrosion resistance is required.

ASTM A240MEN 10088-2
Lean Duplex

SAF 2304

S32304  ·  EN 1.4362  ·  X2CrNiN23-4

Yield Strength
≥ 400 MPa
Hardness Max
290 HBW
PREN
~ 26
Condition
Annealed

Molybdenum-free lean duplex stainless steel with excellent weldability and formability. A cost-efficient alternative to 316L in mild chloride environments. Common applications include architectural structures, water infrastructure, and food-grade processing equipment.

ASTM A240MASTM A789EN 10088-2
Super Duplex

Ferralium 255

S32550  ·  ASTM F61

Yield Strength
≥ 550 MPa
Hardness Max
302 HBW
PREN
~ 38
Condition
Annealed

Copper-bearing super duplex stainless steel with enhanced resistance to reducing acids and dilute sulfuric acid solutions. High strength combined with good machinability makes it ideal for pumps, valve bodies, impellers, and rotating shaft applications in the chemical process industry.

ASTM A276ASTM A479
Standard Duplex

3RE60

S31500  ·  EN 1.4424  ·  X2CrNiMoSi18-5-3  ·  GB 022Cr9Ni5Mo3Si2N

Yield Strength
≥ 440 MPa
Hardness Max
290 HBW
PREN
~ 30
Condition
Annealed

Silicon-bearing duplex stainless steel with particular resistance to chloride stress corrosion cracking in tubular form. Well established in the pulp & paper industry and for shell-and-tube heat exchangers handling dilute sulfuric acid and bleach-plant chemicals.

ASTM A789ASTM A790EN 10088-2
Hyper Duplex

2707 HD

S32707  ·  EN 1.4658  ·  X2CrNiMoCoN28-8-5-1

Yield Strength
≥ 690 MPa
Hardness Max
320 HBW
PREN
≥ 48
Condition
Annealed

The highest tier in the duplex stainless steel family. Hyper duplex 2707 HD features extreme Cr, Mo, and N content for pitting resistance far exceeding conventional super duplex grades. Designed specifically for deep-sea oil & gas downhole tubing and aggressive sour-service environments.

EN 10088-3NORSOK M-630

* Additional grades available on request: S32202 (EN 1.4062), S32900 (329 / EN 1.4477), AL 2003 (S32003), DP-3 (S31260), S31200 (F50 / EN 1.4460), UR52N+ (S32520 / EN 1.4507), 3207 HD (S33207). Contact us with your specification.

Need duplex stainless steel for your project?
Tell us your grade, dimension, and quantity.

Our technical sales team confirms receipt and responds with pricing within 24 business hours. Mill certificates included as standard.

Get a Free Quote Now
Engineering Data

Technical Specifications

All duplex stainless steel grades are supplied to the chemical composition and mechanical property requirements of the applicable ASTM, EN/DIN or JIS standard. The tables below serve as a reference guide; the definitive values are those stated on the Mill Test Certificate shipped with each order.

Chemical Composition of Duplex Stainless Steel Grades (wt%)

Grade / UNS C max (%) Mn (%) Si max (%) Cr (%) Mo (%) Ni (%) N (%) Other Elements EN No.
LDX 2101 / S321010.0404.0–6.01.0021.0–22.00.10–0.801.35–1.700.20–0.25Cu ≤1.01.4162
SAF 2304 / S323040.030≤2.501.0021.5–24.50.05–0.603.0–5.50.05–0.201.4362
S322020.030≤2.001.0021.0–23.0≤0.451.0–2.80.18–0.261.4062
3RE60 / S315000.0301.20–2.001.40–2.0018.0–19.02.50–3.004.25–5.250.05–0.101.4424
2205 / S318030.030≤2.001.0021.0–23.02.5–3.54.5–6.50.08–0.201.4462
2205 / S322050.030≤2.001.0022.0–23.03.0–3.54.5–6.50.14–0.201.4462
S32900 / 3290.080≤1.000.7526.0–29.01.0–2.02.5–5.01.4477
AL 2003 / S320030.030≤2.001.0019.5–22.50.50–2.003.0–4.00.14–0.20
S31200 / F500.030≤2.001.0024.0–26.01.20–2.005.5–6.50.14–0.201.4460
DP-3 / S312600.030≤1.000.7524.0–26.02.5–3.55.5–7.50.10–0.30Cu 0.2–0.8, W 0.1–0.5
Ferralium 255 / S325500.040≤1.501.0024.0–27.02.9–3.94.5–6.50.10–0.25Cu 1.5–2.5
UR52N+ / S325200.030≤1.500.8024.0–26.03.0–4.05.5–8.00.20–0.35Cu 0.5–3.01.4507
SAF 2507 / S327500.030≤1.200.8024.0–26.03.0–5.06.0–8.00.24–0.321.4410
Zeron 100 / S327600.030≤1.001.0024.0–26.03.0–4.06.0–8.00.20–0.30Cu 0.5–1.0, W 0.5–1.01.4501
2707 HD / S327070.030≤1.500.5026.0–29.04.0–5.06.0–9.00.30–0.50Co ≤1.01.4658
3207 HD / S332070.030≤1.200.5029.0–33.03.0–5.06.0–9.00.40–0.60

