1.2162 21MnCr5 20ХГ Cold Work Tool Steel

1.2162 21MnCr5 20ХГ Cold Work Tool Steel

1.2162 21MnCr5 20ХГ Cold Work Tool Steel

1.2162 21MnCr5 20ХГ Cold Work Tool Steel

Grade :  21MnCr5 Number:   1.2162

 

Classification

Alloy cold-work tool steel

 

Standard:

EN ISO 4957: 2000 Tool steels

Cutting:

Precision cutting to standard dimensions

Custom cutting according to client specifications

 

Surface Grinding/Polishing:

Thickness tolerance: -0 to +0.1mm

Flatness: 0.01/100mm

Surface roughness: Ra ≤1.6 or Rz ≤6.3

Characteristics

Manganese-chrome steel for case-hardening with the middle hardenability, with the hardness of case-hardened layer and with the high hardness in the core. Further the steel is characterized by a good ductility at the heat, good workability in the annealed state and it is easy to polish.

We can provide more services:

1、Hardening and tempering
2、Vacuum heat treatment
3、Polished bright surface
4、Milling bright surface
5、CNC machine
6、Deep drilling
7、Cut into small pieces
8、Make it closer to the mold
Welcome to inquiry price from drawing

Cold Work Tool Steel Dimensions

We offer premium cold work tool steel in various forms, manufactured with advanced 5000-ton forging press technology for superior density and performance.

Product Form Specifications
Forged Round Bar Dia. up to 1200mm
Forged Flat Bar Thickness 100-600mm, Width 300-2000mm
Rolled Round Bar Dia. 10-200mm
Hot Rolled Plate Thickness 1-100mm, Width 60-1600mm

 

APPLICATION:

machine parts and moulding plates with a high surface hardness;

synthetic resin press moulds for the processing of thermoplastics and thermosetting plastics.

 

Suitability

For small and middle-size cemented molds for mechanical working of plastic materials and rubber with the demand on higher hardness in the core.

 

Chemical composition%of the ladle analysis of grade 1.2162

C(%) Si(%) Mn(%) P(%) S(%) Cr(%)

0.18-0.24 0.15-0.35 1.10-1.40 Max 0.030 Max 0.030 1.00-1.30

 

Product range

Round bars: D10 – D615

Blocks: 510×1010

Metal sheets: s.5 – s.150

We will deliver any semi-finished products from the above mentioned dimensions. Other dimensions, except for given stock supplies, have to be consulted with us.

 

HEAT TREATMENT:

Soft annealing:

670 to 710 °C for about 2 to 5 hours

slow controlled cooling, further cooling in air, max. 205 HB

Carburising:

900 to 950 °C. The choice of the carburising means and carburising temperature depends on the desired surface carbon content, the carburising graph and the required case depth.

Application:

870 to 930 °C in powder/salt bath, cooling in oil/warm bath at 160 to 250 °C

Intermediate stress-relieving heat treatment:

630 to 650 °C, about 2 to 4 hours with slow furnace cooling

Preheating:

350 °C depending on dimensions

Hardening:

curing temperature 810 to 840 °C in oil of ~ 60 °C warmth

Cooling:

down to about 100 °C in oil, then in air to about 50 °C

Tempering:

1 hour per 20 mm part thickness, at least 2 hours

About Us

Founded in 1998, FuShun covers an area of 3000 square meters, annual sales volume of 20000 tons. We are engaged in the manufacture and export of Tool Steel, Nickel Alloy, Stainless Steel and other special steel products…,View more content About Me.

Contact Lists

General Manager: Ms. Florence

[email protected]

Get A Free Quote!

Find your steel grade and get a quote today.

NOW Send Your Inquiry To : [email protected]

x