What is P530 non-magnetic steel ?

What is P530 non-magnetic steel ? – P530 for drill collar

P530 non-magnetic steel is a kind of high Mn-AL-V non-magnetic steel, chemical composition determines the electromagnetic properties, stable organization, excellent mechanical properties, low permeability and high resistivity, eddy current loss in the magnetic field is very small, in the magnetic field strength of 16000a/m (200 Aust), the magnetic permeability of non-magnetic steel μ≤1.319×10-6 h/m (1.05 high / Aust) stainless steel permeability μ=1.339×10-6h/m (1.1 high/au), austenitic stainless steel is mildly magnetic after cold working. Non-magnetic steel can maintain stable austenite in various states, with very low magnetic permeability, high hardness, strength, and good wear resistance. Due to the cold work hardening phenomenon of high manganese steel, cutting and machining is difficult. Using high temperature annealing process, the particle size, shape and distribution state of carbide can be changed, thus significantly improving the cutting performance of non-magnetic steel.

 

P530 non-magnetic steel uses a gas soft oxidation process to further improve the surface hardness of non-magnetic steel, increasing wear resistance and significantly improving the service life of the parts. Non-magnetic steel is suitable for the manufacture of non-magnetic molds, non-magnetic bearings and other structural parts that require no magnetic induction in strong magnetic fields. In addition, because of its high temperature strength and hardness, non-magnetic steel can also be used to make hot work molds for use below 700°C-800°C.

 

P530 non-magnetic steel maintains stable austenite in all states and has very low magnetic permeability, high strength, hardness, and wear resistance, but poor machinability. With the global economy industrial restructuring, manufacturing and other traditional industries due to the increasing saturation of the European and American markets, labor costs jump higher year by year, profits reduce, the center of gravity to developing countries. China’s labor resources are abundant and cheap, so the potential market for molds in China is large, which determines that China will certainly develop into a large country for mold manufacturing, and the proportion of the world’s non-magnetic steel output value has increased significantly, and the amount of non-magnetic steel is also increasing significantly.

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x