660, S66286, Alloy A-286, Stainless Steel


660 / S66286 / Alloy A-286 – High Temperature Special Steel Manufacturer

660 / S66286 / Alloy A-286 Stainless Steel Manufacturer | Fushun Special Steel

Welcome to FUSHUN SPECIAL STEEL, a premier manufacturer and supplier of high-performance special steels. We specialize in the production of 660 (S66286 / Alloy A-286), an iron-based superalloy known for its exceptional strength and corrosion resistance at elevated temperatures. As a direct manufacturer, we welcome large-scale industrial orders and ensure strict quality control from melting to final delivery.

For inquiries and quotes, please visit https://www.fushunspecialsteel.com.

1. Introduction and Applications of Grade 660 / S66286

Alloy A-286 (UNS S66286), also commonly referred to as Grade 660, is a precipitation-hardening, austenitic stainless steel designed for use at temperatures up to 1300°F (704°C), where high tensile strength, excellent creep strength, and good corrosion resistance are required. It is an iron-base alloy containing nickel and chromium, reinforced with titanium and aluminum for precipitation hardening.

At FUSHUN SPECIAL STEEL, we produce this alloy to meet rigorous industry demands. Its non-magnetic properties and high strength make it versatile for various critical sectors.

Key Applications:

  • Aerospace: Jet engine components, fasteners, and springs.
  • Power Generation: Industrial gas turbine components, blades, and vanes.
  • Automotive: High-performance engine fasteners and supercharger components.
  • Oil & Gas: Non-magnetic cryogenic equipment and deep-well drilling tools.

2. Chemical Composition

The chemical composition of S66286 is carefully controlled during our smelting process to ensure optimal response to heat treatment.

Element Min (%) Max (%)
Carbon (C) – 0.08
Manganese (Mn) – 2.00
Silicon (Si) – 1.00
Phosphorus (P) – 0.025
Sulfur (S) – 0.025
Chromium (Cr) 13.50 16.00
Nickel (Ni) 24.00 27.00
Molybdenum (Mo) 1.00 1.50
Titanium (Ti) 1.90 2.35
Aluminum (Al) – 0.35
Vanadium (V) 0.10 0.50
Boron (B) 0.003 0.010
Iron (Fe) Balance

3. Mechanical Properties

The mechanical properties of Alloy A-286 depend heavily on the heat treatment condition. Below are typical properties for solution treated and aged material (Type 2).

Property Typical Value (Room Temp)
Tensile Strength ≥ 895 MPa (130 ksi)
Yield Strength (0.2% Offset) ≥ 585 MPa (85 ksi)
Elongation ≥ 15%
Reduction of Area ≥ 20%
Hardness 248 – 341 HBW

4. Heat Treatment

Proper heat treatment is crucial to unlocking the potential of 660 / S66286. FUSHUN SPECIAL STEEL provides materials in various conditions, including solution annealed or fully aged.

  • Solution Treatment: Heat to 980°C (1800°F), hold for 1 hour, followed by rapid cooling (oil or water quench). This dissolves the hardening phases.
  • Aging (Precipitation Hardening): Heat to 700°C – 760°C (1300°F – 1400°F), hold for 16 hours, then air cool. This precipitates the Titanium/Aluminum phases that strengthen the alloy.

5. Similar Grades and Standards

Our production adheres to major international standards. We can certify our 660 steel to the following specifications:

Region Standard / Grade
USA (ASTM/AISI/UNS) ASTM A453 Gr 660, UNS S66286, Alloy A-286, AMS 5731, AMS 5732, AMS 5737
Europe (EN/DIN) 1.4980, X6NiCrTiMoVB25-15-2
UK (BS) HR 51, HR 52
Japan (JIS) SUH 660
China (GB) 0Cr15Ni25Ti2MoAlVB

6. Supply Forms and Dimensions

As a comprehensive manufacturer, FUSHUN SPECIAL STEEL offers flexible supply options. We can produce Hot Rolled and Hot Forged materials.

Check our full product range at https://www.fushunspecialsteel.com.

Shape Process Size Range (mm)
Round Bar Hot Rolled Ø 16mm – Ø 150mm
Round Bar Forged Ø 150mm – Ø 800mm
Flat Bar / Block Forged / Rolled Thickness: 20mm – 400mm
Width: 50mm – 800mm
Plate / Sheet Hot Rolled Thickness: 5mm – 100mm
Wire / Coil Cold Drawn Ø 1.0mm – Ø 15mm

*Custom sizes and specific tolerance requirements are available upon request. Please contact our sales team for details.*

7. Why Choose FUSHUN SPECIAL STEEL?

We are not just a trader; we are a manufacturer with complete control over the production lifecycle. Here are our core advantages:

1. Advanced Smelting Technology

For high-end alloys like S66286, purity is paramount. We utilize EAF + LF + VD for basic melting, followed by ESR (Electro-Slag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting). This ensures low gas content, minimal inclusions, and superior microstructure.

2. In-House Heat Treatment

We possess our own industrial heat treatment furnaces. This allows us to precisely control solution annealing and aging processes, ensuring the mechanical properties (yield strength, hardness) meet your exact specifications without relying on third parties.

3. Machining Services

To save our customers time and costs, FUSHUN SPECIAL STEEL offers value-added services. We can provide materials that are Turned (Peeled), Milled, or Grinded. This “Ready-to-Use” surface condition reduces your machining workload.

4. Manufacturer Direct & Fast Delivery

Buying directly from the factory means competitive pricing and better communication. We maintain a stock of ingots and semi-finished billets, allowing us to fulfill orders with short lead times. We welcome bulk orders from global distributors and end-users.

Contact Us Today

For premium 660 / S66286 Alloy A-286 steel, trust the experts at Fushun Special Steel Co., Ltd.

Email: [email protected]

Website: https://www.fushunspecialsteel.com

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x