manufacturer of nickel alloy, stainless steel, tool steel, alloy steel

Stainless Steel Foil

Stainless Steel Foil

stainless steel foil

stainless steel foil

1 Introduce

This is a wide flexible stainless steel foil, which is a high-end product in the field of stainless steel strip. Different with stainless steel cold rolled strip of the thickness 0.05-0.5 mm, it is called stainless steel foil under 0.05 mm thickness. Now the TISCO has produce 0.02mm thickness x 600mm width stainless steel foil.

2 Application

Mainly used in aerospace, automotive, electronics, phone, flexible displays, flexible solar modules, sensors, energy storage cells, etc

3 Chemical component

Grade C Si Mn P S Ni Cr Mo Other
301 ≤0.15 ≤1.00 ≤2.00 ≤0.065 ≤0.030 6.00-8.00 16.00-18.00 – –
302 ≤0.15 ≤1.00 ≤2.00 ≤0.035 ≤0.030 8.00-10.00 17.00-19.00 – –
303 ≤0.15 ≤1.00 ≤2.00 ≤0.20 ≤0.030 8.00-10.00 17.00-19.00 –
303Se ≤0.15 ≤1.00 ≤2.00 ≤0.20 ≤0.030 8.00-10.00 17.00-19.00 – Se≥0.15
304 ≤0.07 ≤1.00 ≤2.00 ≤0.035 ≤0.030 8.00-10.00 17.00-19.00 – –
304L ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.030 8.00-10.00 18.00-20.00 – –
316 ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.030 10.00-14.00 16.00-18.50 2.00-3.00 –
316Ti S31635 ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.030 11.00-14.00 16.00-19.00 1.80-2.50 Ti5*C%-0.70
316L ≤0.030 ≤1.00 ≤2.00 ≤0.035 ≤0.030 12.00-15.00 16.00-18.00 2.00-3.00 –
321 ≤0.12 ≤1.00 ≤2.00 ≤0.035 ≤0.030 8.00-11.00 17.00-19.00 – Ti5(C%-0.02)~0.08

 

Stainless Grade Thickness mm Hardness Thinckness and Splitted Width
SUS301 0.03 190—370° over 2mm / width 350mm
0.04 190—450° over 2mm / width 350mm
0.05 190—630° over 2mm / width 350mm
0.06 190—630° over 2mm / width 350mm
— 190—630° over 2mm / width 350mm
— 190—630° over 2mm / width 350mm
— 190—630° over 2mm / width 350mm
0.7 190—630° over 4mm / width 350mm
0.8 190-580° over 4mm / width 350mm
over 0. 8 190-560° over 4mm / width 350mm
SUS316L 0. 03/0. 04/0. 05 140—350° over 4mm / width 350mm
0.08 140—380° over 4mm / width 350mm
— over 4mm / width 350mm
— over 4mm / width 350mm
0.8 140—380° 4mm/350mm
over 1.0 140—350° over 5mm / width 350mm
SUS304 0. 03/0. 04/0. 05 160—370° over 4mm / width 350mm
0.06 160—410° over 4mm / width 350mm
— 160—410° over 4mm / width 350mm
— 160—410° over 4mm / width 350mm
0.8 160—410° over 4mm / width 350mm
1.0 — 1.5 160—380 over 5mm / width 350mm
SUS201 0.08 190—370° over 4mm / width 350mm
0. 1/0. 8 190—450° over 5mm / width 350mm
over 0. 8 190—430° over 5mm / width 350mm
0. 1–0. 5 450—600° over 4mm / width 350mm

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x