1.2601 X165CrMoV12 Cold Work Tool Steel

1.2601 X165CrMoV12 Cold Work Tool Steel

1.2601 X165CrMoV12 Cold Work Tool Steel

1.2601 X165CrMoV12 Cold Work Tool Steel

X165CrMoV12 1.2601 is a German Cold work tool alloy steel material grade.it is shock resisting steel. it belong to DIN 17350 standard. Digital Grade material number 1.2601. Metal Steel Grade W-Nr X165CrMoV12  It is a die steel, use in extrusion moulds, Hot Cast moulds. like aluminium production, Aluminium cutting mold.

We can provide more services:

1、Hardening and tempering
2、Vacuum heat treatment
3、Polished bright surface
4、Milling bright surface
5、CNC machine
6、Deep drilling
7、Cut into small pieces
8、Make it closer to the mold
Welcome to inquiry price from drawing

Cutting:

Precision cutting to standard dimensions

Custom cutting according to client specifications

Cold Work Tool Steel Dimensions

We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

Applications

Cutting tools, stamping, woodworking, drawing, deep drawing and pressing tools, cold working

rolls , measuring tools .

 

Material equivalent of DIN X165CrMoV12 | 1.2601 steel

Germany Italy Sweden Spain
DIN,WNr UNI SS UNE
X165CrMoV12 | 1.2601 X165CRMOW12KU 2310 X160CRMOV12

 

Chemical composition (wt.%) of 1.2601

C Si
Mn
P
S
Cr Mo Other
1.55-1.75 0.25-0.40 0.20-0.40 0.030 0.030 11.0-12.0 0.50-0.70 V   0.10-0.50
W   0.40-0.60

Smelting Option

1 EAF: Electric Arc Furnace

2 EAF+LF+VD: Refined-smelting and vacuum degassing

3 EAF+ESR: Electro Slag Remelting

4 EAF+PESR: protective atmosphere Electro Slag Remelting

5 VIM+PESR: Vacuum induction melting

 

Forming Option

1 Hot rolling process

2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging

 

Heat-treatment Option

1 +A: Annealed (full/soft/spheroidizing)

2 +N: Normalized

3 +NT: Normalized and tempered

4 +QT: Quenched and tempered (water/oil)

 

Suface Option

1 Black Surface

2 Grounded: Bright but rough ; Not precision

3 Machining for plate: Bright and precision; Little turning scar

4 Peeled/Turned: Bright and precision; Little turning scar

5 Polished: Very Bright and precision size; Not turning scar

 

Other Services

1 Cutting: Small pieces

2 CNC Machine: Produce as your drawing

3 Package: Bare/Nylon/Canvas/Wooden

4 Payment:T/T, L/C, O/A(request credit)

5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)

 

Mechanical Properties of 1.2601

Rp0.2 (MPa) Rm (MPa) Impact
KV (J)
Elongation
A (%)
A Z (%) Delivery Hardness HB
641 (≥) 662 (≥) 23 14 31 Solution & Aging, Ann, Ausaging, Q+T 142

 

Heat treatment of X165CrMoV12 | 1.2601 Cold work tool steel

Annealing: Annealing temperature/℃: 800~830; After the annealing, degree of hardness ≤HBS: 255

Quenching: Hardening temperature/℃: 980~1010, Quenching in oil or air

Tempering: Commonly used drawing temperature/℃: 180~250;  After tempering hardness HRC | 100 ℃ : 63; After tempering hardness HRC | 200 ℃ : 61; After tempering hardness HRC | 300 ℃ : 60 ; After tempering hardness HRC | 400 ℃ : 58

Normalizing:at Normalizing temperature, then cool in furnace

 

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x