Upset Forging

upset forging pipe p1

upset forging pipe p1

upset forging pipe p2

upset forging pipe p2

upset forging pipe p3

upset forging pipe p3

Upset forging increases the diameter of a workpiece by compressing its length. Measured by the number of pieces produced, it is the most widely used forging process in the world — engine valves, couplings, bolts, screws and most other fasteners are made this way.

How the process works

Upsetting is normally done on special high-speed machines called crank presses, though a vertical crank press or a hydraulic press can also be used. The machines are usually set up to work in the horizontal plane, which makes it quick to move a workpiece from one station to the next.

The starting stock is usually wire or rod. Larger machines accept bars up to 25 cm (9.8 in) in diameter and deliver a capacity of over 1,000 tons.

The standard upsetting machine uses split dies containing multiple cavities. The dies open far enough for the workpiece to move from one cavity to the next, then close; the heading tool, or ram, travels longitudinally against the bar and upsets it into the cavity. If every cavity is used on each cycle, a finished part comes off every cycle — which is what makes the process so efficient for mass production.

Design rules for upset parts

Three rules decide whether a part can be upset in one blow or needs several stations. They exist to stop the unsupported length from buckling instead of forming:

  1. The length of unsupported metal upset in one blow, without injurious buckling, is limited to three times the bar diameter.
  2. Stock longer than three times the diameter can still be upset, provided the finished diameter is no more than 1.5 times the stock diameter.
  3. Where the stock is longer than three times the diameter and the cavity is not more than 1.5 times the stock diameter, the unsupported length beyond the die face must not exceed one bar diameter.

Where it is used

Engine valves, couplings, bolts, screws and other fasteners — anything with a local enlargement on a straight shank. The same logic applies to tube: upset ends on pipe give a thicker wall for threading or for a welded joint without machining a separate fitting.

Related reading

Fushun Metal · ISO 9001 · AS9120B
Send the grade, size and standard.

You get chemical composition, mechanical properties and a price — with inspection certificates to EN 10204 3.1 issued against the heat number.

Request a quoteWhatsApp +86 178 7358 1838

[email protected]  ·  +86 731 8990 3933

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x