Valve Steel Grade Introduction and Applications

FUSHUN SPECIAL STEEL proudly presents 1.4748 (X85CrMoV18-2), a premium martensitic valve steel specifically engineered for the most demanding high-performance internal combustion engine applications. This superior valve steel grade fully complies with EN 10090:1998 standards for valve steels and alloys, making it the preferred choice for racing engines, heavy-duty industrial engines, and high-performance automotive applications worldwide.

As a leading manufacturer specializing in premium valve steel production, FUSHUN SPECIAL STEEL produces 1.4748 X85CrMoV18-2 valve steel for critical high-temperature engine valve applications. Our manufacturing capabilities ensure exceptional heat resistance, superior strength, and outstanding wear resistance required for extreme engine environments. We welcome large-volume orders from performance engine manufacturers, racing teams, and heavy-duty equipment producers.

Key Valve Steel Applications: High-performance exhaust valves, racing engine valves, heavy-duty industrial engine valves, turbocharged engine components, and other extreme high-temperature valve applications requiring maximum strength and durability.

Chemical Composition – EN 10090:1998 Valve Steel Specification

Element Carbon (C) Silicon (Si) Manganese (Mn) Phosphorus (P)
Content (%) 0.8 – 0.9 max 1 max 1.5 max 0.04
Element Sulfur (S) Chromium (Cr) Molybdenum (Mo) Vanadium (V)
Content (%) max 0.03 16.5 – 18.5 2 – 2.5 0.3 – 0.6

Advanced alloy composition ensures exceptional high-temperature performance and extended valve service life

Available Valve Steel Processing Types

Hot Rolled Valve Steel

Premium hot rolled 1.4748 valve steel with exceptional dimensional accuracy and superior mechanical properties, manufactured using advanced rolling technology for consistent high-performance valve steel quality.

Hot Forged Valve Steel

Precision hot forged valve steel components with optimized grain structure and enhanced mechanical performance, ideal for critical high-performance valve applications requiring maximum strength and extreme temperature resistance.

FUSHUN SPECIAL STEEL – Your trusted valve steel manufacturer for high-performance automotive and racing applications.

Available Valve Steel Shapes for High-Performance Manufacturing

Round Bars

Precision round valve steel bars for high-performance valve stem machining and racing component manufacturing

Flat Bars

High-quality flat valve steel bars for performance valve head manufacturing and specialized engine components

Plates

Heavy valve steel plates for valve seat manufacturing and large high-performance component production

Wire

Precision valve steel wire products for specialized valve components and high-performance engine applications

Available Valve Steel Sizes and Custom Manufacturing Solutions

Standard Valve Steel Inventory

FUSHUN SPECIAL STEEL maintains comprehensive inventory of standard valve steel sizes for immediate delivery to high-performance engine manufacturers and racing teams. Our extensive stock includes common dimensions for all valve steel shapes, ensuring rapid response to urgent racing and performance engine production requirements.

Request our detailed valve steel stock list and competitive pricing for bulk performance orders. As a dedicated valve steel manufacturer serving the high-performance automotive and racing industry, we specialize in large-volume supply agreements for premium valve steel applications.

Custom Valve Steel Manufacturing

Beyond standard dimensions, FUSHUN SPECIAL STEEL offers comprehensive custom valve steel manufacturing services for specialized high-performance applications. Our state-of-the-art production facilities can accommodate unique specifications for racing engines and industrial high-performance applications.

Consult our valve steel engineering team for custom production capabilities and lead times. We excel in large-scale high-performance valve steel manufacturing projects and provide complete technical support for your critical valve steel requirements.

Mechanical Properties (Heat Treated Valve Steel Conditions)

Property Value Unit Condition
Tensile Strength (Rm) 1000-1200 MPa +QT
0.2% Proof Strength (Rp0.2) 800 MPa +QT
Min. Elongation at Fracture (A) 7 % +QT
Reduction in Cross Section (Z) 12 % +QT
Brinell Hardness (HB) 296-355 HB +QT
Brinell Hardness (HB) 300 HB +A

Heat Treatment Codes: +QT = Quenched and Tempered, +A = Annealed
Note: Superior mechanical properties achieved through precise valve steel heat treatment ensure maximum valve performance and extended service life in extreme high-performance engine applications.

Heat Treatment Specifications for High-Performance Valve Steel

Quenching and Tempering (+QT)

Advanced heat treatment for high-performance valve applications requiring maximum strength, toughness, and extreme temperature resistance. Our precisely controlled valve steel quenching and tempering process ensures consistent mechanical properties and exceptional valve reliability.

Achieves: 1000-1200 MPa tensile strength with superior high-temperature stability for racing and performance applications

Annealing (+A)

Specialized stress relief annealing for improved valve steel machinability and dimensional stability during precision valve manufacturing processes, ensuring optimal machining characteristics for complex valve geometries.

Achieves: 300 HB hardness for superior valve steel machining characteristics and precision surface finish

FUSHUN SPECIAL STEEL Valve Steel Manufacturing Excellence

Advanced Valve Steel Smelting

State-of-the-art ESR (Electroslag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting) technologies ensure ultra-clean valve steel with superior performance characteristics and extended service life in extreme engine conditions.

Precision Valve Steel Heat Treatment

In-house controlled atmosphere heat treatment facilities with precise temperature control ensure consistent valve steel properties, optimal microstructure, and reliable performance in demanding high-performance engine environments.

High-Performance Engine Focus

Specialized expertise in high-performance valve steel requirements with rapid delivery capabilities, quality assurance programs, and technical support designed specifically for racing, performance automotive, and heavy-duty industrial applications.

Complete Valve Steel Processing

Comprehensive machining and surface finishing services reduce downstream processing time and costs, delivering ready-to-use valve steel components with precision dimensions to high-performance engine manufacturers and racing teams.

High-Performance Valve Steel Manufacturing Partner

FUSHUN SPECIAL STEEL is your premier valve steel manufacturer for 1.4748 X85CrMoV18-2 high-performance valve steel. We specialize in large-volume production for racing, performance automotive, and industrial applications with stringent quality control and global delivery capabilities.

Partner with us for your high-performance valve steel requirements – contact our specialized valve steel division today.

Physical Properties

Property Value Unit
Density 7.7 g/cm³

Optimal density providing excellent strength-to-weight ratio for high-performance valve applications

Ready for High-Performance? Contact FUSHUN SPECIAL STEEL

Join leading racing teams and high-performance engine manufacturers worldwide who trust FUSHUN SPECIAL STEEL for their 1.4748 X85CrMoV18-2 valve steel requirements. As your dedicated valve steel manufacturer, we provide comprehensive support for extreme performance valve applications.

Contact our high-performance valve steel division today for technical consultation and competitive bulk pricing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x