What is the difference between 718H mold steel and P20H mold steel?

What are the characteristics of 718H mold steel? What are the characteristics of P20 die steel? What is the difference between 718 mold steel and P20H mold steel?   A: 718H mold steel, corresponding to Chinai’s 3Cr2NiMo mold steel. **Features** 718H is an improved steel grade of

Read more →

We Had a Fantastic Tourism to ZhangJiaJie! Sharing Scenery!

After a tense half-year working time, our boss, Ms Folance, arranged a tour for all employees. From August 14th to 17th, we spent four pleasant days in Zhangjiajie, Hunan Province. We passed through beautiful, tall, and steep natural attractions and experienced the unique local humanistic feelings: Tianmenshan National Forest Park

Read more →

Why is duplex stainless steel used in the cooling water system of nuclear power plants?

The World Nuclear Association’s annual report shows that the global nuclear power generation in 2018 exceeded 250 billion kWh, accounting for 10.5% of the global power supply. As of June 2019, 54 nuclear power plants are under construction worldwide. As a clean energy, nuclear power is a

Read more →

China Successfully Produced Super Large 30CrMnSiNi2A Steel For Ship

30CrMnSiNi2A belongs to low-alloy ultra-high-strength steel, which is obtained by adding 1.4% to 1.8% Ni on the basis of high-strength steel 30CrMnSiA. Due to the addition of Ni, the toughness and plasticity of steel are improved, and the hardenability of steel is greatly improved. Parts with a

Read more →

Fushun Delivered SUS420J2 Cold Rolled Hardened Polished Stainless Strips Order!

We, Fushun Metal, delivered a order of SUS420J2 cold rolled +quenched+tempered+polished stainless steel strip for Egypt clients. Thickness from 1.0 to 2.0 mm and Width from 200 to 300mm. We controlled the tolerance of thickness in the gap of -0, +0.025~+0.045mm and surface roughness Ra0.8μm.   Here

Read more →

Properties and Applications of NAK80 plastic mould Steel

NAK80 plastic mould steel, a Ni Al Cu precipitation age-hardening steel, is characterized by high polishability. NAK80 plastic mould steel is sulphurized to give the steel good machinability, mirror finish and electrical discharge machinability, with good The weldability of the welded part of the hardness first decreases,

Read more →

Intoduce Tool steel Grade Group

Intoduce Tool steel Grade Group Tool steel refers to a spread of steel and steel that are particularly well-suited to be made into tools. Their suitability comes from their distinctive hardness, resistance to abrasion and deformation, and their ability to carry a leading edge at elevated temperatures.

Read more →

Several Ways To Identify Quality Of Different Stainless Steel

There are many different ways to identify stainless steel, common ways to identify stainless steel materials are the following. First, according to the source of stainless steel to identify the stainless steel materials are the following methods. 1, to identify the imported or steel factory ordered stainless

Read more →

Stainless Steel Corrosion Resistance

1 What kind of corrosion does stainless steel have? Among the many industrial applications, stainless steel offers corrosion resistance that is satisfactory today. According to the experience of use, in addition to mechanical failure, stainless steel corrosion is mainly manifested in: a serious form of corrosion of

Read more →

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x