manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

2Cr13 20Cr13 S42020 Stainless Steel

2Cr13 20Cr13 S42020 Stainless Steel

2Cr13 20Cr13 S42020 Stainless Steel

2Cr13 Stainless Steel Introduction

Chinese 2Cr13 steel (20Cr13) is a martensitic stainless steel with magnetic properties, good corrosion resistance and high hardness in the quenched state.

 

2Cr13 stainless steel is used in a wide range of applications, such as cutting tools, surgical tools, and steam turbine blades, material density is 7.75g/cm3, 2Cr13 is an old representation, the new representation is 20Cr13.

 

Steel Grade Designation Of 20Cr13 = 2Cr13 Stainless Steel

20 (or 2) – Average carbon content: 20/10,000 (0.2%), old designation is 2/1,000

Cr – Chromium symbol

13 – Average content of chromium: 13%

 

2Cr13 Material Equivalent

China   USA   Germany   Japan  
Standard Grade Standard Grade (UNS) Standard Grade Standard Grade
GB/T 1220; 20Cr13 AISI, 420 DIN EN 10088-2; X20Cr13 (1.4021) JIS G4303 SUS 420J1

 

Chemical Composition Of (20Cr13) 2Cr13 Stainless Steel

C Si (≤) Mn (≤) P (≤) S (≤) Cr Ni (≤)
0.16 – 0.25 1 1 0.04 0.03 12.00 – 14.00 -0.6

 

(20Cr13) 2Cr13 Steel Mechanical Properties

For Hot Rolled Steel Bar After Quenching and Tempering

Tensile strength: 640 N/mm2

Conditional yield strength (Non-proportional extension strength): ≥440 N/mm2

Elongation: ≥20%

Rate of reduction in area: ≥50%

Impact energy: ≥63 Aku2 (J)

Material hardness:

HBW: ≤ 223 (After annealing);

HBW: ≥ 192 (After quenching and tempering)

Notes:

Data is for steel diameter (d) less than or equal to 75mm.

1 N/mm2 = 1 MPa

 

Physical Properties

Density (g/cm3): 7.75

Melting point: 1470-1510℃

Specific heat capacity (J/Kg·K): 460 at 0-100℃

Thermal conductivity (W/m·K):

22.2 at 100℃

26.4 at 500℃

Coefficients of linear thermal expansion (10-6/K):

10.3 (0-100℃)

12.2 (0-500℃)

Electrical Resistivity (μΩ·m): 0.55 at 20℃

Longitudinal modulus of elasticity (kN/mm2): 200 at 20℃

 

Heat Treatment

Annealing: 800-900℃ (Slow cooling)

Quenching: 920-980℃ (Cooling: Oil)

Tempering: (600-750℃) (Rapid cooling)

 

We also supply :

1.2510/H10, 1.2842, 1.2379/D2, 1.2080/X210Cr12/D3, 1.2436, 1.2365, 1.2885, 1.2343, 1.2344/H13/SKD61, 1.2581/H21, 1.2709, 1.2345, 1.2738/P20NI, 1.2083/420J2, 1.2316, 1.2312/P20S, 1.2311, 1.2764

For all products, please check here: Fushun products

 

Fushun Metal · ISO 9001 · AS9120B
Send the grade, size and standard.

You get chemical composition, mechanical properties and a price — with inspection certificates to EN 10204 3.1 issued against the heat number.

Request a quoteWhatsApp +86 178 7358 1838

[email protected]  ·  +86 731 8990 3933

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]