manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

2.4952, Nimonic 80A, NiCr20TiAl, N07080, Valve Nickel Alloy

 

2.4952 Alloy 80A NiCr20TiAl N07080 Nickel Alloy – Premium Precipitation Hardening Valve Material

High-Temperature Resistant Exhaust Valve Nickel Alloy for Gas Turbines and Power Plant Applications by FUSHUN SPECIAL STEEL

2.4952 Alloy 80A NiCr20TiAl N07080 Nickel Alloy Introduction and Applications

FUSHUN SPECIAL STEEL is a leading manufacturer of 2.4952 (Alloy 80A, NiCr20TiAl, N07080) high-temperature resistant, precipitation hardenable Ni-Cr nickel alloy specifically engineered for demanding valve applications up to 800°C. This premium nickel-chromium alloy exhibits excellent creep strength and resistance against thermal changes, making it ideal for exhaust valves in gas turbines, steam generators, and power plant applications.

As a dedicated manufacturer, FUSHUN SPECIAL STEEL specializes in producing high-quality 2.4952 Alloy 80A NiCr20TiAl N07080 nickel alloy with optimized titanium and aluminum content for enhanced precipitation hardening characteristics. Our advanced VIM (Vacuum Induction Melting) technologies ensure ultra-clean materials and consistent performance for large-volume production requirements in high-temperature valve manufacturing.

Primary High-Temperature Nickel Alloy Applications

  • Exhaust valves for gas turbines operating up to 800°C
  • Steam generator valve components for power plants
  • Turbine blades and valve assemblies
  • Turbocharger valve systems requiring scaling resistance
  • High-temperature fasteners and bolting elements for valve assemblies
  • Industrial valve components for high mechanical loads at elevated temperatures

International Nickel Alloy Grade Equivalents

DIN UNS ASTM Common Name
2.4952 N07080 B637 Alloy 80A
DIN EN Standards Designation
EN 10269, EN 10302, DIN 17742 NiCr20TiAl

International Recognition: 2.4952 Alloy 80A is globally recognized across DIN, UNS, and ASTM standards, ensuring worldwide compatibility and acceptance in high-temperature valve manufacturing industries and gas turbine applications as a premium nickel alloy.

2.4952 Alloy 80A Chemical Composition

C % Si % Mn % P % S %
0.04-0.10 max 1.00 max 1.00 max 0.020 max 0.015
Cr % Ni % Ti % Al % Fe %
18.0-21.0 ≥ 65.0 1.8-2.7 1.0-1.8 max 1.50

2.4952 Alloy 80A Enhanced Nickel Alloy Composition: High nickel content (≥65%) provides excellent high-temperature strength and corrosion resistance. Chromium (18-21%) ensures oxidizing resistance up to 1000°C. Titanium (1.8-2.7%) and aluminum (1.0-1.8%) enable precipitation hardening for superior valve performance.

2.4952 Alloy 80A Mechanical Properties

Yield Strength
(N/mm²)
Tensile Strength
(N/mm²)
Elongation
(%)
Impact
(J)
≥ 620 1000-1300 ≥ 20 ≥ 20

Condition: Solution annealed and precipitation hardened (+AT +P)
2.4952 Alloy 80A Nickel Alloy Valve Performance: Exceptional tensile strength of 1000-1300 N/mm² combined with minimum yield strength of 620 N/mm² makes this nickel alloy ideal for high-stress valve applications in gas turbines and power plants operating up to 800°C.

Heat Treatment for Valve Manufacturing

Solution Annealing

Temperature: 1050-1080°C

Duration: 8 hours

Cooling: Air cooling

1st Precipitation

Temperature: 840-860°C

Duration: 24 hours

Cooling: Air cooling

2nd Precipitation

Temperature: 690-710°C

Duration: 16 hours

Cooling: Air cooling

Multi-Step Precipitation Hardening Process

The comprehensive three-step heat treatment process optimizes 2.4952 Alloy 80A nickel alloy for demanding valve applications. Solution annealing homogenizes the structure, while dual precipitation hardening develops fine titanium and aluminum precipitates for exceptional strength up to 800°C.