Highlighted cells indicate values critical to corrosion performance (PREN = %Cr + 3.3×%Mo + 16×%N). Ranges represent UNS/EN specification limits; individual heat compositions within these ranges vary and are confirmed on the Mill Test Certificate. Sources: ASTM A240M, ASTM A276, ASTM A789, EN 10088-2, EN 10088-3. Always reference the current edition of the applicable standard.

Mechanical Properties of Duplex Stainless Steel Grades — Solution-Annealed Condition

Grade / UNS 0.2% Yield
(MPa) min
UTS
(MPa) min
Elongation
(%) min
Hardness
max (HBW)
PREN
(indicative)
Primary Standard
LDX 2101 / S3210145065030290~26ASTM A240M
SAF 2304 / S3230440060025290~26ASTM A240M
S3220245065025290~26EN 10088-2
3RE60 / S3150044063030290~30ASTM A789
2205 / S3180345062025290~35ASTM A240M / EN 10088-2
2205 / S3220545065525290~35ASTM A240M
S32900 / 32948569020290~30ASTM A240M
AL 2003 / S3200345065525293~32ASTM A240M
S31200 / F5041569020293~30ASTM A182
DP-3 / S3126045069020302~34ASTM A240M
Ferralium 255 / S3255055076015302~38ASTM A276
UR52N+ / S3252055077025310~38EN 10088-3
SAF 2507 / S3275055080015310≥42ASTM A276 / EN 10088-3
Zeron 100 / S3276055075025310≥40ASTM A276 / EN 10088-3
2707 HD / S3270769093015320≥48EN 10088-3
3207 HD / S33207730100015320≥50EN 10088-3

All values are minimum requirements in the solution-annealed and water-quenched condition, tested at room temperature per ASTM A370 or EN ISO 6892-1 (tensile) and EN ISO 6506-1 / ASTM E10 (Brinell hardness). PREN = %Cr + 3.3×%Mo + 16×%N; values shown are indicative and depend on actual heat chemistry. Highlighted rows indicate superior performance tiers. Confirm lot-specific values on the Mill Test Certificate.

Product Forms

Available Forms & Dimensions

Duplex stainless steel is stocked and supplied in the following standard forms. All dimensions shown are indicative; intermediate sizes, tighter tolerances, and non-standard profiles are available on request. Custom machined components — including disc forgings, flanging-quality blanks, and stepped shafts — are produced to drawing.

Round Bar

⌀ 6 – 600 mm
Length up to 6,000 mm
Hot-rolled or forged

Flat Bar

Width: 10 – 400 mm
Thickness: 3 – 100 mm
Length up to 6,000 mm

Plate / Sheet

Thickness: 2 – 100 mm
Width up to 3,000 mm
Length up to 12,000 mm

Strip / Coil

Thickness: 0.10 – 4.0 mm
Width: 5 – 650 mm
Annealed & pickled

Wire

⌀ 0.10 – 16.0 mm
Spools, coils, cut lengths
Various surface finishes

Hex Bar

AF: 8 – 100 mm
Length up to 6,000 mm
Hot-rolled or cold-drawn

Custom dimensions welcome. Non-standard thicknesses, widths, and lengths can be produced to drawing. Custom-profiled sections, machined blanks, and large disc forgings are available with a minimum order of 3 metric tons for made-to-order items. Send your DXF, PDF or written specification to [email protected].

Logistics

Delivery & Packaging

We maintain broad stock of duplex stainless steel in commonly ordered grades and sizes to support fast turnaround. All orders are packed to international export standards with full documentation packages. Dedicated logistics coordinators manage each shipment from warehouse to port of discharge.

30 Days
Maximum Lead Time

Stock items ship within 7–15 business days. Custom dimensions or special processing within 30 calendar days from order confirmation. Expedited scheduling available on request — contact us with project deadlines.

