manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

310Si2, X8CrNiSI25-21, S38340, Stainless Steel

310Si2, X8CrNiSI25-21, S38340, Ultra High Temperature Stainless Steel

Extreme Temperature Performance 900-1200℃ | FUSHUN SPECIAL STEEL


Superior High-Temperature Performance Steel Grade

310Si2 stainless steel manufactured by FUSHUN SPECIAL STEEL is an advanced austenitic stainless steel designed for extreme high-temperature applications. This premium grade exhibits exceptional high-temperature strength and thermal stability, making it the preferred choice for industrial applications operating at temperatures between 900-1200℃.

As a direct manufacturer, FUSHUN SPECIAL STEEL specializes in producing 310Si2 stainless steel with superior creep resistance and long-term durability. The steel demonstrates sensitivity to sulfur-containing environments and may exhibit precipitation-induced embrittlement at temperatures between 600-800℃, but excels in higher temperature ranges.

International Grade Designations

Chinese Standard: S38340 • 16Cr25Ni20Si2 • 1Cr25Ni20Si2

International: SUS314 (JIS) • 1.4841 (DIN) • X8CrNiSI25-21 (EN)

Advanced Alloy Design for Extreme Temperatures

310Si2’s exceptional performance at extreme temperatures is achieved through precise alloy engineering. The elevated chromium and silicon content work synergistically to enhance thermal stability and oxidation resistance.

Key Alloying Elements Function

  • Cr: Increases FeO formation temperature, enhances high-temperature chemical stability
  • Si: Improves thermal stability, ferrite-forming element for structural integrity
  • Ni: Stabilizes austenitic structure, enhances plasticity, prevents brittle phase precipitation

Superior Temperature Performance

  • •Operating Range: 900-1200℃ continuous use
  • •Creep Resistance: Exceptional long-term strength
  • •Thermal Stability: Stable microstructure at high temperatures

Optimized Chemical Composition

FUSHUN SPECIAL STEEL maintains precise control over 310Si2 chemical composition to ensure optimal high-temperature performance and thermal stability:

Element Symbol Content (%) High-Temperature Function
Carbon C ≤0.20 Controlled for optimal high-temperature strength
Silicon Si 1.50~2.50 Enhanced thermal stability and oxidation resistance
Chromium Cr 24.00~27.00 Superior high-temperature oxidation resistance
Nickel Ni 18.00~21.00 Austenitic stability and ductility at high temperatures
Manganese Mn ≤1.50 Controlled for optimal thermal properties

Mechanical Properties and Heat Treatment

Mechanical Properties

  • •Tensile Strength: ≥520 MPa
  • •Yield Strength: ≥205 MPa
  • •Elongation: ≥40%
  • •Reduction of Area: ≥50%

Heat Treatment Parameters

  • •Solution Treatment: 1080-1130℃
  • •Cooling Method: Rapid cooling
  • •Annealing: 1020-1100℃
  • •Hardness: ≤187HBW, ≤90HRB

Advanced Heat Treatment Capabilities

FUSHUN SPECIAL STEEL provides comprehensive heat treatment services designed to optimize 310Si2’s microstructure for extreme temperature applications. Our high-temperature annealing processes ensure stable grain structure and superior mechanical properties for long-term service at 900-1200℃.

Stress Relief: Eliminates processing stresses | Microstructure Stabilization: Optimized for thermal cycling | Grain Control: Enhanced creep resistance

FUSHUN SPECIAL STEEL Manufacturing Excellence

As a leading manufacturer of 310Si2 stainless steel, FUSHUN SPECIAL STEEL offers comprehensive in-house production capabilities. We welcome large volume orders and provide customized solutions for extreme temperature applications.

Available Product Forms

Round Bars: Ø10mm – Ø300mm

Flat Bars: 15×25mm – 100×250mm

Plates: 5mm – 60mm thickness

Forgings: Custom dimensions available

Quality Assurance

State: Solution treated and pickled

Testing: Complete chemical and mechanical testing

Certification: Mill test certificates provided

Traceability: Full material traceability

Specialized manufacturing for extreme temperature applications – Contact FUSHUN SPECIAL STEEL for custom specifications

Extreme Temperature Applications

310Si2 stainless steel from FUSHUN SPECIAL STEEL is specifically engineered for applications requiring exceptional performance at extreme temperatures between 900-1200℃. The steel’s superior creep resistance and thermal stability make it indispensable for critical high-temperature industrial components.

Industrial Furnace Components

Furnace chains, heating elements, structural components, and conveyor systems for extreme temperature processing.

Power Generation Equipment

Industrial boilers, electric furnaces, kilns, and high-temperature steam generation systems.

Aerospace and Automotive

Jet engine components, exhaust systems, catalytic converter housings, and thermal barrier applications.

Petrochemical Processing

High-temperature reactor components, thermal processing equipment, and refinery applications.

Why Choose 310Si2 for Extreme Temperature Applications?

• Superior Creep Resistance: Exceptional long-term strength at high temperatures

• Thermal Cycling Stability: Maintains integrity through repeated heating cycles

• Oxidation Resistance: Forms protective oxide layer at extreme temperatures

• Microstructural Stability: Resists grain growth and phase changes

Partner with FUSHUN SPECIAL STEEL for Extreme Temperature Solutions

Ready to specify 310Si2 stainless steel for your extreme temperature applications? As a leading manufacturer with advanced production capabilities, we provide competitive pricing for large volume orders and custom manufacturing solutions. Contact our technical team for material specifications, performance data, and application engineering support.

FUSHUN SPECIAL STEEL – Your Trusted Partner for Extreme Temperature Stainless Steel Solutions

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.