Steel Grade Introduction and Applications

1.3244 is a premium spray forming high speed steel grade that combines exceptional wear resistance with superior toughness. This tungsten-molybdenum high speed steel manufactured using advanced spray forming technology offers excellent performance for demanding cutting applications. The spray forming process creates a refined microstructure with uniform carbide distribution, resulting in enhanced tool performance and extended service life.

As a leading manufacturer, FUSHUN SPECIAL STEEL specializes in producing high-quality 1.3244 spray forming steel for precision cutting tools, forming dies, and high-performance machine components in aerospace, automotive, and manufacturing industries.

Spray Forming Process Advantages

Process Features:

  • Rapid Solidification: Ultra-fast cooling creates fine microstructures
  • Homogeneous Structure: Eliminates macro-segregation completely
  • Near-Net Shape: Reduces material waste significantly
  • Enhanced Properties: Superior mechanical performance

Performance Benefits:

  • Superior Hardness: Enhanced cutting edge retention
  • Excellent Toughness: Reduced tool breakage risk
  • Uniform Carbides: Consistent particle distribution
  • Extended Tool Life: Outstanding wear resistance

1.3244 Chemical Composition (wt%)

Element C W Mo Cr V Co
1.3244 1.25-1.35 5.1-5.6 5.4-5.7 4.3-4.5 2.9-3.2 4.7-4.9

Note: Chemical composition optimized for spray forming process to achieve superior microstructural uniformity

Physical Properties at Different Temperatures

Property 20°C 400°C 600°C
Density (kg/m³) 8100 8000 8000
Elastic Modulus (MPa) 230,000 205,000 184,000
Thermal Expansion (×10⁻⁴/°C) 11.6 11.9
Thermal Conductivity 24 28 27
Specific Heat (J/kg·°C) 420 510 600

Heat Treatment Process

Softening Annealing

  • Temperature: 860-900°C
  • Hold time: 4 hours
  • Cool to 600°C in furnace
  • Hardness: ≤280HB

Stress Relief

  • Temperature: 600-700°C
  • Hold time: 4 hours
  • Slow cooling
  • After rough machining

Hardening

  • Preheat: 400-500°C
  • Austenitize: 1200-1220°C
  • Quench in air/oil/salt
  • Hardness: 64-66 HRC

Tempering

  • Temperature: 550-570°C
  • Multiple cycles (2-3x)
  • Hold time: 1 hour each
  • Air cooling

Recommended Heat Treatment for Different Tools:

Tool Type Hardening Temp (°C) Tempering Temp (°C)
Single Point Tools 1210 550-570
Multi Point Tools 1170-1210 550-570
Dies 1120-1170 550-570

Available Forms and Specifications

Coils & Strips

  • Thickness: ⌀95-300mm
  • Width: Custom slitting
  • Precision tolerance control
  • Surface finish options

Round Bars

  • Diameter: ⌀8-95mm
  • Length: up to 6000mm
  • Ground or turned finish
  • Straightness guaranteed

Plates & Flats

  • Thickness: (3.5-20)×(16-65)mm
  • Width: ⌀2.5-16.5mm
  • Length: custom lengths
  • Machined to specification

Special Shapes

  • Squares: (50-300)×(10-300)mm
  • Rectangles: (20-200)×(5-80)mm
  • Custom profiles available
  • Near-net-shape forming

Applications of 1.3244 Spray Forming Steel

Cutting Tools

Milling cutters, drill bits, taps, reamers, gear cutters

Knives & Blades

Industrial knives, steel cutting blades, shear blades

Forming Tools

Punches, dies, cold forming tools, extrusion dies

Wear Parts

Wear plates, high-temperature components

Spray Forming vs Conventional Steel Performance Comparison

Property Conventional HSS Spray Forming HSS Improvement
Hardness 62-64 HRC 64-66 HRC +3-5%
Wear Resistance Standard Superior +25-40%
Toughness Good Excellent +15-30%
Red Hardness 58-60 HRC@600°C 60-62 HRC@600°C +3-5%
Tool Life Baseline Extended +30-50%

Technical Advantages

Steel Properties:

  • Excellent wear resistance: Superior carbide distribution
  • High red hardness: Maintains performance at high temperatures
  • Good machinability: Easier processing in annealed state
  • Uniform structure: Consistent properties throughout
  • High toughness: Reduced tool breakage

Manufacturing Benefits:

  • Near-net shape: Minimal material waste
  • Improved yield: Higher material utilization
  • Better surface finish: Reduced finishing requirements
  • Dimensional accuracy: Tighter tolerances achievable
  • Cost effective: Reduced processing time

Quality Assurance & Certifications

ISO Certified

International quality standards compliance

Material Testing

Complete chemical & mechanical analysis

Traceability

Full material certificates provided

Technical Support

Expert guidance & application support

Important Notes & Recommendations

1. Material Selection: Choose appropriate material grade based on specific cutting requirements and application demands.

2. Machining: Use appropriate cutting parameters and coolants to improve tool life during machining operations.

3. Heat Treatment: Follow proper heat treatment procedures to achieve optimal hardness and maintain dimensional stability. Avoid overheating to prevent CBN formation.

4. Storage: Store in dry conditions to prevent corrosion and maintain surface quality.

About FUSHUN SPECIAL STEEL

FUSHUN SPECIAL STEEL is a leading manufacturer specializing in high-quality 1.3244 spray forming high speed steel production. With decades of experience in metallurgy and advanced manufacturing technologies, we provide superior steel products to customers worldwide. Our state-of-the-art spray forming technology ensures consistent quality and exceptional performance.

Our commitment to innovation and quality has made us a trusted partner for industries requiring premium tool steels. We continuously invest in research and development to improve our production processes and deliver products that exceed customer expectations.

Advanced Technology

State-of-the-art spray forming equipment

Global Supply

Worldwide shipping and distribution

Custom Solutions

Tailored products for specific applications

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x