1 Piece
MOQ (Stock Items)

A single piece or bar from in-stock material, no minimum tonnage required. Mixed-grade orders are welcome. Minimum 3 metric tons applies only to custom-manufactured items not held in stock.

3 Options
Packaging Types

Standard Export: Steel-strapped bundles on wooden pallets.
Anti-Rust Pack: VCI film-wrapped in moisture-proof bags.
Bright Surface: Individual PE-sleeved bars in reinforced wooden crates.

52+ Countries
Global Shipping

Regular shipments to the Americas, Europe, Southeast Asia, the Middle East, and Oceania. Ports of loading: Shanghai, Tianjin, Guangzhou. Sea freight, airfreight, and courier options available.

Process Chain

Manufacturing Capability

Hunan Fushun Metal Co., Ltd. controls the complete production chain for duplex stainless steel from primary melting through to final inspection and surface finishing. This vertically integrated capability eliminates sub-contracting risk and ensures full heat-to-delivery traceability at every stage.

Key Metallurgical Control Points for Duplex Stainless Steel Production

1
Primary Melting
30/50/60t EAF
Electric Arc Furnace
2
Ladle Refining
30/60t LF
Argon stirring, desulfurization
3
Vacuum Degassing
30/60t VD/VOD
Ultra-low C and gas
4
ESR Remelting
1–15t ESR
6/12/30t PESR
5
VIM / VAR
0.5–12t VIM
3–12t VAR
6
Forging
4,500t / 8,000t press
1,800t / 2,700t GFM
7
Rolling
250 / 350 / 550 / 850 mm
rolling mill lines
8
Heat Treatment
Solution anneal + water quench
Computer-controlled furnaces
9
NDT Inspection
UT, PT, PMI, chemical
per ASTM / EN
10
Finishing & Dispatch
Straightening, cutting,
marking, MTC issue
Vacuum Induction Melting (VIM)
Precise alloy composition control in a sealed vacuum environment — eliminates contamination and achieves ultra-low gas content required for premium duplex stainless steel grades such as 2707 HD and 3207 HD.
Electroslag Remelting (ESR / PESR)
Eliminates inclusions and macro-segregation, producing homogeneous ingots with uniform chemistry — essential for consistent mechanical and corrosion performance in critical-service duplex stainless steel.
Ultrasonic Testing (UT) — 100% Volumetric
Full volumetric inspection of all forged and rolled products per ASTM A388, EN 10228-3, or customer-specified acceptance criteria, with printed UT reports available for every shipment.
Solution Anneal + Water Quench
All duplex stainless steel grades solution-annealed at 1,020–1,120 °C and rapidly water-quenched to achieve the optimal 35–55% ferrite balance and maximum corrosion resistance per ASTM and EN requirements.
Large-Size Forging — up to 8,000 Tonnes
Hydraulic presses rated to 8,000 tonnes produce large-diameter bars, block forgings, and disc blanks up to 600 mm diameter for flanges, valve bodies, and pressure vessel nozzles in duplex stainless steel.
Ferrite Content Verification
Phase balance (35–55% ferrite) verified by magnetic induction measurement per ASTM E1077 or ASTM A800 on every duplex stainless steel batch — recorded on the MTC and available in the documentation package.
End Markets

Duplex Stainless Steel Industry Applications

The dual-phase microstructure and high PREN values of duplex stainless steel make it indispensable across industries where standard austenitic grades cannot deliver adequate service life. The applications below illustrate the specific value duplex stainless steel delivers in each sector.

Oil & Gas

Duplex stainless steel is the material of choice for offshore risers, subsea manifolds, seawater injection lines, heat exchanger bundles, and high-pressure downhole tubing. Its resistance to hydrogen-induced stress cracking (HISC) and chloride SCC is critical in sour-service H₂S environments per NACE MR0175 / ISO 15156.

SAF 2507Zeron 10022052707 HD

Desalination & Water Treatment

Seawater desalination plants rely on super duplex stainless steel for membrane pressure vessels, high-pressure pump components, and pipework. The PREN ≥40 rating enables thin-wall designs saving weight and capital cost without sacrificing resistance to concentrated chloride attack in RO and MSF processes.

SAF 2507Zeron 100UR52N+

Chemical & Petrochemical Processing

Reactors, columns, heat exchangers, and piping handling chloride-contaminated acids and oxidizing media benefit from duplex stainless steel's broad resistance profile. Copper-bearing grades provide additional resistance to sulfuric and formic acid; silicon-bearing 3RE60 excels in bleach-plant and organic acid service.

