X22CrMoV12-1 1.4923 Martensitic Creep Resisting Stainless Steel


X22CrMoV12-1 1.4923 Martensitic Creep Resisting Stainless Steel


Introduction and Applications

FUSHUN SPECIAL STEEL, as a professional stainless steel manufacturer, is proud to supply high-quality X22CrMoV12-1 (1.4923) martensitic creep resisting stainless steel. This premium grade steel is specifically engineered for demanding high-temperature applications where exceptional mechanical strength and creep resistance are essential requirements.

X22CrMoV12-1 stainless steel is a heat-treatable martensitic grade containing a carefully balanced combination of chromium, molybdenum, vanadium, and nickel elements. This steel grade demonstrates excellent performance at elevated temperatures up to 580°C (1076°F), making it ideal for critical components in power generation and industrial applications. The material is typically produced and heat treated according to QT800 specification, ensuring optimal mechanical properties at both room temperature and elevated operating temperatures.

Primary Applications

Power Generation:
Turbine blades, steam turbine components, and power plant equipment operating at elevated temperatures.
Pressure Equipment:
Pressure vessels, boilers, and high-temperature fasteners for industrial processing systems.
Aerospace Industry:
Aviation components and aerospace applications requiring high strength at elevated temperatures.
Chemical Processing:
Reactor manufacturing and chemical production facility components exposed to high temperatures.

Chemical Composition of X22CrMoV12-1 (1.4923)

The carefully balanced chemical composition of 1.4923 steel ensures optimal creep resistance and mechanical properties at high temperatures. As a trusted manufacturer, FUSHUN SPECIAL STEEL maintains strict control over all alloying elements during the melting process.

C Si Mn Ni P S Cr Mo V
0.18-0.24 ≤0.50 0.40-0.90 0.30-0.80 ≤0.025 ≤0.015 11.0-12.5 0.80-1.20 0.25-0.35

Mechanical Properties of X22CrMoV12-1 (1.4923)

The following mechanical properties are achieved after quenching and tempering (+QT) heat treatment. FUSHUN SPECIAL STEEL guarantees these properties through rigorous quality control and in-house heat treatment facilities.

Property Value Condition
Tensile Strength (Rm) 800-950 MPa +QT
0.2% Proof Strength (Rp0.2) ≥600 MPa +QT
Elongation at Fracture (A) ≥14% +QT
Reduction of Area (Z) ≥40% +QT
Impact Energy (KV) at +20°C ≥27 J +QT
Brinell Hardness (HBW) ≤302 +A (Annealed)

Heat Treatment Guidelines

Proper heat treatment is essential for achieving optimal mechanical properties in X22CrMoV12-1 steel. As a manufacturer with complete in-house heat treatment capabilities, FUSHUN SPECIAL STEEL ensures precise temperature control and consistent results for every batch.

Annealing (+A)

Heat to 750-800°C, hold for adequate time based on section thickness, then furnace cool slowly. This process reduces hardness and improves machinability.

Hardening (Quenching)

Heat to 1020-1070°C, hold until uniformly heated through the section, then oil quench or air cool. Preheating at 650-700°C is recommended for large sections.

Tempering

Temper at 680-750°C for QT800 condition. Hold time depends on section size (minimum 2 hours). Air cool after tempering. Double tempering may be beneficial.

Stress Relieving

Heat to 650-700°C (below tempering temperature), hold for 1-2 hours per 25mm of thickness, then furnace cool or air cool slowly.

Equivalent Grades and International Standards

X22CrMoV12-1 (1.4923) complies with multiple international standards. FUSHUN SPECIAL STEEL can supply materials certified to customer-specified standards.

Standard Grade Designation
EU/EN X22CrMoV12-1 (1.4923)
Germany (DIN/EN) X22CrMoV12-1, X20CrMoV12-1 (1.4922)
France (AFNOR) Z21CDV12
USA (ASTM/AISI) Similar to AISI 422
Japan (JIS) Similar to SUH616
China (GB) 2Cr12NiMoWV, 1Cr12Mo1W1V
UK (BS) Similar to 762

Applicable Standards: EN 10302:2008 (Creep resisting steels), EN 10269:1999 (Steels for fasteners), EN 10088-1:2005 (Stainless steels list)

Available Product Forms and Sizes

As a manufacturer with comprehensive hot rolling and hot forging capabilities, FUSHUN SPECIAL STEEL offers X22CrMoV12-1 (1.4923) in various product forms to meet diverse customer requirements.

Product Form Available Dimensions
Round Bar Diameter: 6 – 600 mm
Plate Thickness: 0.1 – 20 mm; Width: 8 – 1500 mm
Wire Diameter: 0.1 – 30 mm
Strip Thickness: 0.1 – 4 mm; Width: 80 – 1219 mm
Flat & Square Bar Size: 5 – 400 mm

We can produce not only large special-shaped forgings but also small-sized flat steel. Special dimensions and custom sizes are available upon request. Contact us to discuss your specific requirements. Bulk orders are always welcome!

Why Choose FUSHUN SPECIAL STEEL as Your Manufacturer?

As a vertically integrated steel manufacturer, FUSHUN SPECIAL STEEL offers significant advantages for customers requiring high-quality X22CrMoV12-1 (1.4923) steel products.

Advanced Melting Technology

In-house ESR (Electroslag Remelting), VIM (Vacuum Induction Melting), and VAR (Vacuum Arc Remelting) capabilities for producing premium quality steel with superior cleanliness and homogeneity.

In-House Heat Treatment

Complete heat treatment facilities ensure consistent quality, precise property control, and faster delivery times. All processes are performed under strict quality management systems.

Bright Bar & Grinding Services

Our turning (peeled) and grinding facilities provide ready-to-use bright bars, saving downstream customers significant time and machining costs while ensuring tight tolerances.

Reliable Quality & Fast Delivery

Vertical integration from melting to finishing ensures stable quality and shorter lead times. We welcome bulk orders and provide competitive pricing for large volume purchases.

Contact FUSHUN SPECIAL STEEL Today

As a leading manufacturer of specialty steels, we are ready to fulfill your X22CrMoV12-1 (1.4923) requirements. Bulk orders and custom specifications are always welcome!

Visit us at: www.fushunspecialsteel.com

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

info@fushunspecialsteel.com

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : info@fushunspecialsteel.com

x