Lateral Wave Testing Issues and Solutions in Forgings

Surface cracks were visually discovered on wire-cut samples taken from the platform section of aluminum alloy forgings. Metallographic inspection attributed the cracking to excessive residual stress during the cutting process and grain boundary weakening caused by second-phase precipitation. To confirm whether similar defects exist in other forgings,