1.2316 X38CrMo16 Cold Work Tool Steel For Plastic Mould
This steel 1.2316 is mainly used for plastic injection molds, in connection with chemically aggressive and acidic plastics such as thermoplastics and for PVC-arminoplastics, extrusion tools, compressor parts and for special machine parts in the food industry.
We can provide more services:
1、Hardening and tempering
2、Vacuum heat treatment
3、Polished bright surface
4、Milling bright surface
5、CNC machine
6、Deep drilling
7、Cut into small pieces
8、Make it closer to the mold
Welcome to inquiry price from drawing
Cutting:
Precision cutting to standard dimensions
Custom cutting according to client specifications
Surface Grinding/Polishing:
Thickness tolerance: -0 to +0.1mm
Flatness: 0.01/100mm
Surface roughness: Ra ≤1.6 or Rz ≤6.3
Applications :
Molds for pressing of chemically-aggressive plastic substances etc. All kinds of silicon steel sheet and high-speed blanking die. Precise stamping die. Cold extruding forming die. Cavitations Molds, Standard Mould Base, Compression Mould for SMC, blowing mould, Pet preform mold, plastic piping & plumbing injection molds.
We can provide more services:
1、Hardening and tempering
2、Vacuum heat treatment
3、Polished bright surface
4、Milling bright surface
5、CNC machine
6、Deep drilling
7、Cut into small pieces
8、Make it closer to the mold
Welcome to inquiry price from drawing
Equivalent grades of steel X38CrMo16 (1.2316)
| EU EN |
Germany DIN,WNr |
ASTM AISI | JIS | |
| X38CrMo16 |
|
422 | SUS4201J2 |
Chemical composition % of steel X38CrMo16 (1.2316): EN 4957-2000
| C | Si | Mn | Ni | P | S | Cr | Mo |
| 0.33 – 0.45 | max 1 | max 1.5 | max 1 | max 0.03 | max 0.03 | 15.5 – 17.5 | 0.8 – 1.3 |
Smelting Option
1 EAF: Electric Arc Furnace
2 EAF+LF+VD: Refined-smelting and vacuum degassing
3 EAF+ESR: Electro Slag Remelting
4 EAF+PESR: protective atmosphere Electro Slag Remelting
5 VIM+PESR: Vacuum induction melting
Forming Option
1 Hot rolling process
2 Hot Forging: Electro-hydraulic; High-speed-hydraulic; Oil-hydraulic; Precision-forging
Heat-treatment Option
1 +A: Annealed (full/soft/spheroidizing)
2 +N: Normalized
3 +NT: Normalized and tempered
4 +QT: Quenched and tempered (water/oil)
Suface Option
1 Black Surface
2 Grounded: Bright but rough ; Not precision
3 Machining for plate: Bright and precision; Little turning scar
4 Peeled/Turned: Bright and precision; Little turning scar
5 Polished: Very Bright and precision size; Not turning scar
Other Services
1 Cutting: Small pieces
2 CNC Machine: Produce as your drawing
3 Package: Bare/Nylon/Canvas/Wooden
4 Payment:T/T, L/C, O/A(request credit)
5 Transport:FOB/CFR/CIF/DDU/DDP (train/ship/Air)
MECHANICAL PROPERTIES
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
| 116 (≥) | 695 (≥) | 23 | 33 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 443 |
HEAT TREATMENT:
already pre-toughened; usually no heat treatment required
Soft annealing:
760 to 800 °C for about 4 to 5 hours; slow controlled cooling of 10 to 20 °C per hour to about 650 °C; further cooling in air, max. 230 HB
Hardening:
1030 to 1050 °C 15 to 30 minutes keeping curing temperature quenching in water/oil obtainable hardness: 49 HRC
Tempering:
Slow heating to tempering temperature immediately after hardening. Minimum time in furnace: 1 hour per 20 mm part thickness
You get chemical composition, mechanical properties and a price — with inspection certificates to EN 10204 3.1 issued against the heat number.