Inconel® 625 Nickel Alloy – AMS 5666 – UNS N06625

Inconel® 625 Nickel Alloy – AMS 5666 – UNS N06625

Nickel Alloy 625, frequently called Inconel® 625, is a corrosion and heat-resistant Nickel-based alloy.

It is alloyed with Chromium and Iron, along with Niobium-Tantalum and Molybdenum for increased toughness and strength. It is nonmagnetic, and corrosion and oxidation-resistant, with service temperatures ranging from cryogenic to 1800°F. Because of its alloy matrix, precipitation hardening treatments are not required. This alloy is generally double-melted, with either EF-AOD melt (Electric Furnace followed by Argon Oxygen Decarburization) or VIM (Vacuum Induction Melt); and with a second melt by either VAR (Vacuum Arc Remelt), or ESR (Electroslag Reduction).

 

This alloy exhibits excellent corrosion resistance to salt and fresh water, alkaline environments, and air. It is resistant to both oxidizing and non-oxidizing environments, and chloride stress corrosion cracking. Chloride stress corrosion cracking resistance is excellent. The alloy resists scaling and oxidation at high temperatures.

<<Inconel® 625 Nickel Alloy – AMS 5666 – UNS N06625 DATA SHEET>>

Chemical Composition:

Symbol Element Min % Max %
C Carbon 0.10%
Mn Manganese 0.50%
Si Silicon 0.50%
P Phosphorus 0.015%
S Sulfur 0.015%
Cr Chromium 20.00% 23.00%
Mo Molybdenum 8.00% 10.00%
Cb (Nb) Columbium (Niobium) 3.15% 4.15%
Co Cobalt 1.00%
Ti Titanium 0.40%
Al Aluminum 0.40%
Fe Iron 5.00%
Ni Nickel remainder

Annealed Longitudinal Tensile Properties per AMS 5666

Property Up to 4″, incl. Over 4″ to 10″, incl.
Tensile Strength 120 ksi 110 ksi
Yield Strength 0.2% offset 60 ksi 50 ksi
Elongation in 4D 30% 25%
Hardness 287 Bhn max 287 Bhn max

 

Inconel®625 Nickel Applications:

Nickel Alloy 625 aerospace applications include jet engine exhaust systems, propeller blades, heat exchangers, and aircraft applications. It’s also used for heat shields, furnace hardware, chemical plant equipment, and seawater applications.

 

Common Trade Names:

Nickel 625

625 Alloy

CarTech Pyromet® Alloy 625

W-No 2.4856

ISO NW6625

Inconel 625

Haynes 625

Nickelvac 625

Nicrofer 6020

Altemp 625

Chronic 625

 

Common Specifications:

AMS 5666 Bars, Forgings, Extrusions

AMS 5599 Sheet, Strip, Plate

AMS 5837 Welding Wire

AMS 5869 Sheet, Strip, Plate

ASTM B446

ASME SB446

ASTM B564

MS 5837

ASME SB443 Gr 1, SB446 Gr 1

ASTM B443 Gr 1, B446 Gr 1

EN 2.4856

ISO 15156-3

NACE MR0175-3

UNS N06625

Werkstoff 2.4856

DIN 17752

Rod, Bar, Wire and Forging Stock

 

We also supply
MARS190 D6AC AMS 4130
AMS 4340 MOD AMS 4340 AMS 4330 MOD
AMS 9310 AMS 13-8 PH AMS 15-5 PH
AMS 17-4 PH AMS 625 AMS 718
AerMet® 100 Maraging 250 Maraging 300
Maraging 350 Titanium Grade 5 Ti-6Al-4V ELI Titanium

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x