Improvement Measures for Transverse Charpy Impact Strength of Hot Work Tool Steel 1.2344

Improvement Measures for Transverse Charpy Impact Strength of Hot Work Tool Steel 1.2344 As a high-quality heat-resistant tool steel, 1.2344 is known for its uniform composition, good hardenability, excellent machinability, high toughness, hardness, low-temperature wear resistance, and high-temperature fatigue resistance. It is particularly widely used in die-casting

Read more →

The control of cleanliness during the electroslag remelting (ESR) process of die steel 1.2083

The control of cleanliness during the electroslag remelting (ESR) process of die steel 1.2083 is as follows: Die steel is an important industrial material widely used in aerospace, automotive manufacturing, electronics, toys, medical devices, and many other fields. To improve the cleanliness, wear resistance, and impact resistance

Read more →

The control of inclusions during the electroslag remelting (ESR) process of duplex stainless steel F55

The control of inclusions during the electroslag remelting (ESR) process of duplex stainless steel F55 is as follows: Duplex stainless steel F55 has high strength, good formability and weldability, excellent resistance to localized corrosion and stress corrosion cracking caused by chlorides. Typical applications include petrochemicals, fertilizer industries,

Read more →

The effect of aging treatment on the room temperature and low-temperature mechanical properties of 15-5PH stainless steel

The effect of aging treatment on the room temperature and low-temperature mechanical properties of 15-5PH stainless steel is as follows: 15-5PH stainless steel (05Cr15Ni5Cu4Nb) is a martensitic precipitation-hardening stainless steel. Due to its high strength, good toughness, and corrosion resistance, it is widely used in load-bearing structural

Read more →

Electroslag Remelting (ESR) Purity Control of 1.2083 Mold Steel

Electroslag Remelting (ESR) Purity Control of 1.2083 Mold Steel Mold steel is an important industrial material widely used in aerospace, automotive manufacturing, electronics, toys, medical devices, and many other fields. To improve the cleanliness, wear resistance, and impact resistance of this steel to meet user requirements, research

Read more →

The difference about Cast and Forged Steel

The difference about Cast and Forged Steel   Steel products may be manufactured either by casting or forging steel. Steel casting is the process by which a metal is heated until it reaches a liquid state and then poured into a mold that shapes the desired product. Steel

Read more →

Steel and Other Heat-Resistant Metal Qualities

Steel and Other Heat-Resistant Metal Qualities There are several major factors that you may be considering for any project that involves metal materials, and heat resistance is often on this list. Whether a project itself is carried out in high heat conditions or it’s expected that the

Read more →

Broad Basics on the World of Metal Finishing

Broad Basics on the World of Metal Finishing There are a few concepts or processes that are simply vital within the world of metal manufacturing and metalwork, and one of the most notable here is finishing. Finishing is a broad category that speaks to various treatments used

Read more →

HOW DOES ULTRASONIC INSPECTION WORK?

HOW DOES ULTRASONIC INSPECTION WORK?   Ultrasonic inspection normally involves the use of a piezo electric transducer which is both a transmitter and receiver of ultrasound. The transducer must be coupled to the item to be inspected, as ultrasound at the frequency used is not transmitted in air.

Read more →

Machining of nickel base corrosion and temperature resistant alloys

Machining of nickel base corrosion and temperature resistant alloys   Nickel base corrosion and temperature resistant alloys are classified as moderate to difficult when machining, however these alloys can be machined using conventional production methods at satisfactory rates. During the machining processes these alloys work harden rapidly, generate

Read more →

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x