2205Ferralium 2553RE60UR52N+

Marine & Offshore

Structural components, propeller shafts, fasteners, and hull fittings on vessels operating in seawater need materials resistant to biofouling-accelerated pitting and crevice corrosion. Super duplex stainless steel achieves this at significantly reduced wall thicknesses compared with 316L, lowering vessel weight and fuel costs.

SAF 2507Zeron 100SAF 2304

Pulp & Paper

One of the earliest industries to adopt duplex stainless steel, pulp and paper operations use it for digesters, bleach-plant equipment, washers, and process tanks exposed to acidic chloride-bearing bleach chemicals. The combination of SCC resistance and mechanical strength provides long maintenance-free service life.

22053RE60LDX 2101

Power Generation & FGD

Flue gas desulfurization (FGD) absorber towers, condenser tubing, and heat recovery units in power plants face aggressive acid chloride condensate. Duplex stainless steel's pitting and erosion-corrosion resistance makes it the standard material for absorber liners, spray headers, and recirculation pump casings.

SAF 25072205Zeron 100

Food & Beverage Processing

Lean and standard duplex stainless steel grades are increasingly specified for food processing tanks, evaporators, conveyors, and CIP piping. Higher strength versus 316L allows reduced wall thickness, and the improved corrosion resistance in chloride-containing cleaning solutions provides a hygienically superior, longer-lasting surface.

LDX 2101SAF 23042205

Structural & Construction

Lean duplex grades (LDX 2101, SAF 2304, S32202) deliver roughly twice the yield strength of austenitic stainless grades, enabling slimmer sections for bridges, coastal facades, concrete reinforcing bars, and cladding systems. Reduced nickel content also provides more price-stable procurement versus nickel-sensitive austenitic grades.

LDX 2101SAF 2304S32202

Identified your application?
Request a tailored duplex stainless steel quote.

Specify your grade, form, dimensions, and quantity. Our engineers match you with the right solution and respond within 24 hours.

Send Your Inquiry
Quality System

Quality Assurance & Certification

Every order of duplex stainless steel is backed by documented quality control at every stage of production. Our ISO 9001 certified quality management system ensures that no consignment leaves our facility without a complete, verifiable documentation package that meets or exceeds your project specification requirements.

Mill Test Certificate (MTC / MTR)

A full EN 10204 3.1 Mill Test Certificate accompanies every delivery, stating heat number, batch number, chemical composition by heat analysis, mechanical test results, heat treatment records, and ferrite content where applicable. EN 10204 3.2 countersigned certificates are available on request.

Third-Party Inspection

We fully support independent inspection by internationally recognised bodies including SGS, Bureau Veritas, Intertek, and TÜV. Witness testing for chemical analysis, tensile, hardness, impact, and corrosion tests can be arranged during production or as pre-shipment inspection.

Non-Destructive Testing (NDT)

Ultrasonic testing (UT) per ASTM A388 or EN 10228-3, liquid penetrant testing (PT) per ASTM E165, and positive material identification (PMI) by XRF are performed on all critical product forms. Printed inspection reports are included in the shipping documentation.

Corrosion Testing

Intergranular corrosion testing per ASTM A262 Practice E (Strauss test), pitting resistance per ASTM G48 Method A/B, and NACE TM0177 stress corrosion cracking testing are available for specification-critical duplex stainless steel orders. CPT reports per ASTM G48 available for SAF 2507 and S32760.

ISO 9001 Certified Quality Management

Our quality management system is certified to ISO 9001, covering all processes from raw material procurement through production, testing, packing, and delivery. Internal audits, corrective-action procedures, and supplier qualification protocols are applied consistently across all product lines including duplex stainless steel.

Phase Balance Verification

Ferrite content is measured and recorded on each duplex stainless steel batch to confirm the target 35–55% ferrite range per ASTM E1077 / ASTM A800. Deviations trigger material review and additional testing, ensuring consistent microstructure for corrosion-critical and sour-service environments.

Duplex Stainless Steel Traceability Documents Available with Every Order

Heat / Melt Number
Batch / Lot Number
Chemical Analysis Report
Tensile & Hardness Report
Heat Treatment Record
Ferrite Content Certificate
Ultrasonic Test (UT) Report
PMI (XRF) Report
Packing List & Dimensions
Country of Origin Certificate
Track Record

Trusted Worldwide

Since 1998, Hunan Fushun Metal has built a reputation in the global duplex stainless steel market through consistent quality, on-time delivery, and technical support that goes well beyond the data sheet.

