HNFS201113 Cr12MoV Hot Rolled Steel Plate Successful Delivered

On November 2020, We, Fushun Metal, had delivered a batches of Cr12MoV hot rolled steel plate for client from Uzbekistan successful!

 

  1. What is Cr12MoV steel grade?

Cr12MoV steel is a kind of ledeburite cold work tool steel which developed from Cr12 steel, as the added content of Mo, V, and decrease of C, Cr12MoV have the advantage of Higher hardenability, hardness, wear resistance and small heat treatment distortion. It’s regularly be used in manufacturing cold mold with a heavy load, bulk production, and complex shape. Due to Cr12MoV is ledeburite steel, so its toughness is greatly influenced by the carbide morphology and distribution.

 

  1. Where Cr12MoV use to?

used in the manufacture large, complex shape, working under arduous conditions, with a variety of Die and tools, such as die punching, trimming mold, piping die, deep drawing steel mold, circular saws, standards, tools and gauges, thread rolling die and so on.

 

  1. Chemical composition% of Cr12MoV steel
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) Cu(%)
1.45~1.70 ≤0.40 ≤0.40 ≤0.030 ≤0.030 11.00~12.50 ≤0.20 0.40~0.60 0.15~0.30 ≤0.30

 

  1. Cr12MoV equivalents alloy steel
Steel Country Code C(%) V(%) Si(%) Mn(%) P(%) S(%) Cr(%)
SKD11 CNS 1.4-1.6 0.2-0.5 ≦0.4 ≦0.6 ≦0.03 ≦0.03 11.0-13.0
Cr12MoV GB 1.45-1.70 0.15-0.30 ≦0.4 ≦0.4 ≦0.03 ≦0.03 11.0-12.5
SKD11 JIS 1.4-1.6 0.2-0.5 ≦0.4 ≦0.6 ≦0.03 ≦0.03 11.0-13.0
X165Cr-MoV12 DIN 1.55-1.75 0.1-0.5 0.25-0.40 0.2-0.4 ≦0.03 ≦0.03 11.0-12.0

5. Documents

HNFS201113 Cr12MoV Hot Rolled Steel Plate Successful Delivered

HNFS201113 Cr12MoV Hot Rolled Steel Plate Successful Delivered

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x