1.4528 Introduce

W.-Nr. 1.4528 ( DIN X105CrCoMo18-2 ) High carbon martensitic stainless chromium steel with cobalt, molybdenum and vanadium  is equivalent to BOHLER N690 or written as N690Co. It’s a similar version of Japanese VG10 steel.

1.4528 Applications

Hardened cutting tools with excellent edge-holding property, such as knive blades, cutting surgical instruments, rotary knives for the meat processing industry, plate and knive-edge fulcrums, corrosion resistant roller bearings, valve needles and pistons for refrigerating machines.

1.4528 Advantage

Hardness approx. 60 HRC
Very high resistance to rust
Very good to polish
High edge retention on sharpening level B / C
Recommendation for outdoor knives, camping knives, pocket knives, hunting knives, etc.
NOT suitable for Damascus steel!
Hardening: 1050 ° / tempering at 180 ° C for 2 x 2 hours (in between quenching in cold water) gives approx. 60 HRC.

CHEMICAL COMPOSITION (average %)

C Si Mn Cr Mo V Co
1.08 0.40 0.40 17.30 1.10 0.10 1.50

PRODUCT DESCRIPTION

Hardened cutting tools with excellent edge-holding property, such as knive blades, cutting surgical instruments, rotary knives for the meat processing industry, plate and knive-edge fulcrums, corrosion resistant roller bearings, valve needles and pistons for refrigerating machines.

PROPERTY FEATURES

Martensitic chromium steel with cobalt, molybdenum and vanadium addition. For tools and components which can be hardened to very high hardness levels. Surface finish required for good corrosion resistance: fine ground or polished.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x