1.4420, S31655, Stainless Steel


1.4420 S31655 Stainless Steel Manufacturer and Supplier

Professional Manufacturing by FUSHUN SPECIAL STEEL | High Performance Alloy Solutions

1.4420 S31655 Stainless Steel Manufacturer & Supplier | FUSHUN SPECIAL STEEL

1. Introduction and Applications of 1.4420 S31655

FUSHUN SPECIAL STEEL is a premier manufacturer and exporter specializing in high-grade stainless steels, including the robust 1.4420 (S31655) grade. As a leader in the special steel industry since 1998, we utilize advanced smelting technologies to provide materials that meet rigorous international standards.

Grade 1.4420, often associated with the UNS S31655 designation, is a high-alloy austenitic stainless steel. It is characterized by its distinct chemical composition which typically includes Nitrogen additions to enhance strength and corrosion resistance compared to standard 316 types. This steel is engineered to withstand aggressive environments while maintaining excellent formability and weldability.

Typical Applications

Due to its superior properties, 1.4420 S31655 is widely used in industries requiring durability and resistance to pitting and crevice corrosion. Common applications include:

Chemical Processing: Storage tanks, piping systems, and heat exchangers handling organic acids and chlorides.
Marine Environments: Components exposed to seawater and salt atmospheres requiring higher resistance than 316L.
Construction: Structural components in coastal architecture and water treatment facilities.
Pulp and Paper: Bleaching equipment and digesters where high corrosion resistance is mandatory.

At FUSHUN SPECIAL STEEL, we ensure that every batch of 1.4420 S31655 produced meets the specific demands of these critical industries.

2. Chemical Composition of 1.4420 S31655

The chemical balance of 1.4420 S31655 is strictly controlled during our smelting process to ensure optimal performance. The addition of Nitrogen is key to its enhanced mechanical properties.

Grade C (Carbon) Si (Silicon) Mn (Manganese) P (Phosphorus) S (Sulfur) Cr (Chromium) Ni (Nickel) Mo (Molybdenum) N (Nitrogen)
1.4420 / S31655 ≤ 0.030% ≤ 1.00% ≤ 2.00% ≤ 0.045% ≤ 0.015% 16.5 – 18.5% 10.5 – 13.5% 2.0 – 3.0% 0.12 – 0.22%

*Note: Compositions may vary slightly based on specific standard requirements (ASTM/EN). Please consult our sales engineers for exact heat analysis.

3. Mechanical Properties

1.4420 S31655 exhibits higher yield strength than conventional austenitic stainless steels due to solid solution strengthening from Nitrogen. Below are typical properties at room temperature.

Property Value (Typical) Unit
Tensile Strength (Rm) 600 – 850 MPa
Yield Strength (Rp0.2) ≥ 290 MPa
Elongation (A5) ≥ 40 %
Hardness (HB) ≤ 215 HB

4. Heat Treatment of 1.4420 S31655

Proper heat treatment is essential to restore the corrosion resistance and mechanical properties of the steel after hot working. FUSHUN SPECIAL STEEL provides materials in the solution annealed condition unless otherwise specified.

  • Solution Annealing: Heat to a temperature range of 1040°C – 1120°C.
  • Quenching: Rapid cooling in water or air (depending on section thickness) is required to prevent the precipitation of chromium carbides, ensuring maximum corrosion resistance.

5. Equivalent Grades and Standards

We manufacture 1.4420 S31655 in accordance with major international standards to ensure global compatibility.

Region / Standard Grade Designation
Europe (EN / DIN) 1.4420 / X5CrNiMo18-11
USA (ASTM / UNS) S31655 (Related to Type 316LN variants)
Japan (JIS) SUS 316LN (Equivalent category)
China (GB) 022Cr17Ni12Mo2N

6. Supply Forms and Dimensions

As a comprehensive manufacturer, FUSHUN SPECIAL STEEL offers 1.4420 S31655 in a variety of shapes and conditions. We are equipped to handle large-scale production for both Hot Rolled and Hot Forged products.

Round Bar

Process: Hot Rolled / Hot Forged

Diameter: 10mm – 800mm

Surface: Black, Peeled, Polished, or Turned

Flat Bar & Block

Process: Hot Rolled / Forged

Thickness: 20mm – 500mm

Width: 200mm – 1200mm

Plate & Sheet

Process: Hot Rolled

Thickness: 3mm – 100mm

Dimensions: Standard or Custom Cut

Wire & Coil

Process: Cold Drawn / Hot Rolled

Diameter: 0.5mm – 20mm

Condition: Annealed, Pickled

Customization: We understand that every project is unique. If you require special dimensions or tight tolerances not listed above, please contact us. We welcome bulk orders and custom inquiries.

7. Why Choose FUSHUN SPECIAL STEEL?

Choosing FUSHUN SPECIAL STEEL means partnering with a manufacturer that controls the entire production lifecycle. Our commitment to quality ensures you receive the best 1.4420 S31655 material available.

Advanced Smelting

We possess state-of-the-art smelting facilities including EAF, LF, VD, and VOD. For high-end requirements, we utilize ESR (Electro-Slag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting) to ensure high purity and superior internal structure of the steel.

In-House Heat Treatment

Quality stability is our priority. We perform all heat treatment processes in-house. This allows us to strictly control mechanical properties and microstructure, ensuring consistent quality across batches and faster delivery times.

Value-Added Processing

To save our customers time and machining costs, we offer extensive cold processing services. We can supply materials that are turned, peeled, milled, or ground to precise tolerances, ready for your immediate production use.

Global Experience

With an industrial presence in over 18 countries and decades of experience since 1998, our technically trained sales engineers provide extensive product knowledge and application support. We are experts in handling large-volume international orders.

Ready to Order 1.4420 S31655?

Contact FUSHUN SPECIAL STEEL today for a competitive quote. We are your reliable manufacturer for special steel, tool steel, and stainless steel.

Email: [email protected] | Tel: +86-731-89903933

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x