AISI 9260 61SiCr7 1.7108 Spring Steel

AISI 9260 Spring Steel

AISI 9260 Spring Steel

AISI 9260 Spring Steel

 

Alloy Steel 9260, also sold AISI 9260, is a high-silicon, spring alloy steel. It offers users outstanding corrosion resistance, hardness, toughness, and strength. Alloy Steel 9260 is machinable in the annealed condition, and is weldable by most common methods except oxyacetylene welding. You will find Alloy Steel 9260 in a wide variety of applications, most of which demand resistance to bending and failures. Alloy Steel 9260 is used in a number of different products and industries including:

Airplanes

Military weaponry

Rail transportation

Bridges

Machine tools

Knives and swords

 

All About 9260 Steel (Properties, Strength, and Uses)

Physical Properties of 9260 Steel

9260 steel is given its four-digit name by the joint naming index created by the AISI and SAE. To learn more about this naming scheme, as well as the differences between steel grades, review our article on the types of steels.

 

The first digit designates the class of the steel alloy- that is, what the major alloying components are (besides carbon). For this steel, the “9” shows that this steel is of the silicon-manganese class of alloy steels. The second digit represents the percentage of these major elements; the “2” in 9260 steel, therefore, means this class is around 2% silicon/manganese. Finally, the last two digits represent the carbon percentage in the steel, in increments of 0.01%. Using this rule, 9260 steel is 0.60% carbon. The exact chemical composition of 9260 steel is much more specific, (seen below with tolerances), but its name gives a good idea as to its general makeup.

 

9260 steel can often be found as AISI 9260 steel and is considered a high-silicon spring alloy steel. This means it has good spring characteristics and is useful for its flexion as well as its resilience to deformation. It is easily machined when annealed and can be welded by all methods except via oxyacetylene torches. It is generally resistant to corrosion and is hard enough to resist local surface deformation. It is forgeable as well as heat treatable and responds well to quench hardening. 9260 steel has a density of 7.85 g/cm3 (0.284 lb/in3) and is most often found in the form of round bar, plate, tube, and sheet stock. Its optimal spring characteristics make 9260 steel an exceptional choice when producing leaf and conical springs but can also be used in many other areas as a high-strength alloy.

 

Applications of 9260 Steel

Type 9260 steel is a versatile spring steel; its high strength, corrosion resistance, hardness, and workability lend it to any application which favors resilience. It is most commonly used in leaf and conical springs, but some other notable applications can be seen below:

Aircraft parts

Military technology

Bridge supports

Machine tools

Blades and cutlery

Railway applications

 

HEAT TREATMENT

Annealing: To produce a structure of coarse to fine spheroidite, parts should be austenitized at 1400ºF (760ºC) and cooled to 1300ºF (705º) at a rate of 10ºF/hr., or alternately cooled to 1225ºF (660ºC) and held for 10 hours as an iso-anneal.

Normalizing: 1650ºF (900ºC) and air cool. This will be an important treatment for this grade.

Hardening: Austenitize at 1525-1580ºF (830-860ºC) and water quench.

Tempering: 880-970ºF (470-520ºC)

Machinability: Parts could be machined following a spheroidize anneal

Weldability: The grade would not normally be welded.

 

9260 carbon steel, this steel is used to manufacture knives and swords. Flexibility is one of its main qualities, which is used in the manufacture of swords and fencing foils, also for its high resistance to impacts. Easy to work, with very good results.

Its main features:

– High flexibility.

– Medium hardness.

– Average cutting edge retention.

– Up to 61 HRC

– High machinability.

Chemical composition (%): C: 0.65, Si: 1.80, Mn: 0.80, Cr: 0.35

This steel is recommended both for beginners as professionals, the degree of difficulty of work is low. Supplied annealed (soft), to facilitate the work.

 

9260 has the capability to be a harder blade. The silicon alloy increases shock resistance and if tempered correctly is a superior material. The incredibly crafted blade that has both strength and flexibility. It is an excellent material for katanas. It is highly durable in most dojo applications and extremely resistant to bending and failures. The use of 0.6% carbon allows this blade to be sturdy enough for tatami omote yet forgiving enough to resist dangerous chipping on rigid targets.

