manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

4145H MOD Alloy Steel

4145H MOD Alloy Steel

4145H MOD Alloy Steel Drill Collars

4145H MOD Alloy Steel Drill Collars

4145H MOD Alloy Steel forged bar

4145H MOD Alloy Steel forged bar

4145H MOD Alloy Steel stabilizer

4145H MOD Alloy Steel stabilizer

Description

AISI 4145H 120 ksi, API 7-1 Standards is a chromium molybdenum quality alloy steel specification. As a high tensile steel grade AISI 4145H MOD is primarily supplied in the hardened and tempered condition to 30-36HRc range to AISI 4145H MOD. With a slightly higher carbon content AISI 4145H MOD is similar to AISI 4140 in that it offers good ductility, shock resisting characteristics combined with resistance to wear.

 

Advantages:

1 QTC Qualification Test Coupon Passed

2 Superior Hardenability

3 Optimize chemical component

 

Applications

AISI 4145H MOD Steel is commonly used for a variety of applications in the oil and gas sector. Used often for the manufacture of down hole drilling tools such as drill collars. Other applications include gears, shafts for hydraulic presses, rolls for paper mills, pump shafts and tool holders.

Chemical Composition

Grade C Mn Cr Mo Si P S Ni Cu V Al% H max. ppm
Min. 0.420 0.800 0.850 0.150 0.150 – – – – – 0.020 –
Max. 0.450 1.200 1.200 0.250 0.350 0.025 0.025 0.250 0.300 0.300 0.035 1.500

 

Heat Treatment

Normalizing temperature Time Austenizing temperature Time Tempering temperature Time
1600 – 1750℉

(871 – 960℃)

Min. 60 minutes 1562 – 1675℉

(850 – 913℃)

Min. 60 minutes 1050℉ (566℃) Min. 60 minutes

Oil or Polymer or Water. For Water Quenching, the temperature of water shall not exceed 38℃ (100℉) at start of quench. For bath-type quenching, the temperature of water shall not exceed 49℃(120℉) at any time during the quench cycle.

Mechanical Properties

as per ASTM A370 – 20

Yield strength

minimum (0.2% offset)

Tensile strength minimum Elongation in

2” (minimum)

Reduction Area

(minimum)

120,000 psi (828 MPa) 140,000 psi (966 MPa) 18% 45%

 

Quality Inspection

  • Specimen test location & QTC
  • Charpy V-notch impact at 21℃ / -32℃
  • Hardness as per ASTM E10-18: On surface / 1”below surface
  • Volumetric NDE 100% – Ultrasonic
  • Minimum hot work reduction ratio 4.0 to 1
  • Grain size should be #S or Finer as per ASTM E112 – 13
  • Surface inspection

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x