JIS G4053 covers low alloyed steels for machine structural use — the Japanese grades that appear on drawings from Japanese-affiliated plants across Asia: SCM, SNCM, SCr and SMn series.
The series, and what they correspond to
| JIS series | Alloy type | Common equivalent |
|---|---|---|
| SCM | Cr-Mo | SCM440 = 4140 / 42CrMo4; SCM415 = 4118 |
| SNCM | Ni-Cr-Mo | SNCM439 = 4340; SNCM220 = 8620 |
| SCr | Cr only | SCr420 = 5120 |
| SMn | Mn only | SMn433 = 1330 |
The correspondence is close enough that mills publish them side by side, and loose enough that a substitution should be agreed rather than assumed — the specified ranges differ, particularly in nickel and molybdenum.
The H suffix
Grades written SCM440H carry hardenability limits rather than composition alone. That is the JIS equivalent of the AISI H grades, and it is what makes the steel predictable in a part whose section varies. For any quenched and tempered component with more than one section size, the H grade is the safer order.
What to put on the order
- JIS grade, with or without the H suffix
- Condition: hot rolled, annealed, or quenched and tempered
- Whether an ASTM or EN equivalent is acceptable, and which one governs
- Mechanical properties, if the part is supplied heat treated
Download the standard
JIS G4053 — Low alloyed steels for machine structural use (PDF)
Related reading
- SCM440 — the grade behind most 4140 orders from Asia.
- SCM415 — the carburising grade in the same series.
- Standards library — the full index.