Relevant standard:

JIS SUP6 / SUP7

EN/DIN 10089 60SiCr7

ISO 683 60SiCr7

NF  60Cr7 / 25II60

BS Z51A60

OCT 60C2

GB/T1222 60Si2Mn

 

Chemical composition

C Si Mn S P Cr Ni Cu
0.56~0.64 1.50~2.00 0.60~0.90 ≤0.035 ≤0.035 ≤0.35 ≤0.35 ≤0.25

 

Properties  Conditions
T (°C) Treatment
Density (×1000 kg/m3) 7.7-8.03 25
Poisson’s Ratio 0.27-0.30 25
Elastic Modulus (GPa) 190-210 25
Tensile Strength (Mpa) 1758 25 oil quenched, fine grained, tempered at 425°C  more
Yield Strength (Mpa) 1503
Elongation (%) 8
Reduction in Area (%) 24
Hardness (HB) 600 25 oil quenched, fine grained, tempered at 205°C more

 

Chemical composition % of the ladle analysis of grade AISI 9260 and Standards

Designations France: AFNOR 60 S 7 , AFNOR 61 SC 7
Germany: DIN 1.0909
United Kingdom: B.S. 250 A 58
United States: ASTM A29 , ASTM A322 , ASTM A331 , ASTM A505 , ASTM A519 , ASTM A59 , SAE J1268 , SAE J404 , SAE J412 , SAE J770 , UNS G92600

 

Mechanical Properties

Properties  Conditions
T (°C) Treatment
Density (×1000 kg/m3) 7.7-8.03 25
Poisson’s Ratio 0.27-0.30 25
Elastic Modulus (GPa) 190-210 25
Tensile Strength (Mpa) 1758 25 oil quenched, fine grained, tempered at 425°C
Yield Strength (Mpa) 1503
Elongation (%) 8
Reduction in Area (%) 24
Hardness (HB) 600 25 oil quenched, fine grained, tempered at 205°C

 

Machining performance

Download AISI 9260 the mechanical properties of the report, the report provides detailed performance analysis and application.

 

Principal Design Features

One of the most widely used precipitation hardening grades in the business. While soft and ductile in the solution annealed condition, it is capable of high properties with a single precipitation or aging treatment. Characterized by good corrosion resistance, high harness, toughness and strength.

 

Machinability

Long, gummy chips characterize this alloys machinability. It can be machined in the annealed condition, however condition H1150M will yield best results. Post machining solution treatment of parts will be required prior to final hardening if machining in this condition.

 

Heat Treatment

CONDITION A–Soak at 1900 F (1038 C) for 30 minutes and cool below 60 F (16 C) for complete martensite transformation. CONDITION H 950- Treat Condition A material at 900 F(482 C) for 1 hour, air cool.. CONDITION H925, H1025, H1075, H1100, H1150- Soak solution treated material for 4 hours at specified temperature, air cool, CONDITION H1150M- Soak solution treated material at 1400 F (760 C) for 2 hours, air cool, then re-heat to 1150 F (620 C) for 4 hours and air cool.

 

Welding

Successfully welded by common fusion and resistance methods, this alloy should not be joined by oxyacetylene welding. AWS E/ER630 filler metal is recommended if required.

 

Forging

Soak for 1 hour at 2150 F (1177 C) prior to forging. Do not work below 1850 F (1010 C). Post-work solution treatment is required prior to final hardening

 

9260 Steel equivalent

Country Japan BS China USA
Standard JIS G4801 EN 10089 GB/T 1222 ASTM A29
Grade SUP6 61SiCr7 60Si2Mn 9260

 

9260 steel overviews

Size Round Dia 6-120mm
Plate/Flat/Block Thickness
6mm-60mm
Width
20mm-160mm
Heat treatment Normalized ; Annealed ; Quenched ; Tempered
Surface condition Black; Peeled; Polished; Machined; Grinded; Turned; Milled
Delivery condition Forged; Hot rolled; Cold drawn
Test Tensile strength, Yield strength, elongation, area of reduction, impact value, hardness, grain size, ultrasonic test, US inspection, magnetic particle testing, etc.
Payment terms T/T;L/C;/Money gram/ Paypal
Trade terms FOB; CIF; C&F; etc..
Delivery time 30-45 days
Application blades, sword

 

Fushun Metal · ISO 9001 · AS9120B
Send the grade, size and standard.

You get chemical composition, mechanical properties and a price — with inspection certificates to EN 10204 3.1 issued against the heat number.

Request a quoteWhatsApp +86 178 7358 1838

[email protected]  ·  +86 731 8990 3933

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x