manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

AISI O2, 1.2842, 90MnCrV8, Oil Hardening Tool Steel

DIN 1.2842 O2 Tool Steel Oil Hardening Cold Work Steel

1.2842 o2 tool steel

1.2842 o2 tool steel

1 1.2842 Introduction:

1.2842 Cold work tool steels belong to the family of high carbon steels that are further classified into oil-hardening steels, high-carbon, high-chromium steels, and air-hardening steels. Oil-hardening cold-work steels are also known as group O steels consisting of O1, O2, O6, and O7 types.

We can provide more services:

1、Hardening and tempering
2、Vacuum heat treatment
3、Polished bright surface
4、Milling bright surface
5、CNC machine
6、Deep drilling
7、Cut into small pieces
8、Make it closer to the mold
Welcome to inquiry price from drawing

Cutting:

Precision cutting to standard dimensions

Custom cutting according to client specifications

Cold Work Tool Steel Dimensions

We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

2 1.2842 Applications:

Typical applications for DIN 1.2842 tool steel include medium run dies, press tools, drawing punches, broaches, bushings, lathe centres, chuck jaws, master cavity sinking hobs, plug gauges, thread gauges, thread cutting tools and precision measuring tools. It is also a popular tool steel for cams, cloth cutting knives, cold taps, reamers, collets, cutting hobs, strip slitting cutters, trimmer dies, tube expander rolls, plastic moulds and woodworking knives.

3 Quality Standard:

ASTM A681 – 08 Standard Specification for Tool Steels Alloy.

4 All Grades Comparison:

ASTM Material No. AFNOR UNI B.S.
O2 DIN1.2842 90 MV 8 88 Mn V 8 KU Bo 2

5 1.2842 Chemical Composition(%)

C Si Mn P S Cr Cr V
0.85-0.95 0.50 max 1.40-1.80 0.030 max 0.030 max 0.50 max 0.30 max 0.30 max

6 HEAT TREATMENT:

  • FORGING: Heat uniformly to 1000°C. Forge within a range of 850-1050°C reheating if necessary. Cool slowly (preferably in a furnace) to avoid setting up stresses
  • ANNEALING:O2 tool steel is supplied in the annealed and machineable condition. Re-annealing will only be necessary if the steel has been forged or hardened. To anneal, heat uniformly to 720°C, equalise, then furnace cool (hardness about 229 Brinell). Fully machined tools in grade O2 tool steel should be packed during annealing.
  • HARDENING:Heat uniformly to 790-820°C until heated through. (If possible pre-heat at 300-500°C). Allow thirty minutes per 25 millimetre of ruling section and quench immediately in oil.
  • MARTEMPERTINGMartempering of O2 tool steel is an alternative hardening procedure which may be used when suitable salt bath equipment is available.
  • TEMPERING: Heat the O2 tool steel uniformly and thoroughly at the selected tempering temperatures and hold for at least one hour per inch of total thickness.

7 Mill′s test certificate:

EN 10204/3.1 with all relevant data reg. chem. composition, mech. properties and results of testing.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x