manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Sanicro 28 Alloy | N08028 | 1.4563 | Super Austenitic | Fushun Metal

Sanicro 28 N08028 super austenitic stainless steel tube and bar products
Sanicro 28 N08028 tubes & bars

Sanicro 28 / N08028 / 1.4563 — Introduction

Sanicro 28, designated UNS N08028 and EN 1.4563 (also known as Alloy 28, Incoloy alloy 28, or Nicrofer 3127 LC), is an ultra-low-carbon, high-chromium super austenitic stainless steel occupying the performance gap between conventional 904L/254 SMO grades and full nickel-based corrosion alloys such as Inconel 625. With 26–28% chromium—one of the highest levels in any commercially available wrought austenitic grade—combined with 30–34% nickel, 3–4% molybdenum, and 0.6–1.4% copper, it delivers outstanding resistance to sulfuric acid, wet-process phosphoric acid, chloride pitting and crevice corrosion (PREN 32–35), and chloride stress corrosion cracking. Its iron-based matrix (Fe ~33–37%) provides significant cost advantages over pure nickel alloys while retaining near-immunity to Cl−-SCC, making it the most widely used high-alloy austenitic tubular material in sour gas well downhole service and phosphoric acid evaporation plants worldwide.

At Fushun Metal, Sanicro 28 is manufactured through a fully integrated triple-melt route under one roof. VIM primary melting under high vacuum ensures precise recovery of copper and ultra-low carbon content (≤0.020%), eliminating the risk of intergranular chromium carbide precipitation during welding or hot-forming. The VIM electrode passes to VAR, where controlled directional solidification yields chemically homogeneous, low-inclusion electrode stock with minimal micro-segregation—critical for the high chromium content. For the most demanding sour-service and phosphoric acid applications where sulfide-initiated pitting and fluoride-assisted crevice attack are the life-limiting mechanisms, we deploy PESR as the final stage, achieving deep desulfurization and oxide refinement through argon-shielded reactive slag chemistry.

Every heat is solution-annealed, quenched, and tested within Fushun Metal’s certified quality management system—ISO 9001 for manufacturing process control and AS9120B for aerospace distribution traceability. Full digital traceability links each production lot from melt heat number through remelt sequence, hot-working reduction ratio, and final annealing batch. Standard deliverables include intergranular corrosion testing per ASTM A262 Practice C, pitting corrosion testing per ASTM G48 Method A, ultrasonic inspection, chemical re-verification by optical emission and LECO combustion, and room-temperature tensile testing. Mill test certificates to EN 10204 3.1 or 3.2 accompany every shipment.

Equivalent Grades of Sanicro 28 Across International Standards

Sanicro 28 is codified under multiple national and international specification systems. The table below maps its designations and governing standards across major markets. Fushun Metal certifies to all listed specifications and can dual-certify heats where required.

Country / System Designation Key Standards
USA (ASTM/ASME) N08028 / Alloy 28 ASTM B668 (Seamless Tube), B709 (Plate/Sheet), B829 (General Requirements); ASME SB-668, SB-709
Europe (EN) 1.4563 / X1NiCrMoCu31-27-4 EN 10088-2, EN 10088-3, EN 10272
Germany (DIN/W.Nr.) 1.4563 / X1NiCrMoCuN31-27-4 DIN 17456, DIN 17458
France (AFNOR) Z1NCDU31-27-03 NF A49-217
China (GB) NS3401 / 00Cr27Ni31Mo3Cu GB/T 15007
Sweden (Trademark) Sanicro 28 (Sandvik) Proprietary; conforms to UNS N08028 / EN 1.4563

Applications of Sanicro 28

Sanicro 28 fills the critical engineering gap where 904L and duplex stainless steels reach their corrosion limits but the cost of full nickel-based alloys such as C-276 or 625 cannot be justified. Its combination of ultra-high chromium for oxidizing-acid resistance, copper for reducing-acid passivation, and high nickel for chloride SCC immunity makes it the default specification for wet-process phosphoric acid plants and deep sour gas well production tubing and liners.

Phosphoric Acid Production

Wet-process H3PO4 evaporator tubes and shells, filter feed tanks, concentrator heat exchangers, gypsum slurry piping, and fluorine-containing off-gas scrubbers in fertilizer-grade phosphoric acid complexes.

Sour Gas Well Downhole

Cold-worked production tubing and liners for deep sour gas wells (H2S + CO2 + Cl− + elemental sulfur at >150°C). Cold-worked yield strengths up to 140 ksi for high-collapse and burst-rated tubular strings.

Sulfuric Acid Equipment

Sulfuric acid coolers, dilution and distribution piping, acid-regeneration heat exchangers, and spent-acid recovery systems across a wide range of H2SO4 concentrations and temperatures.

Seawater Cooling & Marine

Seawater-cooled heat exchanger tubes and tube sheets, condenser waterboxes, once-through cooling piping, desalination brine heater tubes, and marine-platform firewater and deluge systems.

Pollution Control & FGD

Flue-gas desulfurization quench and absorber sections, wet electrostatic precipitator tubes, chimney liners, and ductwork in coal-fired and waste-to-energy plant FGD systems handling condensing acid vapors.

Nuclear & Chemical Processing

Nuclear fuel reprocessing dissolver off-gas condensers, radioactive waste evaporator tubes, chemical reactor internal coils, pickling acid heating bundles, and high-purity acid distillation columns.

