What is the difference between 718H mold steel and P20H mold steel?

What are the characteristics of 718H mold steel? What are the characteristics of P20 die steel? What is the difference between 718 mold steel and P20H mold steel?

 

718H, P20 and 1.2738 compared on hardness, section capability and cost.
Figure 1: 718H, P20 and 1.2738 compared on hardness, section capability and cost.

A: 718H mold steel, corresponding to Chinai’s 3Cr2NiMo mold steel.

**Features**

718H is an improved steel grade of P20H mold steel(3Cr2Mo mold steel). which has greatly improved quality, making it Fill in the shortage of P20H mold steel and meet the requirements of P20H mold steel.

Except that it cannot be used for plastic mold parts with corrosion resistance requirements, it is currently the most widely used mold steel.

The typical grade of the universal plastic mold steel. Commonly referred to as “advanced”plastic mold steel, newly developed New steel grades often take it as a typical comparison.

 

B: P20 mold steel is a type of mold welding material, the earliest is P20, by P20H,P20Ni phase Features

1.P20H mold steel has the physical characteristics of uniform hardness, and has good polishing performance and photo-etching. Engraving performance, and P20 mold steel excellent processing performance.

2.P20H die steel is made of pure steel through vacuum degassing refining treatment, which is more suitable for polishing or Etching on plastic mold.

3.The P20H mold steel has been pre-hardened to 285-330HB(30-36HRC). which can be directly used for mold processing without heat treatment, greatly shortening the construction period and saving its operating costs. Good dimensional stability.

4.The physical properties of the P20H mold steel are dense after forging and rolling. Ultrasonic inspection can be used to find that the P20H mold steel has no defects such as pinholes and pinholes.

Note:P20H steel is suitable for making plastic molds and die materials for die-casting low-melting metals.

 

C: This steel has good machinability and mirror polishing performance.

Difference between 718H mold steel and P20H mold steel

(1)718H=P20H+1% Ni.

(2) The hardness of 718H steel is 4HRC higher than that of P20H.

(3)P20H is generally used as a less demanding plastic mold or plastic lower mold.718H Good polishing performance Generally used as a plastic mold with polishing requirements.

(4) The 718H die steel is in the annealed state at the factory and the hardness is HB290-310.

(5) The 718H is in a pre-hardened state at the factory, and its hardness is HRC28-36.

 

We are the factory of special steel if you need any tool steel , please kindly contact with me thanks!

What “pre-hardened” actually promises

Both P20 and 718H arrive at working hardness, which removes a heat treatment step, the distortion that comes with it, and the risk of a cavity moving after hardening. That is the main reason they dominate plastic mould work.

The promise has a limit that is easy to miss: it applies at the surface, and only holds through the section if the steel has the hardenability to carry it. P20 is a chromium-molybdenum grade and loses hardness in thick blocks. 718H adds nickel for depth, which is exactly what a large cavity needs.

When 718H is worth the premium

Above roughly 300 mm block thickness, the difference stops being marginal. A P20 block that measures 30 HRC at the face may be several points softer in the middle, and the cavity machined there behaves differently from the one next to it. 718H holds 33–38 HRC more uniformly, so a large mould machines and polishes consistently across its whole face.

Below about 200 mm, the two are close enough that the price difference usually decides — and P20 wins.

What to put on the order

State the block dimensions, the hardness range at the surface and at mid-section, and whether the cavity needs a mirror polish. The last one matters: polishing quality depends on cleanliness, and two heats within the same grade can differ.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x