With over 35 years of industry expertise, Fushun has the industry knowledge and resources to find you the metal products that you need for your specific industry applications. We are in stock and ready to quickly deliver hard-to-find metals. Our ISO 9001-certified metal supply is one of the most comprehensive selections on the market. We provide timely customer support and quick delivery on all quantities of our in stock products.
Contact us for more information regarding our nickel alloy manufacturing and distribution options. Fushun is your trusted nickel alloy supplier for all types of Nickel alloy material.
NICKEL 200 DESCRIPTION
Nickel 200 is a solid solution strengthened, commercially pure wrought materials with excellent mechanical properties and resistance to corrosion. It also has exceptional resistance to caustic alkalis at different concentrations and temperatures. However, the corrosion resistance is better in de-aerated acid. The alloy has low gas content and vapor pressure, and high thermal and electrical conductivities. Nickel 200 (UNS N02200/W.Nr. 2.4060) is commercially pure (99.6%) wrought nickel. It has good mechanical properties and excellent resistance to many corrosive environments. Other useful features of the alloy are its magnetic and magnetostrictive properties, high thermal and electrical conductivities, low gas content and low vapor pressure. The corrosion resistance of Nickel 200 makes it particularly useful for maintaining product purity in the handling of foods, synthetic fibers, and caustic alkalies; and also in structural applications where resistance to corrosion is a prime consideration. Other applications include chemical shipping drums, electrical and electronic parts, aerospace and missile components.
What are the characteristics of Nickel 200/201?
Highly resistant to various reducing chemicals
Excellent resistance to caustic alkalies
High electrical conductivity
Excellent corrosion resistance to distilled and natural waters
Resistance to neutral and alkaline salt solutions
Excellent resistance to dry fluorine
Widely used to handle caustic soda
Good thermal, electrical and magnetostrictive properties
Offers some resistance to hydrochloric and sulfuric acids at modest temperatures and concentrations
Nickel 200/201 ASTM Specifications
| Pipe Smls | Pipe Welded | Tube Smls | Tube Welded | Sheet / Plate | Bar | Fitting |
| B161 | B622 | B161 | B622 | B162 | B160 | B163 |
Mechanical Properties
Room Temperature properties of Various Products
| Product Form | Condition | Tensile (ksi) | .2% Yield (ksi) | Elongation (%) | Hardness (HRB) |
| Rod & Bar | Hot Finished | 60-85 | 15-45 | 55-35 | 45-80 |
| Rod & Bar | Cold Drawn / Annealed or Hot-Finished / Annealed | 55-75 | 15-30 | 55-40 | 45-70 |
| Plate | Hot-Rolled / Annealed | 55-80 | 15-40 | 60-40 | 45-75 |
| Sheet | Annealed | 55-75 | 15-30 | 55-40 | 70 max |
| Tube & Pipe | Seamless Annealed | 55-75 | 12-30 | 60-40 | 70 max |
| Form | ASTM |
| Rod and bar | B 160 |
| Plate, sheet and strip | B 162, B 906 |
| Seamless pipe and tube | B 161, B 829 |
| Welded pipe | B 725, B 775 |
| Welded tube | B 730, B 751 |
| Welding fitting | B 366 |
| Forging | B 564 |
APPLICATIONS
Electronic components where going maybe required
Lead wires
Battery components
Transducers
Sparking electrodes
Heat exchangers
Bands and tags
Chemical composition:
| Grade | Chemical Component % | ||||||
| Ni | Fe | Cu | C | Mn | S | Si | |
| Nickel 200 | Min 99.0 | Max 0.4 | Max 0.25 | Max 0.15 | Max 0.35 | Max 0.01 | Max 0.35 |
PHYSICAL PROPERTIES
Density, 0.321 lbs/in³, 8.89 g/cm³
Specific Heat: BTU/lb/°F (J/kg•K):
32-212°F (0-100°C): 0.12 (456)
Thermal Conductivity, BTU/hr/ft²/ft/°F (W/m•K)
At 212ºF (100ºC): 38.8(67.1)
At 400°F (204°C): 35.4(61.3)
At 600ºF (316ºC): 36.5(56.3)
Mean Coefficient of Thermal Expansion: in/in/°F (μm/m•K)
80-200°F (27- 93°C): 7.4 x 10 (13.3)
80-400°F (27-204°C): 7.7x 10 (13.9)
80-600°F (27-316°C): 8.0x 10 (14.4)
Modulus of Elasticity, KSI (MPa)
30.0x 10³ (207 x 10³)
Melting Range: 2615-2535°F (1435-1445°C)
MECHANICAL PROPERTIES AT ROOM TEMPERATURE
PROPERTIES: ANNEALED
Ultimate Tensile Strength: 55 KSI min (380 MPa min)
Yield Strength (0.2% offset): 15 KSI min (100 MPa min)
Elongation:
35% min: gauges ≤ 0.0035 inches
40% min: gauges > 0.0035 inches
Hardness:
HV 117 max: gauges ≤ 0.010 inches
Rb 66 max: gauges > 0.010 inches
PROPERTIES: TEMPERED
Nickel 200 can be cold rolled to achieve the temper properties required by specific customers and/or manufacturing requirements. Contact Ulbrich Wire for details.