Key Properties for Valve Applications

High-Temperature Resistance

Excellent creep strength and scaling resistance up to 1000°C. Designed for high mechanical loads at elevated temperatures up to 800°C, making this nickel alloy ideal for exhaust valve applications.

Corrosion Resistance

Superior resistance against corrosion in oxidizing media. High chromium content (18-21%) provides exceptional oxidation resistance essential for valve components in harsh operating environments.

Ultra-Clean Quality

High inner cleanliness achieved using VIM and PESR-treatment ensures superior material purity for critical nickel alloy valve applications requiring maximum reliability and performance.

Processing Types We Provide

Hot Rolled

Premium hot rolled 2.4952 Alloy 80A nickel alloy with exceptional dimensional accuracy and superior mechanical properties for valve manufacturing applications. Our manufacturing process ensures consistent precipitation hardening response.

Hot Forged

Precision hot forged components with optimized grain structure for critical 2.4952 Alloy 80A nickel alloy valve applications. As a manufacturer, we control the entire forging process for superior gas turbine valve components.

Available Shapes for Manufacturing

Round Bars

Precision round bars for 2.4952 nickel alloy valve stem manufacturing

Flat Bars

High-quality flat bars for valve head manufacturing

Plates

Heavy plates for large power plant component production

Wire

Precision wire for specialized fasteners and valve applications

Available Sizes and Custom Manufacturing

Standard Inventory Sizes

FUSHUN SPECIAL STEEL maintains comprehensive inventory of standard 2.4952 Alloy 80A nickel alloy sizes for immediate delivery to gas turbine and power plant valve manufacturers. Our extensive stock ensures rapid response to urgent production requirements for large-volume orders.

Request our detailed stock list and competitive pricing for bulk high-temperature nickel alloy orders.

Custom Size Manufacturing

Beyond standard dimensions, FUSHUN SPECIAL STEEL offers comprehensive custom manufacturing services for specialized 2.4952 Alloy 80A nickel alloy valve applications with large-volume requirements.

Consult our engineering team for custom production capabilities and lead times.

FUSHUN SPECIAL STEEL Manufacturing Advantages

Advanced Melting Technology

We operate VIM, ESR, and VAR technologies, ensuring ultra-clean 2.4952 Alloy 80A nickel alloy production with precise titanium and aluminum control for consistent precipitation hardening performance.

In-House Heat Treatment

Our heat treatment facilities ensure stable quality and fast delivery times. Complete control over solution annealing and dual precipitation hardening processes guarantees optimal valve performance up to 800°C.

Precision Finishing Services

We provide in-house turning and grinding services for 2.4952 Alloy 80A nickel alloy products, delivering ready-to-use valve components with superior surface finish and dimensional accuracy.

Large-Volume Manufacturing

As a leading manufacturer, we welcome large-volume orders for 2.4952 Alloy 80A nickel alloy materials and offer competitive pricing for bulk requirements for gas turbine projects.

Leading 2.4952 Alloy 80A Nickel Alloy Manufacturer

FUSHUN SPECIAL STEEL is your premier manufacturer for 2.4952 Alloy 80A NiCr20TiAl N07080 precipitation hardening nickel alloy. We deliver advanced solutions for demanding gas turbine and power plant valve applications with large-volume manufacturing capabilities up to 800°C service temperature.

Experience the 2.4952 Alloy 80A nickel alloy advantage – contact our team today.

Ready for 2.4952 Alloy 80A Nickel Alloy Excellence?

Join gas turbine and power plant manufacturers worldwide who trust FUSHUN SPECIAL STEEL for premium 2.4952 Alloy 80A precipitation hardening nickel alloy solutions. As your dedicated manufacturer, we provide advanced nickel-chromium alloy technology with large-volume manufacturing capabilities for 800°C high-temperature applications.

Contact our 2.4952 Alloy 80A nickel alloy specialists today for technical consultation and competitive bulk pricing.

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]