1.2340 MOD ESR Steel Overview

1.2340 MOD ESR is a premium modified hot work tool steel produced through the Electro Slag Remelting (ESR) process. As a leading steel manufacturer, FUSHUN SPECIAL STEEL has optimized the chemical composition of this grade to deliver enhanced performance compared to standard 1.2340 steel. The addition of nickel and refined vanadium content provides superior thermal fatigue resistance and improved toughness at elevated temperatures.

This modified grade bridges the gap between conventional H11/H13 steels and high-performance grades, offering an excellent balance of hot hardness, thermal conductivity, and wear resistance. The ESR process ensures exceptional cleanliness, homogeneous microstructure, and consistent mechanical properties throughout the material.

1.2340 MOD ESR Applications and Uses

Die Casting Industry

Aluminum and magnesium die casting dies, die inserts, cores, and related tooling requiring excellent thermal fatigue resistance and extended service life.

Forging Applications

Hot forging dies, press forging tools, hammer forging dies, and upsetting tools for steel and non-ferrous metal processing operations.

Extrusion Tooling

Extrusion dies for aluminum, copper, and brass profiles, mandrels, liners, and dummy blocks requiring high hot strength.

Plastic Mold Components

High-temperature plastic injection mold components, hot runner systems, and tooling for processing engineering plastics.

1.2340 MOD ESR Chemical Composition (%)

C Si Mn P S Cr Mo V Ni
0.32-0.40 0.10-0.30 0.10-0.50 ≤0.012 ≤0.005 4.60-5.40 1.10-1.60 0.35-0.60 0.15-0.25

Note: Ultra-low sulfur (≤0.005%) and phosphorus (≤0.012%) content achieved through FUSHUN SPECIAL STEEL’s advanced ESR refining process ensures superior cleanliness and isotropic properties.

1.2340 MOD ESR Mechanical Properties

Hardness After Heat Treatment

Condition Hardness (HRC) Hardness (HB)
Annealed (Supply Condition) ≤229
Hardened and Tempered 44-52

Typical Mechanical Properties at Working Hardness (48-50 HRC)

Property Value Unit
Tensile Strength 1550-1750 MPa
Yield Strength (0.2%) 1350-1500 MPa
Elongation ≥10 %
Impact Toughness (Unnotched) 25-40 J

1.2340 MOD ESR Heat Treatment Guidelines

Annealing (Soft Annealing)

Heat slowly to 800-850°C, hold for adequate time (approximately 1 hour per 25mm thickness), then furnace cool at a rate not exceeding 20°C/hour to 500°C. Final cooling can be done in air. Expected hardness: ≤229 HB.

Stress Relieving

After rough machining, heat to 600-650°C, hold for 2 hours per 25mm of thickness, then cool slowly in furnace to 500°C before air cooling. This process relieves machining stresses before final hardening.

Hardening (Austenitizing)

Preheat in two stages: first to 450-500°C, then to 850-900°C. Austenitize at 1000-1040°C with adequate soaking time. Quench in oil, air, or polymer quenchant depending on section size. Air cooling is recommended for complex dies to minimize distortion.

Tempering

Temper immediately when the tool reaches approximately 50-70°C. Double tempering is required, with each cycle at 550-620°C for minimum 2 hours. Cool to room temperature between tempering cycles. For 48-50 HRC working hardness, temper at 580-600°C. The nickel addition enhances secondary hardening response.

1.2340 MOD ESR Equivalent Steel Grades

1.2340 MOD ESR is a modified grade developed for enhanced performance. Below are similar standard grades for reference. Contact FUSHUN SPECIAL STEEL for detailed comparison and technical consultation.

Standard Country/Region Equivalent Grade
DIN / EN / ISO Germany / Europe 1.2340 (X38CrMoV5-1), 1.2343 (Similar)
ASTM / AISI USA H11 Modified
JIS Japan SKD6 Modified
GB China 4Cr5MoSiV Modified
BS United Kingdom BH11 Modified

1.2340 MOD ESR Available Forms and Sizes

As a professional tool steel manufacturer, FUSHUN SPECIAL STEEL produces 1.2340 MOD ESR through hot rolling and hot forging processes. We offer comprehensive product forms to meet diverse industrial requirements.

Product Form Process Standard Sizes
Round Bar Hot Rolled / Hot Forged Φ20-600mm
Flat Bar Hot Rolled / Hot Forged Thickness 20-300mm × Width 50-800mm
Plate / Block Hot Forged Thickness 50-500mm (Custom sizes available)
Wire Rod Hot Rolled Φ5.5-25mm

For special dimensions, customized shapes, or large volume orders, please contact our technical team for consultation.

Why Choose FUSHUN SPECIAL STEEL as Your Manufacturer

Integrated Melting Capabilities

As a true steel manufacturer, we operate our own melting facilities including ESR (Electro Slag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting) for producing premium and ultra-clean steel grades.

In-House Heat Treatment

Complete heat treatment facilities under one roof ensure consistent quality and faster delivery times. We control every step from annealing to hardening and tempering, guaranteeing reliable mechanical properties.

Machining Services Available

Our turning and grinding facilities provide bright bars and precision-machined surfaces. This saves downstream customers significant time and processing costs while ensuring dimensional accuracy.

Bulk Order Specialist

We welcome large volume orders and long-term supply agreements. Our manufacturing capacity and inventory management systems ensure stable supply and competitive pricing for bulk purchasers.

Request a Quote for 1.2340 MOD ESR Steel

FUSHUN SPECIAL STEEL is your reliable manufacturer for premium hot work tool steel. Whether you need standard stock sizes or custom specifications, our team is ready to assist with your requirements.

Visit www.fushunspecialsteel.com to explore our complete product range and submit your inquiry today.

© FUSHUN SPECIAL STEEL – Professional Tool Steel Manufacturer | Quality · Reliability · Service

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x