Sanicro 28 — Supply Range by Fushun Metal

Fushun Metal stocks and processes Sanicro 28 across all major mill forms from a single integrated facility. Our in-house 6000-ton hydraulic open-die press, 1800-ton precision radial forger (GFM), and multi-stand 850/550/350/250 rolling mills enable a broad dimensional envelope without outsourcing—ensuring uninterrupted lot traceability from melt to delivery under ISO 9001 and AS9120B. All material is supplied in the solution-annealed condition per ASTM B668 / B709 (typically 1070–1120°C, rapid water quench). Cold-worked high-strength tubulars for downhole sour-gas service are also available. Intergranular corrosion testing per ASTM A262 Practice C and pitting corrosion testing per ASTM G48 Method A are standard on every heat. Products are accompanied by mill test certificates to EN 10204 3.1 or 3.2. Welding consumable: ERNiCrMo-3 (Alloy 625 type) or ERNiCrMo-13 (Alloy 59 type) filler; matching ENiCrMo-3/ENiCrMo-13 electrodes.

Rolled Round Bar

Diameter 5 mm – 250 mm. Length 2,000 – 6,000 mm. Solution-annealed per EN 10088-3 / ASTM B829. Peeled, centerless ground, or hot-rolled finish. Supplied as straight random lengths or precision cut-to-order.

Plate & Sheet

Thickness 0.5 mm – 60 mm. Width up to 2,500 mm, length up to 8,000 mm. Solution-annealed and descaled per ASTM B709 / EN 10088-2. Surface: No.1, 2B, or 2D. Plasma/laser/waterjet cut-to-size available.

Seamless Tube & Downhole Tubular

OD 6 mm – 300 mm, wall 0.8 mm – 40 mm. Length up to 14 m per ASTM B668. Annealed or cold-worked high-strength grades. Hydrostatic tested. Sour-service NACE MR0175/ISO 15156 qualified.

Forged Bar & Butt-Weld Fittings

Forged round bar OD 80 mm – 600 mm. Tube fittings: elbows, tees, reducers, stub ends per ASTM A403. Flanges per EN 1092-1. Rough-turned or finish-machined. UT inspected. EN 10204 3.1 certified.

Chemical Composition of Sanicro 28 — ASTM B668 / EN 10088-2

All heats produced by Fushun Metal are melted via VIM+VAR or VIM+PESR and verified against the composition limits below by optical emission spectrometry and LECO combustion analysis. Full chemical certificates are issued with every shipment under ISO 9001 and AS9120B quality management. The 26–28% chromium plateau is the highest available among commercial wrought super austenitic stainless steels and is the primary driver of the alloy’s exceptional oxidizing-acid and pitting resistance (PREN ≈ 32–35). The deliberate copper addition (0.6–1.4%) stabilizes the passive film in reducing-acid environments—particularly dilute to medium-concentration sulfuric acid—where chromium alone is insufficient.

Element Ni Cr Mo Cu Fe C Mn
Wt.% 30.0–34.0 26.0–28.0 3.0–4.0 0.6–1.4 Bal. ≤0.020 ≤2.5
Element Si N P S
Wt.% ≤0.7 ≤0.05 ≤0.030 ≤0.010

Mechanical Properties of Sanicro 28 — Per Product Form

Sanicro 28 is a solid-solution-strengthened, fully austenitic alloy; all mechanical properties in the annealed condition are developed through solution annealing at 1070–1120°C followed by rapid water quenching. The alloy is not hardenable by precipitation heat treatment. Its high chromium content combined with the fully austenitic matrix provides a unique combination of strength, ductility, and corrosion resistance. For downhole sour-gas tubular applications, the alloy can be cold-worked to achieve minimum yield strengths of 110–140 ksi (760–965 MPa) while retaining adequate ductility and full NACE MR0175 / ISO 15156 compliance for H2S service.

Fushun Metal performs all solution annealing in-house under calibrated furnace controls with rapid water-quench capability. The ultra-low carbon content (≤0.020%) eliminates the risk of sensitization during welding, and post-weld solution annealing is generally not required for corrosion resistance—though stress relief at 950–1000°C may be applied for cold-worked components. Welding parameters: ERNiCrMo-3 or ERNiCrMo-13 filler, heat input 0.5–1.5 kJ/mm, interpass temperature <100°C, argon-based shielding gas with backing purge. Post-weld pickling and passivation are recommended to restore full surface corrosion resistance.

Physical constants: Density 8.0 g/cm³; Melting range 1350–1410°C; Hardness ≤155 HB / 70–90 HRB (annealed condition); Modulus of elasticity 200 GPa at 20°C; Thermal conductivity 14.5 W/m·K at 20°C; Coefficient of thermal expansion ~15 μm/m·°C (20–100°C); PREN (Cr + 3.3Mo + 16N) 32–35. The alloy is non-magnetic due to its fully austenitic structure.

Product Form Condition Tensile Strength (MPa) Yield Strength (MPa) Elongation (%) Hardness
Bar & Forgings Annealed ≥500 (typ. 550–700) ≥214 (typ. 250–350) ≥40 (typ. 45–55) ≤155 HB
Plate & Sheet (B709) Annealed ≥500 (typ. 550–650) ≥214 (typ. 250) ≥40 (typ. 45) 70–90 HRB
Seamless Tube (B668) Annealed ≥500 ≥214 ≥40 70–90 HRB
Seamless Tube (B668) Cold-Worked ≥760 (typ. 760–900) ≥760 (typ. 760–965) ≥10 ≤33 HRC
Butt-Weld Fittings (A403) Annealed ≥500 ≥214 ≥40 ≤155 HB

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!