manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

1.4731, X40CrSiMo10-2, SUH3, Valve Stainless Steel

 

1.4731 X40CrSiMo10-2 Valve Steel – Premium Martensitic Solution

High-Performance SUH3 Valve Steel for Internal Combustion Engines by FUSHUN SPECIAL STEEL

Steel Grade Introduction and Applications

FUSHUN SPECIAL STEEL proudly presents 1.4731 (X40CrSiMo10-2), a premium martensitic valve steel specifically engineered for internal combustion engine applications. This high-performance steel grade complies with EN 10090:1998 standards for valve steels and alloys, making it the preferred choice for automotive and industrial engine manufacturers worldwide.

As a leading manufacturer, FUSHUN SPECIAL STEEL specializes in producing 1.4731 SUH3 valve steel for demanding engine valve applications. Our manufacturing capabilities ensure exceptional heat resistance, wear resistance, and mechanical strength required for high-temperature engine environments. We welcome large-volume orders from automotive manufacturers and engine component suppliers.

Key Applications: Engine exhaust valves, intake valves, valve seats, and other high-temperature engine components requiring superior mechanical properties and oxidation resistance.

Chemical Composition – EN 10090:1998

Element Carbon (C) Silicon (Si) Manganese (Mn) Nickel (Ni)
Content (%) 0.36 – 0.45 2 – 3 max 0.8 max 0.5
Element Sulfur (S) Chromium (Cr) Molybdenum (Mo)
Content (%) max 0.04 9.5 – 11.5 0.8 – 1.3

Precise composition control ensures optimal performance in high-temperature engine environments

Available Processing Types

Hot Rolled

Premium hot rolled 1.4731 valve steel with excellent dimensional accuracy and superior mechanical properties, manufactured using advanced rolling technology for consistent quality.

Hot Forged

Precision hot forged components with optimized grain structure and enhanced mechanical performance, ideal for critical valve applications requiring maximum strength and durability.

FUSHUN SPECIAL STEEL – Your trusted manufacturer for automotive industry large-volume orders with guaranteed quality.

Available Shapes for Valve Manufacturing

Round Bars

Precision round bars for valve stem machining and component manufacturing

Flat Bars

High-quality flat bars for valve head manufacturing and specialized components

Plates

Heavy plates for valve seat manufacturing and large component production

Wire

Precision wire products for specialized valve components and springs

Available Sizes and Custom Manufacturing

Standard Inventory Sizes

FUSHUN SPECIAL STEEL maintains extensive inventory of standard valve steel sizes for immediate delivery to automotive manufacturers. Our comprehensive stock includes common dimensions for all product shapes, ensuring rapid response to urgent production requirements.

Request our current stock list and competitive pricing for bulk orders. As a dedicated manufacturer serving the automotive industry, we specialize in large-volume supply agreements and can provide detailed quotations for annual requirements.

Custom Size Manufacturing

Beyond standard dimensions, FUSHUN SPECIAL STEEL offers comprehensive custom manufacturing services for specialized valve applications. Our advanced production facilities can accommodate unique specifications and dimensional requirements.

Consult our engineering team for custom production capabilities and lead times. We excel in large-scale automotive manufacturing projects and provide complete technical support for your valve steel requirements.

Mechanical Properties (Heat Treated Condition)

Property Value Unit Condition
Tensile Strength (Rm) 900-1100 MPa +QT
0.2% Proof Strength (Rp0.2) 700 MPa +QT
Min. Elongation at Fracture (A) 14 % +QT
Reduction in Cross Section (Z) 40 % +QT
Brinell Hardness (HB) 266-325 HB +QT
Brinell Hardness (HB) 300 HB +A

Heat Treatment Codes: +QT = Quenched and Tempered, +A = Annealed
Note: Mechanical properties achieve optimal performance after proper heat treatment, ensuring maximum valve service life.

Heat Treatment Specifications

Quenching and Tempering (+QT)

Optimal heat treatment for valve applications requiring maximum strength and toughness. Our controlled quenching and tempering process ensures consistent mechanical properties.

Achieves: 900-1100 MPa tensile strength with excellent ductility

Annealing (+A)

Stress relief annealing for improved machinability and dimensional stability during manufacturing processes.

Achieves: 300 HB hardness for optimal machining characteristics

FUSHUN SPECIAL STEEL Manufacturing Excellence

Advanced Smelting Technology

State-of-the-art ESR (Electroslag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting) technologies ensure ultra-clean steel with superior valve performance characteristics.

Precision Heat Treatment

In-house controlled atmosphere heat treatment facilities with precise temperature control ensure consistent valve steel properties and optimal performance in engine environments.

Automotive Industry Focus

Specialized expertise in automotive valve steel requirements with rapid delivery capabilities and quality assurance programs designed for high-volume automotive production.

Complete Processing Services

Comprehensive machining and surface finishing services reduce downstream processing time and costs, delivering ready-to-use valve steel components to automotive manufacturers.

Automotive Industry Manufacturing Partner

FUSHUN SPECIAL STEEL is your premier manufacturer for 1.4731 X40CrSiMo10-2 valve steel. We specialize in large-volume automotive production with stringent quality control and reliable supply chain management.

Partner with us for your valve steel requirements – contact our automotive sales team today.

Physical Properties

Property Value Unit
Density 7.7 g/cm³

Optimal density for valve applications requiring strength-to-weight balance

Ready to Partner? Contact FUSHUN SPECIAL STEEL

Join leading automotive manufacturers who trust FUSHUN SPECIAL STEEL for their 1.4731 valve steel requirements. As your dedicated manufacturer, we provide comprehensive support for large-scale automotive production projects.

Contact our automotive division today for technical consultation and competitive bulk pricing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x