Physical Properties
The following table shows the physical properties of Nickel 200 alloy.
| Properties | Metric | Imperial |
| Density | 8.89 g/cm3 | 0.321 lb/in3 |
| Melting point | 1435-1446°C | 2615-2635°F |
Thermal Properties
The thermal properties of Nickel 200 alloy are given in the following table
| Properties | Metric | Imperial |
| Thermal expansion co-efficient (@20-100°C/68-212°F) | 13.3 µm/m°C | 7.39 µin/in°F |
| Thermal conductivity | 70.2 W/mK | 487 BTU.in/hrft².°F |
Fabrication and Heat Treatment
Nickel 200 alloy can be shaped through all hot working and cold working practices. The alloy can be hot worked between 649°C (1200°F) and 1232°C (2250°F), with heavy forming carried out at temperatures above 871°C (1600°F). Annealing is performed at temperature between 704°C (1300°F) and 871°C (1600°F).
Other Designations
Other designations that are equivalent to nickel 200 alloy include the following:
ASME SB-160 – SB-163
DIN 17740
DIN 17750-17754
BS 3072-3076
ASTM B 160 – B 163
ASTM B 725
ASTM B 730
STANDARD WIRE FINISHES
Extra Clean: Extra clean is also referred to as “bright annealed” or “bright annealed and cold rolled”
Grease (round wire only): Drawn in a heavy grease produces an “Ultra bright” finish for decorative applications
Soap (round wire only): Soap is used as a lubricant in the drawing process and is not removed. It acts as a lubricant during customer part forming operation.
A soap finish is available in tempered products.
Plated: Many plating options are available.
Quality & Testing
Fushun supply Certification with all shipments, containing full chemical analysis and also mechanical test results if requested.
All incoming material is visually inspected and PMI (Positive Material Identification) tested before processing begins and all our production material is checked during each stage of processing.
All incoming orders are produced to the individual customer specification, some of which may involve processing sample batches for testing prior to full production.
Final Inspection carried out on all finished material to include:
Visual inspection
Dimensional checks
PMI (Positive Material Identification)
Mechanical tests
Nickel Alloy Material Available Formats
Fushun offers pure Nickel alloy materials in a variety of forms, including:
Seamless & welded pipe
Seamless & welded tube
Bar
Wire
Sheet
Plate
Forgings
Pipe fittings
Flanges
Weld Rod
Nickel Alloy Supply Quantities for Single Items or Full Bills
At Fushun, we can supply single items or full bills of nickel alloy materials for most any project. No inquiry is too small. We offer quick responses to customer inquiries and specialize in the rapid delivery of both large and small quantities of nickel alloy products.
Contact Fushun for Nickel Alloy Materials Today
Contact us for more information regarding our nickel alloy material options, or request a quote for further pricing details today. Fushun is your trusted nickel alloy supplier and manufacturer of premium nickel alloy materials.