1998
Year Founded
52+
Export Countries
400+
Technical Staff
100K t
Annual Capacity
25+
Duplex Grades

We have been sourcing super duplex 2507 round bar for offshore riser components for several years. The material consistently meets NORSOK M-630 requirements, and the EN 10204 3.2 documentation is thorough. Lead times are predictable — exactly what critical project schedules demand.

M. Eriksen
Materials Engineer  ·  Oil & Gas, Norway

We ordered 2205 flat bar and plate for a large reactor vessel project and needed PED-compliant material with full traceability. The documentation package was complete — heat records, mechanical certificates, UT reports — no chasing, no surprises on delivery day.

S. Wagner
Procurement Manager  ·  Chemical Process, Germany

Our desalination project required Zeron 100 tube blanks cut to length with tight tolerances. The team understood the ASTM A276 requirement without lengthy back-and-forth, pricing was competitive, and delivery was on schedule despite a complex multi-port logistics setup.

A. Al-Rashidi
Senior Buyer  ·  Desalination Project, UAE
Common Questions

Frequently Asked Questions About Duplex Stainless Steel

Duplex 2205 (UNS S31803/S32205, EN 1.4462) is the most widely used grade with a Pitting Resistance Equivalent Number (PREN) of approximately 35. It suits moderately aggressive chloride environments — process piping, offshore structural steel, pressure vessels — at operating temperatures below about 250 °C.

Super duplex SAF 2507 (UNS S32750, EN 1.4410) has a minimum PREN of 42, a higher yield strength (≥550 MPa vs. ≥450 MPa for 2205), and significantly better resistance to pitting, crevice corrosion, and stress corrosion cracking. It is engineered for the most demanding environments: seawater injection, deep-sea downhole equipment, and high-chloride chemical reactors. The trade-offs are higher material cost and more controlled welding procedures.

Every shipment is accompanied by a Mill Test Certificate (MTC) per EN 10204 3.1 as standard. This includes heat number, chemical composition by heat analysis, mechanical test results (yield, UTS, elongation, hardness), heat treatment records, and ferrite content where applicable.

EN 10204 3.2 certificates countersigned by an accredited third party (SGS, Bureau Veritas, Intertek, TÜV) are available on request. Additional documents such as UT inspection reports, PMI (XRF) results, corrosion test reports (ASTM G48, ASTM A262 Practice E), and NACE compliance statements can be included based on your project specification.

Yes. In addition to standard mill stock, we supply cut-to-length round bar, saw-cut plate, machined billets, disc forgings, and custom-profiled sections to drawing. Our 4,500–8,000-tonne hydraulic presses and GFM precision forging machines produce large-diameter blocks, stepped shafts, and flanging-quality discs in all major duplex stainless steel grades.

For non-stock items, a minimum order of 3 metric tons applies. Tolerances and surface finish are agreed at quotation stage. Send your drawing, material specification (grade, standard, form, dimensions, quantity) to [email protected] for a rapid technical review and quotation.

Standard grades including duplex 2205 (S32205), SAF 2507 (S32750), LDX 2101 (S32101), and SAF 2304 (S32304) are held in stock in commonly ordered sizes and ship within 7–15 business days following order confirmation and payment receipt.

Custom dimensions, non-stock grades (such as 2707 HD, 3207 HD, DP-3), or orders requiring special heat treatment, additional NDT, or third-party inspection typically carry a 20–30 calendar day lead time. Contact us directly for expedited scheduling on urgent requirements.

Yes. Super duplex grades are specifically designed for seawater service. SAF 2507 (PREN ≥42) and Zeron 100 / S32760 (PREN ≥40) have Critical Pitting Temperatures (CPT) exceeding 50 °C in 6% ferric chloride (ASTM G48), far exceeding the performance of 316L (typical CPT 15–20 °C). Both grades are approved under NACE MR0175 / ISO 15156 for sour service and widely qualified under NORSOK M-630.

For cathodically protected subsea environments, Hydrogen-Induced Stress Cracking (HISC) guidelines should be followed regarding austenite spacing and applied stress. Contact our technical team for project-specific recommendations.

For in-stock material, the minimum order is one piece or bar — no minimum tonnage for stock items. For custom-manufactured or non-stock dimensions, a minimum of 3 metric tons per line item applies.

Mixed-grade and mixed-form shipments are fully supported. Multiple duplex stainless steel grades can be consolidated into a single container, each clearly marked and documented with individual Mill Test Certificates. This is standard practice for procurement projects that cover multiple application areas simultaneously.

Get a Quote

Request a Quote for Duplex Stainless Steel

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]