9CrSi 9SiCr Tool Steel

9CrSi 9SiCr Tool Steel

9CrSi 9SiCr Tool Steel

9CrSi 9SiCr Tool Steel

The 9CrSi steel plate is an alloy tool steel and a low speed low alloy cutting tool steel. 9CsSi has brittleness and hardness, heat sensitivity and surface quenching tendency. The heat treatment of the 9CrSi steel plate is good and the use value will be improved.

 

9CrSi is a commonly used low alloy tool steel, with high hardenability and hardenability, and high tempering stability. It can be used to manufacture tools with complex shapes, small deformation, high wear resistance and low-speed cutting, such as drill bits, thread tools, reamers, die, tap, roller and roller.

We can provide more services:

1、Hardening and tempering
2、Vacuum heat treatment
3、Polished bright surface
4、Milling bright surface
5、CNC machine
6、Deep drilling
7、Cut into small pieces
8、Make it closer to the mold
Welcome to inquiry price from drawing

Cutting:

Precision cutting to standard dimensions

Custom cutting according to client specifications

Cold Work Tool Steel Dimensions

We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

Chemical Components:

Carbon C: 0.85~0.95

Silicon Si: 1.20~1.60

Manganese Mn: 0.30~0.60

Sulfur S :≤0.030

Phosphorus P :≤0.030

Chromium Cr: 0.95~1.25

Nickel Ni: Allowable residual content ≤ 0.25

Copper Cu: Allowable residual content ≤ 0.30

 

Mechanical Properties

9CrSi steel mechanical properties hardness: annealing, 241 ~ 197HB, indentation diameter 3.9 ~ 4.3mm; 187 ~ 229HB (for thread tools); quenching, ≥ 62HRC

 

Applications

Mainly used in the manufacture of low-speed cutting tools (such as woodworking tools, bench tools, drills, milling cutters, broaches, etc.) and measuring tools (such as calipers, micrometers, block gauges, templates, etc.). Measuring tool steel requires high hardness (62 ~ 65HRC), high wear resistance, sufficient toughness, high heat hardness (ie, the cutting tool can maintain high hardness at high temperature); to ensure the accuracy of measurement, the measuring tool is required The cutting tool steel has good dimensional stability.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x