7Cr17MoV Steel

7Cr17MoV High Carbon Stainless Steel

7Cr17MoV

7Cr17MoV

7CR17MOV special high-carbon stainless steel chromium produces an invisible but very dense chromium oxide film, preventing corrosion of the steel and making the tool durable. Molybdenum is mainly used to strengthen the corrosion effect of chromium in steel and keep the cutting tool sharp. Vanadium has the ability of deacidification and oxygen removal in steel, which makes the section crystallization of steel compact and has higher strength., at the same time, this kind of steel can make the cutter sharper, sharp durability is further improved, and to overcome the blade scratch, gap defects.

Dimensions

We offer premium steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

Similar Grade

execution standard ZEICIN Grade GB AISI JIS DIN
GB 7Cr17MoV 7Cr17MoV ASTM 440A SUS 440A/AUS6

 

Main chemical composition %

C Cr Mn Si Mo V
0.65~
0.70
16.40~
17.10
0.40~
0.80
≤1.00 0.50~0.60 0.10~0.
30
Co S P Ni Nb W
– ≤0.01 ≤0.02 <0.4
0
– –

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

5 +AT: Solution annealed

6 +P: Precipitation hardened

Suface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

7Cr17MoV Steel For Knives

In this article, we are going to review 7Cr17MoV steel – its chemical composition, properties and how it compares with similar steel grades- to help you decide whether it’s a good knife blade.

Steels determine a knife’s capability, and it’s important to know what type of steel will suit your needs. 7Cr17MoV is made through blending elements that make it durable and cost effective compared to other steels in it’s range.

 

What is 7Cr17MoV Steel?

7Cr17MoV steel is a Chinese stainless steel used in many survival knives. The steel is a modified version of 440A steel. More vanadium elements have been added to give it extra strength, increase toughness and wear resistance.

 

The high levels of carbon (0.7%) and chromium (17%) increase its hardness and corrosion resistance making it a great choice for survival blades.

 

In terms of quality, 7Cr17MoV steel falls under the mid-range steels. It’s softer compared with high-end grades, but it’s durable thanks to the added elements which boost its wear resistance.

Though 7Cr17MoV may not be the best in regard to edge retention, it does make sharpening an easier experience.

 

Regardless, the steel is resilient under constant hard use which makes it ideal for kitchen and outdoor budget knives.  Another steel we have discussed in detail that is very similar is 8Cr13MoV.

 

Properties of 7Cr17MoV Steel

The properties of a steel are determined by its chemical composition. These properties should help in informing how a particular steel is suitable for your needs.

 

Edge Retention

7Cr17MoV Steel contains Sulphur and Phosphorus. While this increases brittleness and compromise edge retention, the steel compensates for this with good amounts of Carbon and Vanadium. These increase the steel’s hardness, a property that helps boost edge retention.

Overall, 7Cr17MoV Steel may not match up with other high-end steels, but it does have a decent edge retention for its price.

 

Hardness

The high amounts of Carbon in 7Cr17MoV (0.7%), plus Vanadium and Chromium, make the steel considerably hard. After being heat treated, the hardness reaches 60 HRC. This makes 7Cr17MoV steel blades reliable for both general and outdoor use.

 

Toughness

Having hailed 7Cr17MoV for its hardness, one may conclude that the steel is equally tough. Far from it. Hardness and toughness may mean the same thing in general language, but when it comes to steel, it’s different.

 

While hardness refers to a metal’s ability to withstand abrasion, toughness of the steel is determined by its ability to resist fracture.

 

7Cr17MoV steel does not score highly in terms of toughness. Though compared to other high-end steels, it does hold up decently well against abuse.

 

Corrosion Resistance

One of the properties that make 7Cr17MoV steel great for outdoor and survival blades is its high corrosion resistance. It does feature high amounts of Chromium elements which prevents staining.  With a good maintenance routine, 7Cr17MoV steel knives will stay stainless for long, even with some level of abuse.

 

Sharpening

Owing to its relatively low hardness, 7Cr17MoV steel sharpens fairly easily. However, it’s a softer steel compared to others and therefore also loses its sharpness easily.

 

7Cr17MoV Equivalent Steels

The closest equivalent of 7Cr17MoV steel is the 440A. Actually, 7Cr17MoV is a modified 440A, with added Vanadium elements for hardness and wear resistance. Other than the absence of Vanadium in 440A, the chemical composition of the two is almost identical.

 

Another close match is AUS-6. Only that 7Cr17MoV steel has slightly higher amounts of Carbon and Chromium.   Also closely related is 5Cr15Mov which has slightly lower amounts of carbon and chromium. A similar steel that shows a decent increase in edge retention is 9Cr18MoV.

 

Is 7Cr17MoV Steel a Good Knife Steel?

7Cr17MoV is a decent steel that features mostly on hunting, camping, and chef knives. If you intend to use a knife with this steel for such purposes, then yes, 7Cr17MoV steel is a fairly great blade.

 

Its hardness and corrosion resistance properties make it a durable low budget steel that offers decent performance. And even though it does hold up well against rust and wear, basic maintenance would go a long way in prolonging the knife’s usability.

The edge retention is also decent for its price range. 7Cr17MoV is among the best entry-level steels that offers high performance for anyone looking to buy a great steel on a budget.

 

In terms of quality, 7Cr17MoV steel falls under the mid-range steels. It’s softer compared with high-end grades, but it’s durable thanks to the added elements which boost its wear resistance.

Though 7Cr17MoV may not be the best in regard to edge retention, it does make sharpening an easier experience.

Regardless, the steel is resilient under constant hard use which makes it ideal for kitchen and outdoor budget knives.  Another steel we have discussed in detail that is very similar is 8Cr13MoV.

 

Fushun Metal · ISO 9001 · AS9120B
Send the grade, size and standard.

You get chemical composition, mechanical properties and a price — with inspection certificates to EN 10204 3.1 issued against the heat number.

Request a quoteWhatsApp +86 178 7358 1838

[email protected]  ·  +86 731 8990 3933

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.